Non-Coulomb friction in gross sliding fretting conditions with aluminium bronze against quenched and tempered steel

被引:15
作者
Hintikka, Jouko [1 ]
Lehtovaara, Arto [1 ]
Mantyla, Antti [2 ]
机构
[1] Tampere Univ Technol, Dept Mat Sci, FIN-33101 Tampere, Finland
[2] Wartsila Finland Oy, Res & Dev, Vaasa 65101, Finland
关键词
Fretting; Friction; Wear; Topography; TI-6AL-4V SUBSTRATE; ROPE WIRES; WEAR; BEHAVIOR; FATIGUE; CONTACT; DISPLACEMENT; AMPLITUDE; TITANIUM; DAMAGE;
D O I
10.1016/j.triboint.2014.06.004
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
A series of fretting tests were performed in gross sliding conditions to study the properties of non-Coulomb friction occurring in the contact of an aluminium bronze sphere against a quenched and tempered steel plane. Measurements were analysed by studying measured fretting loops and the topographies of fretting scars with 3D optical profilometry. Measured fretting loops showed non-Coulomb tangential behaviour, in which the tangential force depended on the tangential displacement. Measurements in which the tangential displacement amplitude was suddenly increased or reduced showed a temporary reduction in the maximum friction force. Fretting wear modified initially polished surfaces producing a tangentially interlocked fretting scar surface profile, which may explain the non-Coulomb increase in the friction force. (C) 2014 Elsevier Ltd. All rights reserved.
引用
收藏
页码:151 / 161
页数:11
相关论文
共 35 条
[1]  
[Anonymous], EL CONT HOLM 2012 IE
[2]  
Bolton W, 2011, MECHATRONICS
[3]   Investigation of variable amplitude loading on fretting fatigue behavior of Ti-6Al-V [J].
Cortez, R ;
Mall, S ;
Calcaterra, JR .
INTERNATIONAL JOURNAL OF FATIGUE, 1999, 21 (07) :709-717
[4]   Fretting cracking behaviour on pre-stressed aluminium alloy specimens [J].
Degat, PR ;
Zhou, ZR ;
Vincent, L .
TRIBOLOGY INTERNATIONAL, 1997, 30 (03) :215-223
[5]   EDGE-BONDED DISSIMILAR ORTHOGONAL ELASTIC WEDGES UNDER NORMAL AND SHEAR LOADING [J].
DUNDURS, J ;
BOGY, DB .
JOURNAL OF APPLIED MECHANICS, 1969, 36 (03) :650-&
[6]   Measurement of tangential contact hysteresis during microslip [J].
Filippi, S ;
Akay, A ;
May, A ;
Gola, MM .
JOURNAL OF TRIBOLOGY-TRANSACTIONS OF THE ASME, 2004, 126 (03) :482-489
[7]   A quantitative approach of Ti-6Al-4V fretting damage:: friction, wear and crack nucleation [J].
Fouvry, S ;
Duó, P ;
Perruchaut, P .
WEAR, 2004, 257 (9-10) :916-929
[8]  
Hills D.A., 1994, MECH FRETTING FATIGU
[9]   Fretting fatigue and friction of quenched and tempered steel in dry contact with aluminum bronze [J].
Hintikka, Jouko ;
Lehtovaara, Arto ;
Mantyla, Antti .
WEAR, 2013, 308 (1-2) :155-165
[10]   Effect of start-up schemes and amplitude of tangential motion on friction behavior in fretting point contact [J].
Hintikka, Jouko ;
Lehtovaara, Arto ;
Lonnqvist, Christian .
TRIBOLOGY INTERNATIONAL, 2011, 44 (11) :1535-1543