Effect of Bonding Time on Dissimilar Transient Liquid Phase (TLP) Bonding of IN939 to IN625 Superalloys: Microstructural Characterization and Mechanical Properties

被引:16
作者
Sadeghian, Amirhossein [1 ,2 ]
Mirsalehi, Seyyed Ehsan [2 ]
Arhami, Farzam [2 ,3 ]
Malekan, Ahmad [4 ]
Saito, Noritaka [5 ]
Nakashima, Kunihiko [5 ]
机构
[1] Coventry Univ, Inst Future Transport & Cities, Coventry CV1 5FB, W Midlands, England
[2] Amirkabir Univ Technol, Tehran Polytech, Dept Mat & Met Engn, Tehran 158754413, Iran
[3] Concordia Univ, Dept Mech Ind & Aerosp Engn MIAE, Montreal, PQ H3G 1M8, Canada
[4] Mat & Energy Res Ctr, Ceram Div, Tehran 141554777, Iran
[5] Kyushu Univ, Dept Mat Sci & Engn, Nishi Ku, 744 Motooka, Fukuoka 8190395, Japan
来源
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE | 2021年 / 52卷 / 04期
关键词
ISOTHERMAL SOLIDIFICATION COMPLETION; HEAT-TREATMENT; EVOLUTION; TEMPERATURE; BEHAVIOR; INTERLAYER; SILICON; JOINTS;
D O I
10.1007/s11661-021-06176-x
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The microstructure and mechanical properties of transient liquid phase (TLP) bonded joints between dissimilar precipitation hardened IN939 and solid solution hardened IN625 with a Ni-Cr-Si-Fe-B filler alloy were studied. The TLP bonding was conducted in different bonding times (i.e., 15, 25, 35, 45, 60, and 90 minutes). Different phases, formed in the isothermally solidified zone (ISZ), on-cooling solidified zone, and diffusion affected zone (DAZ), were characterized using EDS, XRD, and EPMA analyses. A Ni-rich gamma solid solution, CrB, and Ni3B were detected in the centerline of samples with incomplete isothermal solidification (i.e., 15 and 25 minutes), formed by binary and ternary eutectic reactions. Raising the time of bonding boosted isothermal solidification, resulting in a joint without deleterious eutectic microconstituents in bonding times of 35 minutes and higher. Chromium-rich borides were discovered in the DAZ of IN939, while the IN625-DAZ side was composed of chromium-molybdenum-rich borides. The concentration of alloying elements in the ISZ experienced an increment by further raising the bonding time to 90 minutes, creating a more homogenous bond with increased ISZ microhardness and mechanical properties. The highest shear strength (similar to 92 and similar to 77 Pct that of the IN939 and IN625, respectively) and failure energy were attained for the 90-minutes sample. The fracture mechanism was also switched from a brittle semi-cleave morphology to a more ductile dimple-like morphology by increasing the bonding time from 15- to 90-minutes.
引用
收藏
页码:1526 / 1539
页数:14
相关论文
共 50 条
  • [31] Effect of two-step heating process on joint microstructure and properties during transient liquid phase bonding of dissimilar materials
    Wang, Xuegang
    Li, Xingeng
    Wang, Chengguo
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 560 : 711 - 716
  • [32] Effect of bonding time on microstructure and mechanical properties of transient liquid phase bonded magnesium AZ31 alloy
    Jin, Y. J.
    Khan, T. I.
    MATERIALS & DESIGN, 2012, 38 : 32 - 37
  • [33] Evolution of microstructure and mechanical properties on dissimilar transient liquid phase (TLP) bonding of GTD-111 and IN-718 by BNi-9 (AWS A5.8/A5.8M) interlayer
    Ghahferokhi, Ali Izadi
    Kasiri-Asgarani, Masoud
    Amini, Kamran
    Ebrahimi-kahrizsangi, Reza
    Rafiei, Mahdi
    WELDING IN THE WORLD, 2021, 65 (02) : 329 - 343
  • [34] Effect of bonding temperature on microstructure and shear strength of the dissimilar Al/Al-27Si joints bonded by partial transient liquid phase bonding
    Xu, Lei
    Wang, Haibo
    Sun, Qingzhu
    Wan, Weicai
    Chen, Hongsheng
    JOURNAL OF MANUFACTURING PROCESSES, 2019, 41 : 297 - 306
  • [35] Effect of powders on microstructures and mechanical properties for Sn-Ag transient liquid phase bonding in air
    Bao, Yudian
    Wu, Aiping
    Shao, Huakai
    Zhao, Yue
    Zou, Guisheng
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2018, 29 (12) : 10246 - 10257
  • [36] On the Effect of Liquid-State Diffusion on Isothermal Solidification Completion Time During Transient Liquid-Phase Bonding of Dissimilar Materials
    Ojo, O. A.
    Aina, O.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2018, 49A (05): : 1481 - 1485
  • [37] Hot corrosion mechanism in transient liquid phase bonded HX superalloy: Effect of bonding time
    Bakhtiari, H.
    Farvizi, M.
    Rahimipour, M. R.
    Malekan, A.
    JOURNAL OF ADVANCED JOINING PROCESSES, 2025, 11
  • [38] Joint formation and mechanical properties of ultrasonic-assisted transient liquid bonding of dissimilar Al/Mg with a Zn interlayer in air
    Liu, Xuesong
    Li, Zhengwei
    Xu, Zhiwu
    Chen, Shu
    Peng, Liming
    Yan, Jiuchun
    JOURNAL OF MANUFACTURING PROCESSES, 2022, 77 : 632 - 641
  • [39] Microstructural characteristics and mechanical response of transient liquid-phase diffusion bonding AlCoCrFeNi2.1 high entropy alloy utilizing BNi-5 interlayer
    Guo, Zilong
    Li, Zhaoxi
    Guo, Wei
    Guo, Yi
    Li, Jinglong
    Xiong, Jiangtao
    JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 1009
  • [40] Effect of Bonding Time, Composition of Interlayer, and Postbond Heat Treatment on Transient Liquid Phase Joints of Inconel 718 Superalloy
    Chen, Shiqi
    Liu, Guangyin
    Li, Hanbing
    Yang, Liu
    Zhang, Xiankun
    Shen, Jun
    ADVANCED ENGINEERING MATERIALS, 2024, 26 (15)