Synthesis of CaO•2MgO•8Al2O3 (CM2A8) and its slag resistance mechanism

被引:17
作者
Chen, Junhong [1 ]
Chen, Haiyang [1 ]
Mi, Wenjun [1 ]
Cao, Zheng [1 ]
Li, Bin [1 ]
Li, Guangqi [2 ]
机构
[1] Univ Sci & Technol Beijing, Sch Mat Sci & Engn, Beijing 100083, Peoples R China
[2] Shandong Ceram Co Ltd, Shandong 255100, Peoples R China
关键词
CM(2)A(8); High-purity; CA(2) coating; Slag viscosity; AL-RICH PART; MICROSTRUCTURAL EVOLUTION; CORROSION-RESISTANCE; SYSTEM CAO-AL2O3-MGO; STRUCTURE REFINEMENT; HIGH-ALUMINA; SPINEL; CASTABLES; AL2O3-MGO;
D O I
10.1016/j.jeurceramsoc.2016.11.018
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
CM(2)A(8) is a solid solution of MA and CA(6). As a component in the ternary phase diagram of CaO-Al2O3-MgO, it was not reported in detail. So in this work, analytically pure CaO, MgO and Al2L3 were adopted as starting materials and batched stoimotrically according to CM(2)A(8). The raw materials were ground, mixed, shaped and reaction-sintered at different temperatures (1550 degrees C, 1650 degrees C, 1700 degrees C, and 1750 degrees C) to synthesize CM(2)A(8). The synthesized specimens were analyzed by XRD, SEM, and TEM and the corrosion mechanism against LF slag was also researched. The results show that high-purity CM(2)A(8) can be synthesized by reaction sintering at 1750 degrees C. During synthesis, granular MA and flake CA6 form and grow together; at 1650 degrees C, they solid-solve together to form C(2)M(2)A(14). As the temperature rises, solid solution reaction goes on, which results in the disappearance of CA(6), C(2)M(2)A(14), and MA in succession and forms high-purity CM(2)A(8) growing towards hexagonal column crystals. In the high temperature reaction between CM(2)A(8) and steel slag, Ca2+ in the slag reacts with CM(2)A(8) to form CA(2), damaging the structure of CM(2)A(8) and releasing excessive Mg2+ and A13* which move towards the molten slag. As the reaction between Ca2+ and CM(2)A(8) proceeds, a dense CA(2) coating forms on the surface of CM(2)A(8). The slag viscosity increases as well because of the entrance of Mg2+ and Al3+. Thus, the formation of the CA(2) coating and the enhancement of the slag viscosity restrain the penetration and corrosion of slag towards CM(2)A(8). (C) 2016 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1799 / 1804
页数:6
相关论文
共 28 条
[21]  
Nurse R.W., 1965, BRIT CERAM T J, V64, P409
[22]   DISSOLUTION IN CERAMIC SYSTEMS .3. BOUNDARY LAYER CONCENTRATION GRADIENTS [J].
OISHI, Y ;
COOPER, AR ;
KINGERY, WD .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1965, 48 (02) :88-&
[23]   Potential models for multicomponent oxides: Hexa-aluminates [J].
Park, JG ;
Cormack, AN .
PHILOSOPHICAL MAGAZINE B-PHYSICS OF CONDENSED MATTER STATISTICAL MECHANICS ELECTRONIC OPTICAL AND MAGNETIC PROPERTIES, 1996, 73 (01) :21-31
[24]   The corrosion resistance of microsilica-containing Al2O3-MgO and Al2O3-spinel castables [J].
Sako, E. Y. ;
Braulio, M. A. L. ;
Pandolfelli, V. C. .
CERAMICS INTERNATIONAL, 2012, 38 (06) :4783-4789
[25]   In-Depth Microstructural Evolution Analyses of Cement-Bonded Spinel Refractory Castables: Novel Insights Regarding Spinel and CA6 Formation [J].
Sako, Eric Y. ;
Braulio, Mariana A. L. ;
Zinngrebe, Enno ;
van der Laan, Sieger R. ;
Pandolfelli, Victor C. .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2012, 95 (05) :1732-1740
[26]   Corrosion of high alumina and near stoichiometric spinels in iron-containing silicate slags [J].
Sarpoolaky, H ;
Zhang, S ;
Lee, WE .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2003, 23 (02) :293-300
[27]  
Tak JB, 1982, CERAM B, V61, P725
[28]   STRUCTURE REFINEMENT OF CAO.6AL2O3 [J].
UTSUNOMIYA, A ;
TANAKA, K ;
MORIKAWA, H ;
MARUMO, F ;
KOJIMA, H .
JOURNAL OF SOLID STATE CHEMISTRY, 1988, 75 (01) :197-200