The effect of cooling conditions on Ti 6%Al 4%V microstructure observed using high-temperature in-situ scanning electron microscopy

被引:2
|
作者
Kane, Genevieve A. [1 ,2 ]
Andersen, Dustin [1 ,2 ]
Frey, M. David [2 ]
Hull, Robert [1 ,2 ]
机构
[1] Rensselaer Polytech Inst, Dept Mat Sci & Engn, 110 8th St, Troy, NY 12180 USA
[2] Rensselaer Polytech Inst, Ctr Mat Devices & Integrated Syst, 110 8th St, Troy, NY 12180 USA
基金
美国国家科学基金会;
关键词
Microstructural evolution; Surface faceting; Phase change kinetics; Lamellar growth; Scanning electron microscopy; TITANIUM-ALLOY; HEAT-TREATMENT; CRACK-GROWTH; TI-6AL-4V; FATIGUE; DEFORMATION; SUPERPLASTICITY; DECOMPOSITION; MECHANISMS; BEHAVIOR;
D O I
10.1557/s43578-020-00102-4
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This study focuses on continuous imaging of microstructural changes in Ti 6% Al 4% V when cooling from the beta transus of similar to 995 degrees C or above. A range of microstructures were obtained by accessing different cooling rates. With cooling rates of 0.1-0.5 degrees C/s, lamellar microstructures were observed, which initiate in a colony microstructure below temperatures of similar to 930 degrees C. When the lamellar microstructure began forming at grain boundaries, cooling was interrupted to further observe the kinetics in the system. Lamellae changed in projected length from 40 mu m to similar to 160-320 mu m over three minutes at similar to 930 degrees C, within the alpha + beta mixed phase. On further time at temperature, the lengthening of lamellae stagnated. With further cooling at 0.1 degrees C/s, lamellae grew in projected width, while the projected length remained the same. In addition, a surface topography formed at elevated temperatures (around 800 degrees C), evolved during the alpha to beta heating transition, and persisted upon cooling.
引用
收藏
页码:717 / 728
页数:12
相关论文
共 50 条
  • [41] Microstructure and mechanical property of Ti and Ti6Al4V prepared by an in-situ shot peening assisted cold spraying
    Luo, Xiao-Tao
    Wei, Ying-Kang
    Wang, Yan
    Li, Chang-Jiu
    MATERIALS & DESIGN, 2015, 85 : 527 - 533
  • [42] High-temperature fatigue and creep damage mechanism in additively manufactured Ti-6Al-4V alloy
    Bhandari, Litton
    Gaur, Vidit
    Briffod, Fabien
    Shiraiwa, Takayuki
    Enoki, Manabu
    Engineering Failure Analysis, 2025, 174
  • [43] Enhancing high-temperature oxidation resistance of Ti6Al4V alloy by simple surface aluminization
    Wang, Xiaoyang
    Li, Chun
    Li, Mingshen
    Cao, Jian
    CORROSION SCIENCE, 2021, 192
  • [44] Transmission electron microscopy of deformed Ti-6Al-4V micro-cantilevers
    Ding, Rengen
    Gong, Jicheng
    Wilkinson, Angus J.
    Jones, Ian P.
    PHILOSOPHICAL MAGAZINE, 2012, 92 (25-27) : 3290 - 3314
  • [45] The Effect of Annealing and Cryogenic Treatment on the Microstructure and Mechanical Properties of Ti-6Al-4V Alloy
    Song, Xin
    Qi, Huiping
    Sun, Zongshuai
    Jia, Yanlong
    Hu, Yong
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2025, 34 (03) : 2063 - 2070
  • [46] Effect of hydrogen on the microstructure and mechanical properties of high temperature deformation of Ti6Al4V additive manufactured
    Qi, Fangjuan
    Yao, Jiachen
    Dai, Guoqing
    Chen, Xiaolong
    Guo, Yanhua
    Sun, Zhonggang
    Wang, Yaoqi
    Liu, Hongbing
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2023, 48 (40) : 15292 - 15302
  • [47] Effect of Processing Parameters on Microstructure and Mechanical Properties in High Temperature Deformation of Ti-6Al-4V Alloy
    Yu Weixin
    Li Miaoquan
    Luo Jiao
    RARE METAL MATERIALS AND ENGINEERING, 2009, 38 (01) : 19 - 24
  • [48] A Comparative Study on the High-Temperature Forming and Constitutive Modeling of Ti-6Al-4V
    Uz, Murat Mert
    Yoruc, Afife Binnaz Hazar
    Aydogan, Cahit Sertac
    Yapici, Guney Guven
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (10) : 4376 - 4390
  • [49] Investigation on high-temperature stress relaxation behavior of Ti-6Al-4V sheet
    Luo, Jingfeng
    Xiong, Wei
    Li, Xifeng
    Chen, Jun
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 743 : 755 - 763
  • [50] Effect of Ti addition on high-temperature properties of AlCoCrFeNi2.1 coating prepared on Ti-6Al-4V alloy
    Dong, Jie
    Long, Xiaojiang
    Zhou, Lvjun
    Deng, Hao
    Zhang, Haicheng
    Qiu, Wenbin
    Yin, Ming
    Yin, Guofu
    Chen, Longqing
    CORROSION SCIENCE, 2023, 217