Effect of Severe Plastic Deformation on Structure and Properties of Al-Sc-Ta and Al-Sc-Ti Alloys

被引:12
|
作者
Berezina, Alla [1 ]
Monastyrska, Tetiana [1 ]
Davydenko, Olexandr [2 ]
Molebny, Oleh [1 ]
Polishchuk, Sergey [1 ]
机构
[1] Natl Acad Sci Ukraine, GV Kurdyumov Inst Met Phys, 36 Acad Vernadsky Blvd,Kyiv 142, UA-03680 Kiev, Ukraine
[2] Natl Acad Sci Ukraine, OO Galkin Donetsk Inst Phys & Engn, 46 Prospect, UA-03039 Kiev, Ukraine
来源
NANOSCALE RESEARCH LETTERS | 2017年 / 12卷
关键词
Al-Sc alloy; Severe plastic deformation; Hydrostatic extrusion; Equal-channel angular hydroextrusion; Dynamic recrystallization; Disclinations; Deformation bands; Low-angle and high-angle boundaries; Aging; Supersaturated solid solution; CHANNEL ANGULAR EXTRUSION; TEXTURE EVOLUTION; MICROSTRUCTURE;
D O I
10.1186/s11671-017-1995-y
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The comparative analysis of the effect of monotonous and non-monotonous severe plastic deformations (SPD) on the structure and properties of aluminum alloys has been carried out. Conventional hydrostatic extrusion (HE) with a constant deformation direction and equal-channel angular hydroextrusion (ECAH) with an abrupt change in the deformation direction were chosen for the cases of monotonous and non-monotonous SPD, respectively. Model cast hypoeutectic Al-0.3%Sc alloys and hypereutectic Al-0.6%Sc alloys with Ta and Ti additives were chosen for studying. It was demonstrated that SPD of the alloys resulted in the segregation of the material into active and inactive zones which formed a banded structure. The active zones were shown to be bands of localized plastic deformation. The distance between zones was found to be independent of the accumulated strain degree and was in the range of 0.6-1 mu m. Dynamic recrystallization in the active zones was observed using TEM. The dynamic recrystallization was accompanied by the formation of disclinations, deformation bands, low-angle, and high-angle boundaries, i.e., rotational deformation modes developed. The dynamic recrystallization was more intense during the non-monotonous deformation as compared with the monotonous one, which was confirmed by the reduction of texture degree in the materials after ECAH.
引用
收藏
页数:9
相关论文
共 50 条
  • [1] Effect of Severe Plastic Deformation on Structure and Properties of Al-Sc-Ta and Al-Sc-Ti Alloys
    Alla Berezina
    Tetiana Monastyrska
    Olexandr Davydenko
    Oleh Molebny
    Sergey Polishchuk
    Nanoscale Research Letters, 2017, 12
  • [2] Formation of Metastable Aluminides in Al-Sc-Ti (Zr, Hf) Cast Alloys
    Popova, E.
    Kotenkov, P.
    Shubin, A.
    Gilev, I.
    METALS AND MATERIALS INTERNATIONAL, 2020, 26 (10) : 1515 - 1523
  • [3] Effect of annealing on the structure and properties of Al–Li–Cu–Zr–Sc–Ag alloy subjected to severe plastic deformation
    L. I. Kaigorodova
    D. Yu. Rasposienko
    V. G. Pushin
    V. P. Pilyugin
    S. V. Smirnov
    The Physics of Metals and Metallography, 2015, 116 : 932 - 941
  • [4] Effect of annealing on the structure and properties of Al-Li-Cu-Zr-Sc-Ag alloy subjected to severe plastic deformation
    Kaigorodova, L. I.
    Rasposienko, D. Yu.
    Pushin, V. G.
    Pilyugin, V. P.
    Smirnov, S. V.
    PHYSICS OF METALS AND METALLOGRAPHY, 2015, 116 (09) : 932 - 941
  • [5] Influence of Severe Plastic Deformation on the Structure and Properties of Al–Li–Cu–Mg–Zr–Sc–Zn Alloy
    L. I. Kaigorodova
    D. Yu. Rasposienko
    V. G. Pushin
    V. P. Pilyugin
    S. V. Smirnov
    Physics of Metals and Metallography, 2018, 119 : 161 - 168
  • [6] Assessments of Sc-Containing Ternary Systems Al-Sc-Ti and Al-Sc-Zr Within the Thermodynamic Database for Aluminium Alloys, TCAL5
    Chen, Hai-Lin
    Chen, Qing
    Mason, Paul
    LIGHT METALS 2018, 2018, : 347 - 353
  • [7] Influence of Severe Plastic Deformation on the Structure and Properties of Al-Li-Cu-Mg-Zr-Sc-Zn Alloy
    Kaigorodova, L. I.
    Rasposienko, D. Yu.
    Pushin, V. G.
    Pilyugin, V. P.
    Smirnov, S. V.
    PHYSICS OF METALS AND METALLOGRAPHY, 2018, 119 (02) : 161 - 168
  • [8] Al3(Sc,Zr)-based precipitates in Al-Mg alloy: Effect of severe deformation
    Buranova, Yu.
    Kulitskiy, V.
    Peterlechner, M.
    Mogucheva, A.
    Kaibyshev, R.
    Divinski, S. V.
    Wilde, G.
    ACTA MATERIALIA, 2017, 124 : 210 - 224
  • [9] Precipitation strengthening in Al (Sc,Ti) alloys
    van Dalen, ME
    Dunand, DC
    Seidman, DN
    AFFORDABLE METAL MATRIX COMPOSITES FOR HIGH-PERFORMANCE APPLICATIONS II, 2003, : 195 - 201
  • [10] Effect of cold plastic deformation and subsequent aging on the strength properties of Al-Mg2Si alloys with combined (Sc plus Zr) and (Sc plus Hf) additions
    Bochvar, N. R.
    Rybalchenko, O. V.
    Leonova, N. P.
    Tabachkova, N. Yu.
    Rybalchenko, G. V.
    Rokhlin, L. L.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 821