Texture evolution of cold-rolled Zr-1Sn-0.3Nb-0.3Fe-0.1Cr alloy during annealing

被引:17
|
作者
Chen, Jing [1 ,2 ]
Jiang, Yilan [1 ,2 ]
Liu, Huiqun [1 ,2 ]
Yi, Danqing [1 ,2 ]
Zhang, Ruiqian [3 ,4 ]
Dai, Xun [3 ,4 ]
Liu, Shaoqiang [3 ,4 ]
机构
[1] Cent S Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R China
[2] Cent S Univ, State Key Lab Powder Met, Changsha 410083, Hunan, Peoples R China
[3] Nucl Power Inst China, Chengdu 610213, Sichuan, Peoples R China
[4] Sci & Technol Reactor Fuel & Mat Lab, Chengdu 610213, Sichuan, Peoples R China
基金
中国国家自然科学基金;
关键词
Zr alloy; Critical deformation; Texture; Cold-rolled; Annealing; ABNORMAL GRAIN-GROWTH; ZIRCONIUM SINGLE-CRYSTALS; COMMERCIALLY PURE ZR; RECRYSTALLIZATION BEHAVIOR; ZIRCALOY-4; ALLOY; SCHMID FACTORS; HEAT-TREATMENT; NB; DEFORMATION; MICROSTRUCTURE;
D O I
10.1016/j.jnucmat.2019.06.038
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
We herein report our investigation into the influence of cold-rolling on the recrystallization texture of the Zr-lSn-0.3Nb-0.3Fe-0.1Cr alloy during annealing. The as-received plates were cold-rolled at 25 degrees C with different reductions of 6, 10, 14, 18, 30, 40, 50 and 70%. All cold-rolled sheets were annealed at 580 degrees C for 3 h, while 14 and 30% cold-rolled samples were also annealed at 580 degrees C for 12 h. The microstructures of the annealed samples were characterized by scanning electron microscopy (SEM) and electron backscatter diffraction (EBSD). Abnormal grains growth with about 23 mu m in size appeared in the samples with 14% reduction and annealed at 580 degrees C for 3 h, which corresponded to the critical degree of alloy deformation. The texture of the 14% cold-rolled sheet was typical rolling texture <0001>//ND, after annealing, cold rolling texture was still retained. While the texture of the 30% cold-rolled sheet was <11<(2)over bar>0> parallel to the rolling direction (<11<(2)over bar>0>//RD), which changed to the recrystallization texture <0001>//ND, <10<(1)over bar>0>//RD and <11<(2)over bar>0>//RD characteristics after annealing. The loading direction is along the rolling direction (RD), the slip system and the Schmid factor are analyzed to more deeply understand and evaluate the plasticity of further rolling or punching. When the loading direction is along the rolling direction (RD), the predominant slip systems of annealed 14% reduction samples was prismatic and pyramidal plane system, and the annealed 30% reduction samples were prismatic with a pyramidal plane system. This implies that the use of 30% cold-rolled reduction and annealing at 580 degrees C for 12 h imparts a superior plasticity to the alloy, which may allow its application in future deformations, such as rolling or punching. (C) 2019 Elsevier B.V. All rights reserved.
引用
收藏
页码:226 / 238
页数:13
相关论文
共 50 条
  • [21] Static Recrystallization of Cold Rolled Intermetallic Fe17Al4Cr0.3Zr Alloy
    Kratochvil, P.
    Schindler, I.
    Hanus, P.
    Kral, R.
    Harcuba, P.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2012, 21 (09) : 1932 - 1936
  • [22] Recrystallization behavior of cold-rolled Zr-1Nb alloy
    Tian, Hang
    Wang, Xitao
    Gong, Weijia
    Zhou, Jun
    Zhang, Hailong
    JOURNAL OF NUCLEAR MATERIALS, 2015, 456 : 321 - 328
  • [23] Precise determination of the α → α+β phase transformation temperature of Zr-1.0Sn-0.3Nb-0.3Fe alloy
    QIU RiSheng
    LUAN BaiFeng
    CHAI LinJiang
    ZHANG XiYan
    LIU Qing
    Science China(Technological Sciences) , 2013, (01) : 60 - 65
  • [24] Precise determination of the α→α+β phase transformation temperature of Zr-1.0Sn-0.3Nb-0.3Fe alloy
    RiSheng Qiu
    BaiFeng Luan
    LinJiang Chai
    XiYan Zhang
    Qing Liu
    Science China Technological Sciences, 2013, 56 : 60 - 65
  • [25] Precise determination of the α → α+β phase transformation temperature of Zr-1.0Sn-0.3Nb-0.3Fe alloy
    QIU RiSheng
    LUAN BaiFeng
    CHAI LinJiang
    ZHANG XiYan
    LIU Qing
    Science China(Technological Sciences), 2013, 56 (01) : 60 - 65
  • [26] Texture evolution and mechanical anisotropy of cold-rolled Zr-4 alloy tube after recrystallization annealing
    Cui, Changxing
    Li, Yanchao
    Wang, Feng
    Jiao, Benqi
    Huang, Li
    Zhang, Wen
    Zhou, Lian
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2023, 110
  • [27] Effects of annealing on the microstructures and mechanical properties of biomedical cold-rolled Ti-Nb-Zr-Mo-Sn alloy
    Dai, Shijuan
    Wang, Yu
    Chen, Feng
    MATERIALS CHARACTERIZATION, 2015, 104 : 16 - 22
  • [28] Recrystallization behaviour during annealing of cold-rolled Cu-5Fe-2Sn alloy
    Zhang, Jun ting
    Lin, Jinbao
    Wang, Qianqian
    Du, Xiu li
    Wang, You hong
    MATERIALS SCIENCE AND TECHNOLOGY, 2020, 36 (11) : 1162 - 1168
  • [29] Microstructure of Zr-0.8Sn-1Nb-0.3Fe Zr Alloys
    Liu Chenwei
    Ran Guang
    Lei Penghui
    Liu Tengjiao
    Zhang Ruiqian
    Shang Jiacheng
    RARE METAL MATERIALS AND ENGINEERING, 2016, 45 (12) : 3313 - 3318
  • [30] Annealing texture of a cold-rolled Fe-Mn-Al-Si-C alloy
    Bhattacharya, Basudev
    Ray, Ranjit Kumar
    PHILOSOPHICAL MAGAZINE, 2015, 95 (27) : 3002 - 3013