Hydrogen desorption kinetics of a LaNi4.7Al0.3 metal hydride electrode using potentiostatic measurements

被引:12
作者
Feng, F
Han, JW
Geng, MM
Northwood, DO
机构
[1] Ryerson Polytech Univ, Fac Engn & Appl Sci, Toronto, ON M5B 2K3, Canada
[2] Univ Windsor, Windsor, ON N9B 3P4, Canada
关键词
metal hydride electrode; kinetics; phase transformation;
D O I
10.1016/S0927-0248(99)00135-X
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
The reaction kinetics of an activated LaNi4.7Al0.3 metal hydride (MH) electrode during the discharge process were studied using charge/discharge and potentiostatic measurements. The electrochemical measurements were conducted at varying applied potentials and temperatures. The potentiostatic measurements show that the reacted fraction alpha(t) (alpha(t) is the ratio of the discharge capacity at time, t, to the maximum discharge capacity) of the MH electrode during the discharge process depends on both the applied potential and temperature. Analysis of the kinetic data indicates that the primary rate controlling step for the discharge process of the LaNi4.7Al0.3 electrode is the beta --> alpha phase transformation process at temperatures in the range 298-328 K and at applied potentials in the range from - 0.8 to - 0.6 V vs. Hg/HgO. The dependence of reacted fraction alpha(t) of the MH electrode reaction on time t obeys a nucleation and growth (ng) equation: -ln(1 - alpha(t)) = kt(m) (k and m are material parameters of the MH electrode during the discharge process; the reaction rate constant K-ng = k(1/m); t is the discharge time (min)). The increase in applied potential leads to a decrease in the hydrogen activity. The nucleation and growth of the alpha-hydride phase, resulting from the decrease in the hydrogen activity, leads to an increase in the reacted fraction. The reaction rate constant (K-ng) increases with increasing temperature which is in agreement with an Arrhenius-type temperature behavior. The calculated apparent activation energy (E-a) from the Arrhenius equation for the discharge reaction of the MH electrode was 41.1 kJ (mol H)(-1) for temperatures ranging from 298 to 328 K. (C) 2000 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:51 / 61
页数:11
相关论文
共 17 条
  • [1] [Anonymous], J ELECTROCHEM SOC
  • [2] BARD AJ, 1980, ELECTROCHEMICAL METH, P101
  • [3] Studies on the diffusion coefficient of hydrogen through metal hydride electrodes
    Chen, J
    Dou, SX
    Bradhurst, DH
    Liu, HK
    [J]. INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 1998, 23 (03) : 177 - 182
  • [4] Christian J.W., 1975, THEORY TRANSFORMATIO
  • [5] ELECTROCHEMICAL STUDIES OF HYDROGEN STORAGE IN AMORPHOUS NI64ZR36 ALLOY
    CIUREANU, M
    RYAN, DH
    STROMOLSEN, JO
    TRUDEAU, ML
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1993, 140 (03) : 579 - 584
  • [6] HYDRIDING AND DEHYDRIDING RATES OF THE LANI5-H SYSTEM
    GOODELL, PD
    RUDMAN, PS
    [J]. JOURNAL OF THE LESS-COMMON METALS, 1983, 89 (01): : 117 - 125
  • [7] DESORPTION-KINETICS OF LANI5, LANI4.7AL0.3, (CFM)NI5 AND MNI4.5AL0.5 HYDRIDES
    GOUDY, AJ
    WALLINGFORD, RA
    [J]. JOURNAL OF THE LESS-COMMON METALS, 1984, 99 (02): : 249 - 256
  • [8] SURFACE MODIFICATION OF METAL HYDRIDE NEGATIVE ELECTRODES AND THEIR CHARGE DISCHARGE PERFORMANCE
    IWAKURA, C
    MATSUOKA, M
    ASAI, K
    KOHNO, T
    [J]. JOURNAL OF POWER SOURCES, 1992, 38 (03) : 335 - 343
  • [9] Hydrogen desorption kinetics in MmNi4.2Al0.8-H SYSTEM
    Mungole, MN
    Balasubramaniam, R
    [J]. INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 1998, 23 (05) : 349 - 353
  • [10] Kinetics of hydride formation in massive LaNi5 samples
    Osovizky, A
    Bloch, J
    Mintz, MH
    Jacob, I
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 1996, 245 : 168 - 178