Deuterium retention in V-4Cr-4Ti alloy after deuterium ion irradiation

被引:14
作者
Yamauchi, Y
Yamada, T
Hirohata, Y
Hino, T
Muroga, T
机构
[1] Hokkaido Univ, Dept Nucl Engn, Kita Ku, Sapporo, Hokkaido 0608628, Japan
[2] Natl Inst Fus Sci, Toki 5095292, Japan
关键词
D O I
10.1016/j.jnucmat.2004.04.081
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The deuterium retention properties of vanadium alloy, V-4Cr-4Ti, were investigated by thermal desorption spectroscopy after deuterium ion irradiation. The deuterium ion irradiation was carried out at 380, 573 and 773 K with ion energy of 1.7 keV. Deuterium retained in the sample was desorbed in the forms of D-2, HD, HDO and D2O. The amount of retained deuterium at 380 K increased with the ion fluence, and did not saturate to a fluence up to 1 x 10(19) D/cm(2). In addition, more than 100% of implanted D was retained at high deuterium fluence. The retained amount at 380 K was one and two orders of magnitude larger than graphite and tungsten, respectively. For the irradiation at 773 K, the amount of retained deuterium decreased with increase in ion fluence in the high fluence region, and the retained amount was almost the same as that for graphite or tungsten. (C) 2004 Elsevier B.V. All rights reserved.
引用
收藏
页码:397 / 400
页数:4
相关论文
共 14 条
  • [1] LOW ACTIVATION MATERIALS FOR FUSION APPLICATIONS
    BLOOM, EE
    CONN, RW
    DAVIS, JW
    GOLD, RE
    LITTLE, R
    SCHULTZ, KR
    SMITH, DL
    WIFFEN, FW
    [J]. JOURNAL OF NUCLEAR MATERIALS, 1984, 122 (1-3) : 17 - 26
  • [2] VOID GROWTH AND THERMAL-DESORPTION OF DEUTERIUM FROM VOIDS IN TUNGSTEN
    ELEVELD, H
    VANVEEN, A
    [J]. JOURNAL OF NUCLEAR MATERIALS, 1994, 212 : 1421 - 1425
  • [3] Tritium inventory of carbon dust in ITER
    Hino, T
    Yoshida, H
    Yamauchi, Y
    Hirohata, Y
    Nakamura, K
    Akiba, M
    [J]. FUSION ENGINEERING AND DESIGN, 2002, 61-62 : 605 - 609
  • [4] Suppression of hydrogen absorption to V-4Cr-4Ti alloy by TiO2/TiC coating
    Hirohata, Y
    Motojima, D
    Hino, T
    Sengoku, S
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2003, 313 : 172 - 176
  • [5] Deuterium retention of V-4Cr-4Ti alloy exposed to the JFT-2M tokamak environment
    Hirohata, Y
    Oda, T
    Hino, T
    Sengoku, S
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2001, 290 (290-293) : 196 - 200
  • [6] HIROHATA Y, 1987, JPN J VAC SOC, V33, P34
  • [7] *IAEA, 2000, ITER EDA DOC SER, V19
  • [8] NIFS program for large ingot production of a V-Cr-Ti alloy
    Muroga, T
    Nagasaka, T
    Iiyoshi, A
    Kawabata, A
    Sakurai, S
    Sakata, M
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2000, 283 (283-287) : 711 - 715
  • [9] SURFACE-LIMITED RELEASE OF DEUTERIUM FROM IRON
    WAMPLER, WR
    [J]. JOURNAL OF NUCLEAR MATERIALS, 1987, 145 : 313 - 316
  • [10] SATURATION OF DEUTERIUM RETENTION IN CARBON A NEW CALIBRATION FOR PLASMA EDGE PROBES
    WAMPLER, WR
    BRICE, DK
    MAGEE, CW
    [J]. JOURNAL OF NUCLEAR MATERIALS, 1981, 102 (03) : 304 - 312