Phase diagram and superabundant vacancy formation in Cr-H alloys

被引:42
作者
Fukai, Y [1 ]
Mizutani, M [1 ]
机构
[1] Chuo Univ, Dept Phys, Tokyo 1128551, Japan
关键词
chromium; hydrogen; phase diagram; superabundant vacancy; high pressure; X-ray diffraction;
D O I
10.2320/matertrans.43.1079
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
X-ray diffraction measurements on the Cr-H system were made using synchrotron radiation at high hydrogen pressures and high temperatures, and the phase diagram was determined up to p(H-2) = 5.5 GPa and T less than or equal to 1400 K. Three solid phases were found to exist; a bcc phase (alpha) of low hydrogen concentrations, x = [H]/[Cr]less than or equal to0.03 existing at low hydrogen pressures (less than or equal to4.4 GPa), and two high-pressure phases, an hcp (epsilon) phase at lower temperatures and an fee (gamma) phase at higher temperatures, both having high hydrogen concentrations xsimilar to1. A drastic reduction of the melting point is caused by dissolution of hydrogen. A gradual lattice contraction observed in the fee phase indicates the formation of superabundant Cr-atom vacancies (vacancy-hydrogen clusters). Thermal desorption measurements after recovery from high p(H-2), T treatments revealed several desorption stages including those due to the release from vacancy-hydrogen clusters and from hydrogen-gas bubbles, and allowed determination of relevant trapping energies.
引用
收藏
页码:1079 / 1084
页数:6
相关论文
共 40 条
[21]   High-pressure studies of high-concentration phases of the Ti-H system [J].
Nakamura, K ;
Fukai, Y .
JOURNAL OF ALLOYS AND COMPOUNDS, 1995, 231 (1-2) :46-50
[22]   TRENDS IN HYDROGEN HEATS OF SOLUTION AND VACANCY TRAPPING ENERGIES IN TRANSITION-METALS [J].
NORDLANDER, P ;
NORSKOV, JK ;
BESENBACHER, F .
JOURNAL OF PHYSICS F-METAL PHYSICS, 1986, 16 (09) :1161-1171
[23]   MULTIPLE DEUTERIUM OCCUPANCY OF VACANCIES IN PD AND RELATED METALS [J].
NORDLANDER, P ;
NORSKOV, JK ;
BESENBACHER, F ;
MYERS, SM .
PHYSICAL REVIEW B, 1989, 40 (03) :1990-1992
[24]   The melting temperature of iron hydride at high pressures and its implications for the temperature of the Earth's core [J].
Okuchi, T .
JOURNAL OF PHYSICS-CONDENSED MATTER, 1998, 10 (49) :11595-11598
[25]   Agglomeration of hydrogen-induced vacancies in nickel [J].
Osono, H ;
Kino, T ;
Kurokawa, Y ;
Fukai, Y .
JOURNAL OF ALLOYS AND COMPOUNDS, 1995, 231 (1-2) :41-45
[26]  
Pearson W. B., 1958, HDB LATTICE SPACINGS
[27]  
PEISL H, 1978, HYDROGEN METALS, V1, P53
[28]   DEFECT TRAPPING OF GAS ATOMS IN METALS [J].
PICRAUX, ST .
NUCLEAR INSTRUMENTS & METHODS, 1981, 182 (APR) :413-437
[29]  
PONYATOVSKII EG, 1976, DOKL AKAD NAUK SSSR, V229, P1171
[30]   PARAMAGNETIC SUSCEPTIBILITY OF CHROMIUM HYDRIDE [J].
ROY, RJ ;
GIBB, TRP .
JOURNAL OF INORGANIC & NUCLEAR CHEMISTRY, 1967, 29 (02) :341-&