Characteristics of Al alloy surface after EDC with sintered Ti electrode and TiN powder additive

被引:24
|
作者
Chen, Hsin-Jen [1 ]
Wu, Kun-Ling [2 ]
Yan, Biing-Hwa [1 ]
机构
[1] Natl Cent Univ, Dept Mech Engn, Jhongli 32054, Taiwan
[2] Tungnan Univ, Dept Mech Engn, New Taipei City 222, Taiwan
关键词
Electrical discharge coating (EDC); Wet; Dry; Ti; TiC; TiN; Coefficient of friction (COF); Spallation resistance; METAL BIPOLAR PLATES; DISCHARGE; RATIO;
D O I
10.1007/s00170-014-5669-y
中图分类号
TP [自动化技术、计算机技术];
学科分类号
0812 ;
摘要
Electrical discharge coating (EDC) performs not only machining but also surface modification of workpiece by changing the polarity of the electrode and dielectric medium. As a candidate of metal bipolar plate in proton exchange membrane fuel cell application, machined Al alloy needs surface coating to overcome its poor corrosion resistance. The goal of this study was to investigate the coating characteristics of 6061-T6 aluminum (Al) alloy machined using titanium (Ti)-sintered electrodes in wet and dry EDC. The results show that in wet EDC using cathodic T-8 sintered electrode, both material removal rate (MRR) and tool wear rate (TWR) were kept reasonably low. Discharge current (I (p)) and pulse duration (T (on)) are the main determinants of the morphology of the EDCed Al alloy surface. The appropriate parameters for wet EDC are found to be 1 A < I (p) < 8 A and 9 mu s < T (on) < 100 mu s at DF = 27 %. Adding TiN powder to kerosene not only improved the EDCed surface quality but also decreased the coefficient of friction. The formation of a TiC layer on the machined surface prolonged the onset of friction transition, which would in turn enhance the wear resistance of the machined surface. However, no TiN layer was formed during wet EDC. On the other hand, in dry EDC using anodic T-6 and T-8 sintered electrodes, both MRR and TWR were below zero. A pure TiN layer of 20-mu m thickness was deposited on the EDCed surface and featured good spallation resistance. The appropriate dry EDC parameters for forming a pure TiN layer on a workpiece surface are found to be 1 A < I (p) < 30 A and 6 mu s < T (on) < 72 mu s at DF = 16 %. From the experimental results of this study, the application of EDC to surface modification during fabrication of the fluid pattern on an Al metal bipolar plate can be expected.
引用
收藏
页码:319 / 332
页数:14
相关论文
共 50 条
  • [21] Hydrogen embrittlement of Ti-6Al-4V alloy with surface modification by TiN coating
    Yilbas, BS
    Coban, A
    Kahraman, R
    Khaled, MM
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 1998, 23 (06) : 483 - 489
  • [22] Corrosion and hardness characteristics of Ti/TiN-modified Ti6Al4V alloy in marine environment
    Lin, Liyang
    Tian, Yuanhao
    Yu, Wenxing
    Chen, Susu
    Chen, Yafei
    Chen, Wei
    CERAMICS INTERNATIONAL, 2022, 48 (23) : 34848 - 34854
  • [23] Characteristics of hydrogen storage alloy electrode with cupric oxide additive
    Zhang, Sen
    Shi, Pengfei
    Deng, Chao
    SOLID STATE IONICS, 2006, 177 (13-14) : 1193 - 1197
  • [24] Influence of Powder Characteristics on Formation of Porosity in Additive Manufacturing of Ti-6Al-4V Components
    Maurizio Iebba
    Antonello Astarita
    Daniela Mistretta
    Ivano Colonna
    Mariacira Liberini
    Fabio Scherillo
    Carmine Pirozzi
    Rosario Borrelli
    Stefania Franchitti
    Antonino Squillace
    Journal of Materials Engineering and Performance, 2017, 26 : 4138 - 4147
  • [25] Influence of Powder Characteristics on Formation of Porosity in Additive Manufacturing of Ti-6Al-4V Components
    Iebba, Maurizio
    Astarita, Antonello
    Mistretta, Daniela
    Colonna, Ivano
    Liberini, Mariacira
    Scherillo, Fabio
    Pirozzi, Carmine
    Borrelli, Rosario
    Franchitti, Stefania
    Squillace, Antonino
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (08) : 4138 - 4147
  • [26] The Changes of Rheological Behavior of Ti-6Al-4V Alloy Powders for Additive Manufacturing by Powder Oxidation
    Kakegawa, Naoki
    Zhou, Weiwei
    Nomura, Naoyuki
    Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 2025, 72
  • [27] Effect of milling time on powder characteristics and mechanical performance of Ti4wt%Al alloy
    Singh, Pradeep
    Abhash, Amit
    Yadav, B. N.
    Shafeeq, M.
    Singh, I. B.
    Mondal, D. P.
    POWDER TECHNOLOGY, 2019, 342 : 275 - 287
  • [28] A study on the electrode characteristics of V-Ti alloy surface-modified by ballmilling process
    Kim, SH
    Lee, SM
    Lee, PS
    Lee, JY
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2001, 148 (07) : A696 - A700
  • [29] Research on sintered behavior and structure performance of Ti-NdAl alloy for powder metallurgy
    Tang, HP
    Liu, Y
    Huang, BY
    Liu, HY
    Huang, YP
    RARE METAL MATERIALS AND ENGINEERING, 2004, 33 (12) : 1270 - 1273
  • [30] Surface Characteristics of Ti-6Al-4V Alloy Based on the Process Parameter and Abrasive Process in the Laser Powder Bed Fusion
    Kim, Won Yeong
    Yoon, Eun Yoo
    Kim, Ji Hoon
    Kim, Sangwoo
    METALS AND MATERIALS INTERNATIONAL, 2023, 29 (08) : 2345 - 2357