Coatings on Ti6A14V as palliatives for fretting fatigue in cryogenic environment

被引:13
作者
Caron, I.
Gras, R.
Ganne, T.
De Monicault, J. M.
机构
[1] Inst Super Mecan Paris, LISMMA, EA2336, F-93407 St Ouen, France
[2] SNECMA Moteurs, Div Moteur Fusees, F-27208 Vernon, France
关键词
fretting fatigue; Ti6A14V; coatings; cryogenic environment;
D O I
10.1016/j.triboint.2006.02.016
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Fretting.. also known as small oscillatory sliding motion, can lead to catastrophic failure in industrial applications. To reduce the damage caused by fretting increasing use has been made of surfaces treatments. These treatments result in multilayer solids (coating, diffusion layer...). The understandings of fretting fatigue have enabled us to evaluate the fretting resistance of homogeneous and coated materials. The experimental part is associated to a numerical one to obtain cracking threshold of the coated materials to obtain lifetime evaluation. This present study seeks to compare the behaviour of bare substrate and coated substrate submitted to fretting and evaluates the improvement of the fretting fatigue strength. (c) 2006 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1045 / 1051
页数:7
相关论文
共 11 条
[1]  
AUDRAIN V, 1992, 3 EUR C RES STRESS F
[2]  
CARON I, 2000, THESIS U ORLEANS
[3]  
CARON I, 1998, 17 JOURN PRINT SF2M
[4]   A multiaxial fatigue analysis of fretting contact taking into account the size effect [J].
Fouvry, S ;
Kapsa, P ;
Vincent, L .
FRETTING FATIGUE: CURRENT TECHNOLOGY AND PRACTICES, 2000, 1367 :167-182
[6]  
Hertz H., 1882, J. Reine Angew. Math, V92, P156, DOI DOI 10.1515/CRLL.1882.92.156
[7]   A machine for fretting fatigue and fretting wear testing in cryotechnical and normal environment [J].
Koenen, A ;
Virmoux, P ;
Gras, R ;
Blouet, J ;
Dewulf, JM ;
DeMonicault, JM .
WEAR, 1996, 197 (1-2) :192-196
[8]  
KOENEN A, 1995, THESIS ECOLE NATL SU
[9]  
MINDLIN RD, 1949, J APPL MECH-T ASME, V16, P259
[10]  
VANDANG, 1973, SUR RESISTANCE FATIG