Natural Rubber/Styrene Butadiene Rubber/Recycled Nitrile Glove (NR/SBR/rNBRg) Ternary Blend: Curing Characteristics and Swelling Test

被引:1
作者
Yahya, Nik Zakaria Nik [1 ]
Zulkepli, Nik Noriman [1 ]
Ismail, Hanafi [2 ]
Salleh, Mohd Arif Anuar Mohd [1 ]
Santiagoo, Ragunathan [3 ]
机构
[1] Univ Malaysia Perlis, Sch Mat Engn, Ctr Excellence Geopolyrner & Green Technol CEGeoG, Kompleks Pengajian Jejawi 2, Arau 02600, Perlis, Malaysia
[2] Univ Sains Malaysia, Sch Mat & Mineral Resources Engn, Nibong Tebal 14300, Penang, Malaysia
[3] Univ Malaysia Perlis, Sch Environm Engn, Arau 02600, Perlis, Malaysia
来源
ADVANCED MATERIALS ENGINEERING AND TECHNOLOGY II | 2014年 / 594-595卷
关键词
natural rubber; styrene butadiene rubber (SBR); recycled nitrile glove (rNBRg); curing characteristics; crosslink density; ternary blend; MORPHOLOGICAL PROPERTIES; MECHANICAL-PROPERTIES; RUBBER; NBR; SBR;
D O I
10.4028/www.scientific.net/KEM.594-595.634
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Curing characteristics and swelling behavior of natural rubber/styrene butadiene rubber/recycled nitrile glove (NR/SBR/rNBRg) blends were investigated. Eleven composition ratio; 50/50/0, 50/40/10, 50/30/20, 50/20/30, 50/10/40, 50/0/50, 40/50/10, 30/50/20, 20/50/30, 10/50/40, and 0/50/50 of SMRL/SBR/rNBRg with the size of rNBRg; 2.5-3.0 cm(2) were prepared by using two roll mill at room temperature. Cure characteristics such as scorch time,t(2), cure time,t(90), minimum torque, M-L, maximum torque, M-H, and swelling behavior of SMRL/SBR/rNBRg ternary blends were examined. Results indicated that the scorch time and maximum torque of the NR/SBR/rNBRg blends decreased with increasing rNBRg content. The minimum torque of the blends increased as rNBRg content increased. The cure time of NR/SBR/rNBRg blends show a unique trend, which are depending on the domain rubber content. The increment in rNBRg content decreased the crosslink density of NR/SBR/rNBRg blends.
引用
收藏
页码:634 / +
页数:2
相关论文
共 14 条
[1]  
El-Sabbagh S.H., 2007, EGYPT J SOLIDS, V30, P157
[2]   Statistical mechanics of cross-linked polymer networks II Swelling [J].
Flory, PJ ;
Rehner, J .
JOURNAL OF CHEMICAL PHYSICS, 1943, 11 (11) :521-526
[3]   Cure wand mechanical behavior of rubber compounds containing ground vulcanizates: Part III. Tensile and tear strength [J].
Gibala, D ;
Thomas, D ;
Hamed, GR .
RUBBER CHEMISTRY AND TECHNOLOGY, 1999, 72 (02) :357-360
[4]   Fatigue and mechanical properties of NR SBR and NR NBR blend vulcanizates [J].
Ismail, MN ;
El-Sabbagh, SH ;
Yehia, AA .
JOURNAL OF ELASTOMERS AND PLASTICS, 1999, 31 (03) :255-270
[5]  
Malaysia Rubber Export Promotion Council (MREPC), 2012, AN DOUBL DIG GROWTH
[6]   DIELECTRIC INVESTIGATION OF SBR-NBR AND CR-NBR BLENDS [J].
MANSOUR, AA ;
ELSABAGH, S ;
YEHIA, AA .
JOURNAL OF ELASTOMERS AND PLASTICS, 1994, 26 (04) :367-378
[7]  
Mcdonel F. T., 1978, POLYM BLENDS, V2
[8]   Compounding, mechanical and morphological properties of carbon-black-filled natural rubber/recycled ethylene-propylene-diene-monomer (NR/R-EPDM) blends [J].
Nabil, H. ;
Ismail, H. ;
Azura, A. R. .
POLYMER TESTING, 2013, 32 (02) :385-393
[9]   Curing characteristics and mechanical and morphological properties of styrene butadiene rubber/virgin acrylonitrile-butadiene rubber (SBR/vNBR) and styrene butadiene rubber/recycled acrylonitrile-butadiene rubber (SBR/rNBR) blends [J].
Noriman, N. Z. ;
Ismail, H. ;
Rashid, Azura .
POLYMER-PLASTICS TECHNOLOGY AND ENGINEERING, 2008, 47 (10) :1016-1023
[10]   Effect of reprocessing and accelerated ageing on thermal and mechanical polycarbonate properties [J].
Perez, J. M. ;
Vilas, J. L. ;
Laza, J. M. ;
Arnaiz, S. ;
Mijangos, F. ;
Bilbao, E. ;
Rodriguez, M. ;
Leon, L. M. .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2010, 210 (05) :727-733