Effects of temperature of HIP process on characteristics of Inconel 718 superalloy

被引:20
作者
Chang, S. H. [1 ]
Lee, S. C.
Tang, T. P.
Ho, H. H.
机构
[1] Natl Cheng Kung Univ, Dept Mat Sci & Engn, Tainan 701, Taiwan
[2] Natl Taipei Univ Technol, Dept Mat & Mineral Resources Engn, Taipei 106, Taiwan
[3] Chung Shan Inst Sci & Technol, Mat & Electroopt Res Div, Lungtan 325, Taiwan
关键词
Inconel; 718; superalloy; hot isostatic pressing; porosity; segregation;
D O I
10.1179/136404606225023399
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The present study focuses on the effects of the temperature of the hot isostatic pressing (HIP) procedure on Inconel 718 superalloy. HIP temperatures used were 1150, 1175, 1180 and 1205 degrees C. HIP pressure was maintained at 1000 bar (98(.)6 MPa) and the soaking time was 2 h. Both room and high temperature tensile and bending tests were used to evaluate the effects of HIP temperature on Inconel 718 superalloy. Porosity tests and microstructural examination were performed. The results showed that the optimum HIP process temperature for 718 superalloy is 1180 degrees C. Processing at this temperature can significantly reduce porosity and improve the microstructure segregation of Inconel 718 superalloy. Under these conditions, the superalloy showed an 18.28% increase in tensile strength at room temperature, a 7(.)38% increase at 540 degrees C, and a 3(.)84% increase at 650 degrees C. The elongation increased by 55(.)6% at room temperature, 109(.)71% at 540 degrees C, and 19(.)91% at 650 degrees C. Finally, the results of three-point bending tests showed that hipping at 1180 degrees C can enhance the bending strength by 39(.)5% at room temperature and 13(.)83% at 540 degrees C.
引用
收藏
页码:175 / 180
页数:6
相关论文
共 17 条
[1]  
*AM SOC MET, 1981, MAT HDB, V4
[2]  
ANTOLOVICH SD, 1992, SUPERALLOYS 1992, P23
[3]   Evaluation of fatigue crack growth rate and life prediction of Inconel 718 at room and elevated temperatures [J].
Chen, Q ;
Kawagoishi, N ;
Nisitani, H .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 277 (1-2) :250-257
[4]  
DONACHIE MJ, 1988, SUPERALLOYS TECHNICA, P47
[5]  
Durand-Charre M., 1997, MICROSTRUCTURE SUPER, P29
[6]  
Flow Autoclave System Inc, 1996, HOT IS PRESS APPL
[7]  
Garvare T., 1987, P INT C HOT IS PRESS, P3
[8]  
HAN X, 2003, J MATER PROCESS TECH, V137, P17
[9]  
KOIZUMI M, 1992, P 3 INT C HOT IS PRE, P195
[10]   Isolation and determination for δ, γ′ and γ" phases in Inconel 718 alloy [J].
Li, RB ;
Yao, M ;
Liu, WC ;
He, XC .
SCRIPTA MATERIALIA, 2002, 46 (09) :635-638