Growth-rate Enhancement of High-quality, Low-loss CVD-produced Diamond Disks Grown for Microwave Windows Application

被引:24
作者
Bogdanov, Sergey [1 ]
Vikharev, Anatoly [1 ]
Gorbachev, Aleksei [1 ]
Muchnikov, Anatoly [1 ]
Radishev, Dmitry [1 ]
Ovechkin, Nikolai [1 ]
Parshin, Vladimir [1 ]
机构
[1] RAS, Inst Appl Phys, Nizhnii Novgorod 603950, Russia
关键词
CVD diamond growth; Dielectric losses; Microwave window; Nitrogen addition; CHEMICAL-VAPOR-DEPOSITION; NITROGEN; FILMS; CONDUCTIVITY;
D O I
10.1002/cvde.201307058
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The effect of nitrogen addition on the growth rate, quality, and properties of polycrystalline diamond grown by microwave plasma assisted (MPA)CVD is investigated. Two series of experiments are performed at two different microwave power densities (40 and 110W cm(-3)) using a 2.45 GHz cylindrical microwave reactor. The results show that the beneficial effect of nitrogen is more distinct at higher microwave power densities. To investigate the properties of polycrystalline diamond grown with nitrogen addition, a thick diamond disk of 50mm diameter is grown with an addition of 50ppm nitrogen using a 2.45 GHz ellipsoidal microwave reactor. The grown diamond disk has a thermal conductivity of 17.3W cm(-1) K-1 and dielectric loss tangent of 3.7x10(-5) at a frequency of 170 GHz, and its parameters are suitable for application in microwave windows (e.g., gyrotron windows). Our results indicate that it is possible to achieve the increased (by a factor of 2.5) growth rates by nitrogen addition without significant degradation of diamond quality, and properties such as thermal conductivity and dielectric loss tangent. The effect of nitrogen addition on the MPACVD synthesis of polycrystalline diamond is investigated with the aim of growth-rate enhancement of high-quality, low-loss CVD-produced diamond disks. Experiments are performed at microwave power densities of 40 and 110 W cm(-3) using a 2.45 GHz microwave reactor. The amount of added nitrogen needed to grow CVD disks of high quality (suitable for application in microwave windows) 2.5 times faster compared with the nitrogen-free synthesis, is determined.
引用
收藏
页码:32 / 38
页数:7
相关论文
共 21 条
[1]   Coupled effect of nitrogen addition and surface temperature on the morphology and the kinetics of thick CVD diamond single crystals [J].
Achard, J. ;
Silva, F. ;
Brinza, O. ;
Tallaire, A. ;
Gicquel, A. .
DIAMOND AND RELATED MATERIALS, 2007, 16 (4-7) :685-689
[2]   A mechanism for crystal twinning in the growth of diamond by chemical vapour deposition [J].
Butler, James E. ;
Oleynik, Ivan .
PHILOSOPHICAL TRANSACTIONS OF THE ROYAL SOCIETY A-MATHEMATICAL PHYSICAL AND ENGINEERING SCIENCES, 2008, 366 (1863) :295-310
[3]  
Cao G. Z., 1995, APPL PHYS LETT, V68, P688
[4]   Growth of {100} textured diamond films by the addition of nitrogen [J].
Cao, GZ ;
Schermer, JJ ;
vanEnckevort, WJP ;
Elst, WALM ;
Giling, LJ .
JOURNAL OF APPLIED PHYSICS, 1996, 79 (03) :1357-1364
[5]   A molecular dynamics study of N-incorporation into carbon systems: doping, diamond growth and nitride formation [J].
Frauenheim, T ;
Jungnickel, G ;
Sitch, P ;
Kaukonen, M ;
Weich, F ;
Widany, J ;
Porezag, D .
DIAMOND AND RELATED MATERIALS, 1998, 7 (2-5) :348-355
[6]  
Funer M, 1998, APPL PHYS LETT, V72, P1149, DOI 10.1063/1.120997
[7]  
Garin B.M., 2013, RECENT ADV BROADBAND, P79
[8]   Nature of millimeter wave losses in low loss CVD diamonds [J].
Garin, BM ;
Parshin, VV ;
Myasnikova, SE ;
Ralchenko, V .
DIAMOND AND RELATED MATERIALS, 2003, 12 (10-11) :1755-1759
[9]   Measurements of thermal conductivity and thermal diffusivity of CVD diamond [J].
Graebner, JE .
INTERNATIONAL JOURNAL OF THERMOPHYSICS, 1998, 19 (02) :511-523
[10]   EFFECT OF NITROGEN ON THE GROWTH OF DIAMOND FILMS [J].
JIN, S ;
MOUSTAKAS, TD .
APPLIED PHYSICS LETTERS, 1994, 65 (04) :403-405