The influence of CO2 and H2O on the storage properties of Pt-Ba/Al2O3 LNT catalyst studied by FT-IR spectroscopy and transient microreactor experiments

被引:29
|
作者
Morandi, S. [1 ,2 ]
Prinetto, F. [1 ,2 ]
Ghiotti, G. [1 ,2 ]
Castoldi, L. [3 ]
Lietti, L. [3 ]
Forzatti, P. [3 ]
Daturi, M. [4 ]
Blasin-Aube, V. [4 ]
机构
[1] Univ Turin, Ctr Excellence, Dipartimento Chim, I-10125 Turin, Italy
[2] Univ Turin, NIS, I-10125 Turin, Italy
[3] Politecn Milan, Dipartimento Energia, Ctr Excellence, Lab Catalysis & Catalyt Proc,NEMAS, I-20133 Milan, Italy
[4] Univ Caen, CNRS, ENSICAEN, Catalyse & Spectrochim Lab, F-14050 Caen, France
关键词
Pt-Ba/Al2O3; NO storage; CO2; operando FT-IR; Transient microreactor experiments; NOX STORAGE/REDUCTION CATALYST; NSR CATALYSTS; REDUCTION; ADSORPTION; WATER; POTASSIUM; OXIDE; TPD;
D O I
10.1016/j.cattod.2013.12.036
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
The effect of CO2 and H2O on the NO/O-2 storage over a Pt-Ba/Al2O3 LNT catalyst was investigated in the temperature range 150-350 degrees C by combining FT-IR spectroscopy and microreactor flow experiments. It is found that the presence of water shows negligible effect on the NO storage at all the temperatures studied. Otherwise, the presence of CO2 inhibits the "nitrite route" (initial formation of surface nitrites and their subsequent evolution to nitrates), whereas the "nitrate route" (involving NO oxidation to NO2 over Pt and its subsequent adsorption on Ba in the form of nitrates) proceeds as in the absence of CO2. The inhibition effect of CO2 on nitrite formation increases on increasing the temperature. This behavior is likely related to the different thermal stability of nitrites and carbonates and, in particular, to the decreasing ability of nitrites to displace carbonates on increasing temperature. Simultaneously, the presence of CO2 in the feed significantly shortens or eliminates the dead time in the NO breakthrough at the reactor outlet. As a consequence, the presence of dead time in the absence of CO2 has been correlated to the occurrence of the nitrite route. (C) 2014 Elsevier B.V. All rights reserved.
引用
收藏
页码:116 / 124
页数:9
相关论文
共 50 条
  • [21] Reaction Pathways in the Reduction of NOx Species by CO over Pt-Ba/Al2O3: Lean NOx Trap Catalytic Systems
    Nova, Isabella
    Lietti, Luca
    Forzatti, Pio
    Frola, Francesca
    Prinetto, Federica
    Ghiotti, Giovanna
    TOPICS IN CATALYSIS, 2009, 52 (13-20) : 1757 - 1761
  • [22] Al2O3 support triggering highly efficient photoreduction of CO2 with H2O on noble-metal-free CdS/Ni9S8/Al2O3
    Li, Sha
    Wang, Qianqian
    Yan, Xiaoliang
    Zhuang, Hua-Qiang
    Yuan, Chen
    Feng, Junpeng
    Wang, Meijun
    Li, Ruifeng
    Li, Wenyang
    Pan, Yun-Xiang
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2019, 240 : 174 - 181
  • [23] Influence of reductant on the regeneration of SO2-poisoned Pt/Ba/Al2O3 NOx storage and reduction catalyst
    Liu, ZQ
    Anderson, JA
    JOURNAL OF CATALYSIS, 2004, 228 (01) : 243 - 253
  • [24] CO2 methanation catalyzed by a Fe-Co/Al2O3 catalyst
    Yu, Wen-Zhu
    Fu, Xin-Pu
    Xu, Kai
    Ling, Chen
    Wang, Wei-Wei
    Jia, Chun-Jiang
    JOURNAL OF ENVIRONMENTAL CHEMICAL ENGINEERING, 2021, 9 (04):
  • [25] Temperature-programmed FT-IR study of the adsorption of CO and co-adsorption of CO and H-2 on Ni/Al2O3
    Hu, CW
    Chen, YQ
    Li, P
    Min, H
    Chen, Y
    Tian, AM
    JOURNAL OF MOLECULAR CATALYSIS A-CHEMICAL, 1996, 110 (02) : 163 - 169
  • [26] Detailed kinetic modeling of NOx storage and reduction with hydrogen as the reducing agent and in the presence of CO2 and H2O over a Pt/Ba/Al catalyst
    Lindholm, Anna
    Currier, Neal W.
    Li, Junhui
    Yezerets, Aleksey
    Olsson, Louise
    JOURNAL OF CATALYSIS, 2008, 258 (01) : 273 - 288
  • [27] Investigation on Deactivation of Cu/ZnO/Al2O3 Catalyst for CO2 Hydrogenation to Methanol
    Liang, Binglian
    Ma, Junguo
    Su, Xiong
    Yang, Chongya
    Duan, Hongmin
    Zhou, Huanwen
    Deng, Shaoliang
    Li, Lin
    Huang, Yanqiang
    INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2019, 58 (21) : 9030 - 9037
  • [28] Labeled 15NO Study on N2 and N2O Formation Over Pt-Ba/Al2O3 NSR Catalysts
    Lietti, L.
    Righini, L.
    Castoldi, L.
    Artioli, N.
    Forzatti, P.
    TOPICS IN CATALYSIS, 2013, 56 (1-8) : 7 - 13
  • [29] Chemical poisoning by zinc and phosphorous of Pt/Ba/Al2O3 NOx storage catalysts
    Jonsson, Rasmus
    Ilmasani, Rojin Feizie
    Pingel, Torben Nilsson
    Skoglundh, Magnus
    Olsson, Eva
    Berggrund, Malin
    Olsson, Louise
    APPLIED CATALYSIS A-GENERAL, 2019, 571 : 158 - 169
  • [30] Quantified NOxadsorption on Pt/K/gamma-Al2O3 and the effects of CO2 and H2O
    Toops, TJ
    Smith, DB
    Epling, WS
    Parks, JE
    Partridge, WP
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2005, 58 (3-4) : 255 - 264