The role of 0-2 mm fine recycled concrete aggregate on the compressive and splitting tensile strengths of recycled concrete aggregate concrete

被引:112
作者
Khoshkenari, Adel Gorjinia [1 ]
Shafigh, Payam [2 ]
Moghimi, Mahmoud [3 ]
Bin Mahmud, Hilmi [2 ]
机构
[1] Islamic Azad Univ, Dept Civil Engn, Ayatollah Amoli Branch, Amol, Iran
[2] Univ Malaya, Fac Engn, Dept Civil Engn, Kuala Lumpur 50603, Malaysia
[3] Univ Teknol Malaysia, Fac Civil Engn, Johor Baharu, Malaysia
关键词
Recycled concrete aggregate; Compressive strength; Splitting tensile strength; Normal strength concrete; High strength concrete; MECHANICAL-PROPERTIES; STRUCTURAL CONCRETE; SILICA FUME; PERFORMANCE; PREDICTION; PERMEABILITY; REPLACEMENT; DURABILITY;
D O I
10.1016/j.matdes.2014.07.048
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The aim of this study is to investigate the role of 0-2 mm fine aggregate on the compressive and splitting tensile strengths of recycled concrete aggregate (RCA) concrete with normal and high strengths. Normal coarse and fine aggregates were substituted with the same grading of RCAs in two normal and high strength concrete mixtures. In addition, to keep the same slump value for all mixes, additional water or superplasticizer were used in the RCA concretes. The compressive and splitting tensile strengths were measured at 3, 7 and 28 days. Test results show that coarse and fine RCAs, which were achieved from a parent concrete with 30 MPa compressive strength, have about 11.5 and 3.5 times higher water absorption than normal coarse and fine aggregates, respectively. The density of RCAs was about 20% less than normal aggregates, and, hence, the density of RCA concrete was about 8-13.5% less than normal aggregate concrete. The use of RCA instead of normal aggregates reduced the compressive and splitting tensile strengths in both normal and high strength concrete. The reduction in the splitting tensile strength was more pronounced than for the compressive strength. However, both strengths could be improved by incorporating silica fume and/or normal fine aggregates of 0-2 mm size in the RCA concrete mixture. The positive effect of the contribution of normal sand of 0-2 mm in RCA concrete is more pronounced in the compressive strength of a normal strength concrete and in the splitting tensile strength of high strength concrete. In addition, some equation predictions of the splitting tensile strength from compressive strength are recommended for both normal and RCA concretes. (C) 2014 Elsevier Ltd. All rights reserved.
引用
收藏
页码:345 / 354
页数:10
相关论文
共 58 条
[41]  
OLUOKUN FA, 1991, ACI MATER J, V88, P115
[42]  
OLUOKUN FA, 1991, ACI MATER J, V88, P302
[43]  
Parrott LJ, 1988, LIT REV HIGH STRENGT
[44]   The effect of superplasticisers on the workability and compressive strength of concrete made with fine recycled concrete aggregates [J].
Pereira, P. ;
Evangelista, L. ;
de Brito, J. .
CONSTRUCTION AND BUILDING MATERIALS, 2012, 28 (01) :722-729
[45]  
ROOS F, 1998, S SUST CONSTR US REC
[46]   USE OF RECYCLED CONCRETE AGGREGATE IN CONCRETE: A REVIEW [J].
Safiuddin, Md. ;
Alengaram, Ubagaram Johnson ;
Rahman, Md. Moshiur ;
Salam, Md. Abdus ;
Jumaat, Mohd. Zamin .
JOURNAL OF CIVIL ENGINEERING AND MANAGEMENT, 2013, 19 (06) :796-810
[47]   Study on the influence of attached mortar content on the properties of recycled concrete aggregate [J].
Sanchez de Juan, Marta ;
Alaejos Gutierrez, Pilar .
CONSTRUCTION AND BUILDING MATERIALS, 2009, 23 (02) :872-877
[48]  
SHAH SP, 1985, J PRESTR CONCRETE I, V30, P92
[49]  
Shayan A, 2003, ACI MATER J, V100, P371
[50]   Compressive strength and resistance to chloride ion penetration and carbonation of recycled aggregate concrete with varying amount of fly ash and fine recycled aggregate [J].
Sim, Jongsung ;
Park, Cheolwoo .
WASTE MANAGEMENT, 2011, 31 (11) :2352-2360