Phase diagram and superabundant vacancy formation in Cr-H alloys

被引:42
作者
Fukai, Y [1 ]
Mizutani, M [1 ]
机构
[1] Chuo Univ, Dept Phys, Tokyo 1128551, Japan
关键词
chromium; hydrogen; phase diagram; superabundant vacancy; high pressure; X-ray diffraction;
D O I
10.2320/matertrans.43.1079
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
X-ray diffraction measurements on the Cr-H system were made using synchrotron radiation at high hydrogen pressures and high temperatures, and the phase diagram was determined up to p(H-2) = 5.5 GPa and T less than or equal to 1400 K. Three solid phases were found to exist; a bcc phase (alpha) of low hydrogen concentrations, x = [H]/[Cr]less than or equal to0.03 existing at low hydrogen pressures (less than or equal to4.4 GPa), and two high-pressure phases, an hcp (epsilon) phase at lower temperatures and an fee (gamma) phase at higher temperatures, both having high hydrogen concentrations xsimilar to1. A drastic reduction of the melting point is caused by dissolution of hydrogen. A gradual lattice contraction observed in the fee phase indicates the formation of superabundant Cr-atom vacancies (vacancy-hydrogen clusters). Thermal desorption measurements after recovery from high p(H-2), T treatments revealed several desorption stages including those due to the release from vacancy-hydrogen clusters and from hydrogen-gas bubbles, and allowed determination of relevant trapping energies.
引用
收藏
页码:1079 / 1084
页数:6
相关论文
共 40 条
[1]   NEUTRONENBEUGUNG AN HEXAGONALEM CHROM [J].
ALBRECHT, G ;
DOENITZ, FD ;
KLEINSTUCK, K ;
BETZL, M .
PHYSICA STATUS SOLIDI, 1963, 3 (07) :K249-K252
[2]  
BARANOWSKI B, 1972, ROCZ CHEM, V46, P525
[3]  
Baranowski B., 1974, P 4 INT C HIGH PRESS, P577
[4]  
BARANOWSKI B, 1978, HYDROGEN METALS, V2, P157
[6]  
Fromm E., 1980, International Metals Reviews, V25, P269
[7]   EVIDENCE OF COPIOUS VACANCY FORMATION IN NI AND PD UNDER A HIGH HYDROGEN PRESSURE [J].
FUKAI, Y ;
OKUMA, N .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 2-LETTERS & EXPRESS LETTERS, 1993, 32 (9A) :L1256-L1259
[8]   FORMATION OF SUPERABUNDANT VACANCIES IN PD HYDRIDE UNDER HIGH HYDROGEN PRESSURES [J].
FUKAI, Y ;
OKUMA, N .
PHYSICAL REVIEW LETTERS, 1994, 73 (12) :1640-1643
[9]   Hydrogen-induced superabundant vacancies and diffusion enhancement in some FCC metals [J].
Fukai, Y ;
Haraguchi, T ;
Hayashi, E ;
Ishii, Y ;
Kurokawa, Y ;
Yanagawa, J .
DIFFUSIONS IN MATERIALS: DIMAT2000, PTS 1 & 2, 2001, 194-1 :1063-1068
[10]   Formation of superabundant vacancies in Pd-H alloys [J].
Fukai, Y ;
Ishii, Y ;
Goto, Y ;
Watanabe, K .
JOURNAL OF ALLOYS AND COMPOUNDS, 2000, 313 :121-132