Joining high volume fraction SiC particle reinforced aluminum matrix composites (SiCp/Al) by low melting point stannous oxide-zinc oxide-phosphorus pentoxide glass

被引:20
作者
Guo, Wei [1 ,2 ,3 ]
Hou, Jing [1 ]
Lin, Tiesong [2 ]
He, Peng [2 ]
机构
[1] Northwestern Polytech Univ, Sch Mat Sci & Engn, Xian 710072, Peoples R China
[2] Harbin Inst Technol, State Key Lab Adv Welding & Joining, Harbin 150001, Peoples R China
[3] Nanyang Technol Univ, Sch Mat Sci & Engn, Singapore 639798, Singapore
基金
中国博士后科学基金;
关键词
Joining; Brazing; Phosphate glass; High volume fractions SiCp/Al composites; Shear strength; BRAZING FILLER METAL; CRYSTALLIZATION BEHAVIOR; MECHANICAL-PROPERTIES; MICROSTRUCTURE; WETTABILITY; PLATES; MMC;
D O I
10.1016/j.ceramint.2020.09.259
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
This study focused on joining high volume fraction SiC particles reinforced aluminum matrix composites (55 vol % SiCp/Al) with 50SnO-20ZnO-30P(2)O(5) (SZP) glass directly in air. Prior to joining, various properties of the SZP glass and its wettability on the composites were investigated. The results showed that the coefficient of thermal expansion of the glass was 10.58 x 10(-6)/degrees C (20-369 degrees C), which closely match with 55 vol% SiCp/Al composites. The glass transition, crystallization, and softening temperature were identified to be 369, 397, and 486 degrees C, respectively. Subsequent wetting tests confirmed excellent wettability of the glass on the composites. The joint exhibited sound bonding that was free of defects when brazed at 550 degrees C for 10 min Zn2P2O7 was formed adjacent to the composites due to the crystallization of the glass. The mechanical properties of the joint were proven to be suitable, exhibiting an average shear strength of 55.3 MPa.
引用
收藏
页码:3955 / 3963
页数:9
相关论文
共 41 条
[1]   Application of Nd2O3-Al2O3-SiO2 glass solder for joining of silicon carbide components [J].
Ahmad, S. ;
Herrmann, M. ;
Mahmoud, M. M. ;
Lippmann, W. ;
Hurtado, A. ;
Seifert, H. J. .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2016, 36 (07) :1559-1569
[2]   Effect of process parameters on bead properties of A359/SiC MMCs welded by laser [J].
Bassani, Paola ;
Capello, Edoardo ;
Colombo, Daniele ;
Previtali, Barbara ;
Vedani, Maurizio .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2007, 38 (04) :1089-1098
[3]  
Bourhis EL, 2014, Glass: Mechanics and Technology
[4]   Structural properties of Er3+ doped lead zinc phosphate glasses [J].
Chowdhury, Swarup ;
Mandal, Pabitra ;
Ghosh, Subhankar .
MATERIALS SCIENCE AND ENGINEERING B-ADVANCED FUNCTIONAL SOLID-STATE MATERIALS, 2019, 240 :116-120
[5]   Friction stir welding of thick plates of aluminum alloy matrix composite with a high volume fraction of ceramic reinforcement [J].
Cioffi, F. ;
Fernandez, R. ;
Gesto, D. ;
Rey, P. ;
Verdera, D. ;
Gonzalez-Doncel, G. .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2013, 54 :117-123
[6]   Aging behavior of high volume fraction SiCp/Al composites fabricated by pressureless infiltration [J].
Cui, Yan ;
Jin, Tingzhu ;
Cao, Leigang ;
Liu, Fengbin .
JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 681 :233-239
[7]   Wetting of ceramics by molten silicon and silicon alloys: a review [J].
Drevet, Beatrice ;
Eustathopoulos, Nicolas .
JOURNAL OF MATERIALS SCIENCE, 2012, 47 (24) :8247-8260
[8]   New design of sapphire joints brazed with bismuth-borate glass [J].
Guo, Wei ;
Fu, Li ;
Lin, Tiesong ;
He, Peng ;
Wang, Chunyue ;
Wang, Tong ;
Liu, Hongzhi .
CERAMICS INTERNATIONAL, 2019, 45 (04) :5036-5049
[9]   Microstructure evolution during air bonding of Al2O3 to Al2O3 joints using bismuth-borate-zinc glass [J].
Guo, Wei ;
Lin, Tiesong ;
Wang, Tong ;
He, Peng ;
Sekulic, D. P. ;
Guo, Shu .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2017, 37 (13) :4015-4023
[10]  
[何鹏 He Peng], 2016, [材料工程, Journal of Materials Engineering], V44, P123