Deformation and strength of Ti-6Al-4V alloyed with B at cryogenic temperatures

被引:40
作者
Singh, Gaurav [1 ]
Bajargan, Govind [1 ,2 ]
Datta, Ranjan [3 ]
Ramamurty, Upadrasta [1 ,3 ,4 ]
机构
[1] Indian Inst Sci, Dept Mat Engn, Bangalore 560012, Karnataka, India
[2] Vikram Sarabhai Space Ctr, Light Alloy Div, Trivandrum 695022, Kerala, India
[3] JNCASR, Int Ctr Mat Sci, Bangalore 560064, Karnataka, India
[4] King Abdulaziz Univ, Ctr Excellence Adv Mat Res, Jeddah 21589, Saudi Arabia
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2014年 / 611卷
关键词
Titanium alloys; Cryogenic temperature; Plastic deformation; Twinning; Microstructure refinement; CYCLE FATIGUE PROPERTIES; CAST TITANIUM-ALLOYS; MECHANICAL-PROPERTIES; PLASTIC-DEFORMATION; TENSILE PROPERTIES; BORON ADDITION; GRAIN-SIZE; 20; K; SINGLE-CRYSTALS; PM TI-6AL-4V;
D O I
10.1016/j.msea.2014.05.075
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Plastic deformation and strength of Ti-6Al-4V (Ti64) alloyed with minor additions of B at cryogenic temperatures were investigated through unnotched and notched tensile tests at 20 and 77 K Marked microstructural refinement that occurs with the trace addition of B to Ti64 was exploited for examining the role of microstructural length scales on the cryogenic plastic deformation. The tensile tests were complemented with detailed microstructural characterisation using transmission electron microscopy and electron back scattered diffraction imaging of the deformed specimens. Experimental results show that the addition of 0.30 wt% and above of B to Ti64 reduces ductility, and in turn enhances the notch sensitivity to the extent that those alloys become unsuitable for low temperature applications. However, the addition of similar to 0.10 wt% B is beneficial in enhancing the low temperature strength. An examination of the yield strength variation at various temperatures reveals that at 77 K, the colony size determines the yield strength of the alloy, just as it does at room temperature; implying dislocation-mediated plasticity continues to dominate up to 77 K At 20 K however, twinning dominates the flow response, with the activation of {11 (2) over bar1} and {5 (6) over bar1 (3) over bar} twinning in addition to {10 (1) over bar2} in the base alloy resulting in enhanced ductility of it as compared to either B-modified alloys at 20 K or the base alloy itself at 77 K The observation of a reasonable correlation between the lath aspect ratio, given by the colony-to-lath thickness ratios, and yield strength variation at 20 K suggests that coarse colony size in the base alloy allows for the activation of additional twinning mechanisms. (C) 2014 Elsevier B.V. All rights reserved.
引用
收藏
页码:45 / 57
页数:13
相关论文
共 64 条
  • [1] AKHTAR A, 1975, METALL TRANS, VA 6, P1105, DOI 10.1007/BF02661366
  • [2] Role of interphases in the deformation mechanisms of an α/β titanium alloy at 20 K
    Ambard, A
    Guétaz, L
    Louchet, F
    Guichard, D
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 319 : 404 - 408
  • [3] [Anonymous], AM SOC TEST MATS
  • [4] [Anonymous], 1996, E1450 ASTM
  • [5] SUBZERO TENSILE PROPERTIES OF 7010-ALUMINUM ALLOY AND TI-6A1-4V AND IMI550 TITANIUM-ALLOYS IN SHEET FORM
    BINNING, MS
    PARTRIDGE, PG
    [J]. CRYOGENICS, 1984, 24 (02) : 97 - 105
  • [6] The Elevated-Temperature Creep Behavior of Boron-Modified Ti-6Al-4V Alloys
    Boehlert, C. J.
    Chen, W.
    [J]. MATERIALS TRANSACTIONS, 2009, 50 (07) : 1690 - 1703
  • [7] Boyer R, 1994, MAT PROPERTIES HDB T, P68
  • [8] On the process of transition of the cubic-body-centered modification into the hexagonal-close-packed modification of zirconium
    Burgers, WG
    [J]. PHYSICA, 1934, 1 : 561 - 586
  • [9] Elevated-Temperature Mechanical Behavior of As-Cast and Wrought Ti-6Al-4V-1B
    Chen, W.
    Boehlert, C. J.
    Howe, J. Y.
    Payzant, E. A.
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2011, 42A (10): : 3046 - 3061
  • [10] Chernetsov VI, 1959, MET SCI HEAT TREAT M, V1, P29