Failure analysis in API X70 pipeline steel in sour environment with an emphasis on fracture surfaces and crack propagation

被引:5
|
作者
Mohtadi-Bonab, M. A. [1 ]
Masoumi, Mohammad [2 ]
Szpunar, J. A. [3 ]
机构
[1] Univ Bonab, Dept Mech Engn, Bonab, Iran
[2] Univ Fed ABC, Ctr Engn Modelagem & Ciencias Socials Aplicadas, BR-09210580 Santo Andre, SP, Brazil
[3] Univ Saskatchewan, Dept Mech Engn, 57 Campus Dr, Saskatoon, SK S7N 5A9, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Failure; EBSD; Fracture surface; Electrochemical hydrogen charging; Taylor factor; Kernel average misorientation; HYDROGEN-INDUCED CRACKING; SULFIDE STRESS CRACKING; CRYSTALLOGRAPHIC TEXTURE; TRAPPING EFFICIENCY; CORROSION CRACKING; MICROSTRUCTURE; RESISTANCE; BEHAVIOR; SUSCEPTIBILITY; TEMPERATURE;
D O I
10.1016/j.ijpvp.2021.104600
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The aim of this study is to investigate the fracture surfaces and crack propagation in an API X70 pipeline steel in acidic environment. To this purpose, as-received and electrochemically hydrogen-charged tensile specimens are subjected to tensile testing. Moreover, EBSD measurements were carried out on the cross section (RD-ND plane) in as-received and hydrogen-charged specimens. The results showed that hydrogen charging and strain rate of tensile testing were considered as two effective parameters in determining the type of fracture. Moreover, the fracture of the uncharged specimens was quite ductile and the strain rate had little effect on the fracture type. A direct correlation was found between type of fracture and the strain rate in hydrogen-charged specimens. With increasing strain rate, the fracture in hydrogen-charged specimens did not have enough time to initiate from inclusions and precipitates and connect to the main fracture surface. < 001 >||ND oriented grains have the highest hydrogen atoms due to the largest interatomic space and the distortion energy accumulated at grain boundaries due to the lack of sufficient activated slip system. The variation of KAM distribution to higher values of hydrogen-charged specimen could be effectively associated to the formation of dislocation walls and dislocation tangles especially in the vicinity of bcc grain boundaries. The higher volume fraction of the grains with high Taylor factor data formed in the hydrogen-charged specimen were highly susceptible to plastic instability, enhancing the crack propagation.
引用
收藏
页数:12
相关论文
共 50 条
  • [32] RESEARCH OF FATIGUE CRACK GROWTH BEHAVIOR OF X70 PIPELINE STEEL IN CORROSIVE ENVIRONMENT AND EVALUATION OF DEFECT
    Wang, Jing
    Li, Xiao-yang
    Li, Shu-rui
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE 2010, VOL 5, 2010, : 455 - 462
  • [33] Crack growth behaviour and crack tip chemistry of X70 pipeline steel in near-neutral pH environment
    Cui, Z. Y.
    Liu, Z. Y.
    Wang, X. Z.
    Li, Q.
    Du, C. W.
    Li, X. G.
    Zhang, W.
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2016, 51 (05) : 352 - 357
  • [34] Fatigue crack propagation of API 5L X70 steel in a modified simulated fuel-grade ethanol (MSFGE) environment
    Marcomini, Jose Benedito
    dos Santos, Elielson Alves
    Sordi, Vitor Luiz
    Giorgetti, Vinicius
    Della Rovere, Carlos Alberto
    Baptista, Carlos Antonio Reis Pereira
    Paes, Marcelo
    JOURNAL OF THE BRAZILIAN SOCIETY OF MECHANICAL SCIENCES AND ENGINEERING, 2023, 45 (12)
  • [35] Fatigue crack propagation of API 5L X70 steel in a modified simulated fuel-grade ethanol (MSFGE) environment
    José Benedito Marcomini
    Elielson Alves dos Santos
    Vitor Luiz Sordi
    Vinícius Giorgetti
    Carlos Alberto Della Rovere
    Carlos Antonio Reis Pereira Baptista
    Marcelo Paes
    Journal of the Brazilian Society of Mechanical Sciences and Engineering, 2023, 45
  • [36] Different delamination cracks during fracture and their influences on the fracture of X70 pipeline steel
    Yang, Zheng
    Beom, Hyeon Gyu
    Kim, Chang-Boo
    Cho, Chongdu
    ADVANCES IN FRACTURE AND MATERIALS BEHAVIOR, PTS 1 AND 2, 2008, 33-37 : 91 - 96
  • [37] A novel semi-empirical technique for improving API X70 pipeline steel fracture toughness test data
    Movahedi, Mohammad Reza
    Hashemi, Sayyed Hojjat
    STEEL AND COMPOSITE STRUCTURES, 2024, 51 (04): : 351 - 361
  • [38] Experimental investigation on crack tip opening angle of X70 pipeline steel
    Faculty of Mechanical and Electronic Engineering, China University of Petroleum, Beijing 102249, China
    不详
    不详
    Gongcheng Lixue, 2008, 7 (201-205):
  • [39] Crystallographic texture and the mechanical properties of API 5L X70 pipeline steel designated for an arctic environment
    Davani, Reza Khatib Zadeh
    Ohaeri, Enyinnaya George
    Yadav, Sandeep
    Szpunar, Jerzy A.
    Su, Jing
    Gaudet, Michael
    Rashid, Muhammad
    Arafin, Muhammad
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 889
  • [40] Anodic Dissolution Behavior of the Crack Tip of X70 Pipeline Steel in Near-Neutral pH Environment
    Cui, Zhongyu
    Wang, Liwei
    Liu, Zhiyong
    Du, Cuiwei
    Li, Xiaogang
    Wang, Xin
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2016, 25 (12) : 5468 - 5476