Dislocations and Plastic Deformation in MgO Crystals: A Review

被引:81
作者
Amodeo, Jonathan [1 ]
Merkel, Sebastien [2 ,3 ]
Tromas, Christophe [4 ]
Carrez, Philippe [2 ]
Korte-Kerzel, Sandra [5 ]
Cordier, Patrick [2 ]
Chevalier, Jerome [1 ]
机构
[1] Univ Lyon, INSA Lyon, CNRS, MATEIS UMR5510, F-69621 Villeurbanne, France
[2] Univ Lille, CNRS, INRA, ENSCL,UMR 8207,UMET Unite Mat & Transformat, F-59000 Lille, France
[3] Inst Univ France, F-75005 Paris, France
[4] Univ Poitiers, Inst Pprime, CNRS, UPR 3346,ENSMA,Dept Phys & Mecan Mat, SP2MI Bd Marie & Pierre Curie BP 30179, F-86962 Futuroscope, France
[5] Rhein Westfal TH Aachen, Inst Phys Met & Met Phys, Kopernikusstr 14, D-52074 Aachen, Germany
基金
欧洲研究理事会;
关键词
MgO; dislocations; mechanical properties; nano-mechanics; multi-scale modeling; extreme conditions; FRACTURE SURFACE ENERGIES; ATOMIC-FORCE MICROSCOPY; HIGH-TEMPERATURE CREEP; PEIERLS-NABARRO MODEL; IN-SITU DEFORMATION; STEADY-STATE CREEP; SINGLE-CRYSTALS; MAGNESIUM-OXIDE; HIGH-PRESSURE; SCREW DISLOCATIONS;
D O I
10.3390/cryst8060240
中图分类号
O7 [晶体学];
学科分类号
0702 ; 070205 ; 0703 ; 080501 ;
摘要
This review paper focuses on dislocations and plastic deformation in magnesium oxide crystals. MgO is an archetype ionic ceramic with refractory properties which is of interest in several fields of applications such as ceramic materials fabrication, nano-scale engineering and Earth sciences. In its bulk single crystal shape, MgO can deform up to few percent plastic strain due to dislocation plasticity processes that strongly depend on external parameters such as pressure, temperature, strain rate, or crystal size. This review describes how a combined approach of macro-mechanical tests, multi-scale modeling, nano-mechanical tests, and high pressure experiments and simulations have progressively helped to improve our understanding of MgO mechanical behavior and elementary dislocation-based processes under stress.
引用
收藏
页数:53
相关论文
共 283 条
[101]   Deformation of MnGeO3 post-perovskite at lower mantle pressure and temperature [J].
Hirose, Kei ;
Nagaya, Yukio ;
Merkel, Sebastien ;
Ohishi, Yasuo .
GEOPHYSICAL RESEARCH LETTERS, 2010, 37
[102]  
Hirth J.P., 1982, Theory of Dislocations, P221
[103]   Fracture modes in micropillar compression of brittle crystals [J].
Howie, Philip R. ;
Korte, Sandra ;
Clegg, William J. .
JOURNAL OF MATERIALS RESEARCH, 2012, 27 (01) :141-151
[104]   A model of size effects in nano-indentation [J].
Huang, Y ;
Zhang, F ;
Hwang, KC ;
Nix, WD ;
Pharr, GM ;
Feng, G .
JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 2006, 54 (08) :1668-1686
[105]   EFFECT OF CRYSTAL ORIENTATION ON PLASTIC DEFORMATION OF MAGNESIUM OXIDE [J].
HULSE, CO ;
COPLEY, SM ;
PASK, JA .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1963, 46 (07) :317-323
[106]   MECHANICAL PROPERTIES OF MAGNESIA SINGLE CRYSTALS IN COMPRESSION [J].
HULSE, CO ;
PASK, JA .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1960, 43 (07) :373-378
[107]   Deformation T-Cup: A new multi-anvil apparatus for controlled strain-rate deformation experiments at pressures above 18 GPa [J].
Hunt, Simon A. ;
Weidner, Donald J. ;
McCormack, Richard J. ;
Whitaker, Matthew L. ;
Bailey, Edward ;
Li, Li ;
Vaughan, Michael T. ;
Dobson, David P. .
REVIEW OF SCIENTIFIC INSTRUMENTS, 2014, 85 (08)
[108]   DISLOCATION-STRUCTURE DURING CREEP OF MGO SINGLE-CRYSTALS [J].
HUTHER, W ;
REPPICH, B .
PHILOSOPHICAL MAGAZINE, 1973, 28 (02) :363-371
[109]   Evidence for {100}⟨011⟩ slip in ferropericlase in from high-pressure/high-temperature experiments Earth's lower mantle [J].
Immoor, J. ;
Marquardt, H. ;
Miyagi, L. ;
Lin, F. ;
Speziale, S. ;
Merkel, S. ;
Buchen, J. ;
Kurnosov, A. ;
Liermann, H. -P. .
EARTH AND PLANETARY SCIENCE LETTERS, 2018, 489 :251-257
[110]   In situ investigation of MgO nanocube deformation at room temperature [J].
Issa, I. ;
Amodeo, J. ;
Rethore, J. ;
Joly-Pottuz, L. ;
Esnouf, C. ;
Morthomas, J. ;
Perez, M. ;
Chevalier, J. ;
Masenelli-Varlot, K. .
ACTA MATERIALIA, 2015, 86 :295-304