Fatigue failure load of two resin-bonded zirconia-reinforced lithium silicate glass-ceramics: Effect of ceramic thickness

被引:58
|
作者
Monteiro, Jaiane Bandoli [1 ]
Riquieri, Hilton [1 ]
Prochnow, Catina [2 ]
Guilardi, Luis Felipe [2 ]
Rocha Pereira, Gabriel Kalil [2 ,3 ]
Souto Borges, Alexandre Luiz [4 ]
de Melo, Renata Marques [4 ]
Valandro, Luiz Felipe [2 ]
机构
[1] Sao Paulo State Univ UNESP, Inst Sci & Technol, Sao Jose Dos Campos, SP, Brazil
[2] Univ Fed Santa Maria, Fac Odontol, Santa Maria, RS, Brazil
[3] Merid Fac IMED, Sch Dent, Passo Fundo, RS, Brazil
[4] Sao Paulo State Univ UNESP, Dept Dent Mat & Prosthodont, Inst Sci & Technol, Sao Jose Dos Campos, SP, Brazil
关键词
Dental ceramics; Fatigue; Finite element analysis; Glass ceramics; Mechanical behavior; Monolithic full-contour restorations; Staircase method; FRACTURE-RESISTANCE; FINITE-ELEMENT; LAYER STRUCTURES; DENTAL CERAMICS; STRENGTH; CROWNS; DISILICATE; OCCLUSAL; SURFACE; RESTORATIONS;
D O I
10.1016/j.dental.2018.03.004
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. To evaluate the effect of ceramic thickness on the fatigue failure load of two zirconia-reinforced lithium silicate (ZLS) glass-ceramics, adhesively cemented to a dentin analogue material. Methods. Disc-shaped specimens were allocated into 8 groups (n = 25) considering two study factors: ZLS ceramic type (Vita Suprinity VS; and Celtra Duo CD), and ceramic thickness (1.0; 1.5; 2.0; and 2.5 mm). A trilayer assembly (0 = 10 mm; thickness = 3.5 mm) was designed to mimic a bonded monolithic restoration. The ceramic discs were etched, silanized and luted (Variolink N) into a dentin analogue material. Fatigue failure load was determined using the Staircase method (100,000 cycles at 20 Hz; initial fatigue load-60% of the mean monotonic load-to-failure; step size-5% of the initial fatigue load). A stainless-steel piston (0 = 40 mm) applied the load into the center of the specimens submerged in water. Fractographic analysis and Finite Element Analysis (FEA) were also performed. Results. The ceramic thickness influenced the fatigue failure load for both ZLS materials: Suprinity (716 N up to 1119 N); Celtra (404 N up to 1126 N). FEA showed that decreasing ceramic thickness led to higher stress concentration on the cementing interface. Significance. Different ZLS glass-ceramic thicknesses influenced the fatigue failure load of the bonded system (i.e. the thicker the glass ceramic is, the higher the fatigue failure load will be). Different microstructures of the ZLS glass-ceramics might affect the fatigue behavior. FEA showed that the thicker the glass ceramic is, the lower the stress concentration at the tensile surface will be. (C) 2018 The Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:891 / 900
页数:10
相关论文
共 35 条
  • [1] Fatigue Failure Load of Resin-bonded Simplified Lithium Disilicate Glass-Ceramic Restorations: Effect of Ceramic Conditioning Methods
    Mendes Tribst, Joao Paulo
    Monteiro, Jaiane Bandoli
    Venturini, Andressa Borin
    Rocha Pereira, Gabriel Kalil
    Bottino, Marco Antonio
    de Melo, Renata Marques
    Valandro, Luiz Felipe
    JOURNAL OF ADHESIVE DENTISTRY, 2019, 21 (04) : 373 - 381
  • [2] Influence of fatigue load on various adhesive resin luting agents in a zirconia-reinforced lithium silicate ceramic bonded to dentin
    Watananiyom, Ratikorn
    Srisawasdi, Sirivimol
    AMERICAN JOURNAL OF DENTISTRY, 2021, 34 (05) : 261 - 266
  • [3] Zirconia-reinforced lithium silicate crowns: Effect of thickness on survival and failure mode
    Bergamo, Edmara T. P.
    Bordin, Dimoruan
    Ramalho, Ilana S.
    Lopes, Adolfo C. O.
    Gomes, Rafael S.
    Kaizer, Marina
    Witek, Lulzasz
    Bonfante, Esteuam A.
    Coelho, Paulo G.
    Del Bel Cury, Altair A.
    DENTAL MATERIALS, 2019, 35 (07) : 1007 - 1016
  • [4] Fatigue failure load of zirconia-reinforced lithium silicate glass ceramic cemented to a dentin analogue: Effect of etching time and hydrofluoric acid concentration
    Monteiro, Jaiane Bandoli
    Oliani, Marcelo Gallo
    Guilardi, Luis Felipe
    Prochnow, Catina
    Rocha Pereira, Gabriel Kalil
    Bottino, Marco Antonio
    de Melo, Renata Marques
    Valandro, Luiz Felipe
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2018, 77 : 375 - 382
  • [5] Load effect on the mechanical behaviour of zirconia-reinforced lithium silicate glass ceramics
    Alao, Abdur-Rasheed
    Haziq, Muhammad
    CERAMICS INTERNATIONAL, 2021, 47 (01) : 1353 - 1363
  • [6] Machinability: Zirconia-reinforced lithium silicate glass ceramic versus lithium disilicate glass ceramic
    Chen, Xing-Peng
    Xiang, Zhong-Xia
    Song, Xiao-Fei
    Yin, Ling
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2020, 101
  • [7] Ceramic firing protocols and thermocycling: effects on the load-bearing capacity under fatigue of a bonded zirconia lithium silicate glass-ceramic
    Diniz, Vandeberg
    Conde Oliveira Prado, Pedro Henrique
    Meireles Rodrigues, Jonas Vinicius
    Monteiro, Jaiane Bandoli
    Zucuni, Camila
    Valandro, Luiz Felipe
    Melo, Renata M.
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2020, 110
  • [8] Finishing technique effect on strength of zirconia-reinforced lithium silicate ceramic
    Benalcazar-Jalkh, Ernesto Byron
    Cunha, Verena Souza
    Bergamo, Edmara Tatiely Pedroso
    Alves, Larissa Marcia Martins
    de Monteiro-Sousa, Raphaelle Santos
    Campos, Tiago Moreira Bastos
    Tanaka, Ricardo
    Marcolino, Giovana de Assis
    de Souza, Felipe Machado
    Bonfante, Estevam Augusto
    EUROPEAN JOURNAL OF ORAL SCIENCES, 2024, 132 (01)
  • [9] Survival probability of zirconia-reinforced lithium silicate ceramic: Effect of surface condition and fatigue test load profile
    de Oliveira Dal Piva, Amanda Maria
    Mendes Tribst, Joao Paulo
    Venturini, Andressa Borin
    Anami, Lilian Costa
    Bonfante, Estevam Augusto
    Bottino, Marco Antonio
    Kleverlaan, Cornelis Johannes
    DENTAL MATERIALS, 2020, 36 (06) : 808 - 815
  • [10] Staining and bleaching susceptibility of zirconia-reinforced lithium silicate glass-ceramics with different thicknesses, translucencies, and fabrication methods
    Al-Johani, Hanan
    Alhotan, Abdulaziz
    Alhijji, Saleh
    Silikas, Nick
    Satterthwaite, Julian
    JOURNAL OF PROSTHETIC DENTISTRY, 2024, 131 (03) : 530.e1 - 530.e11