New insights into the role of zero-valent iron surface oxidation layers in persulfate oxidation of dibutyl phthalate solutions
被引:137
作者:
Li, Huanxuan
[1
,3
]
Wan, Jinquan
[1
,4
]
Ma, Yongwen
[1
,4
]
Huang, Mingzhi
[2
]
Wang, Yan
[1
,3
]
Chen, Yangmei
[4
,5
]
机构:
[1] S China Univ Technol, Coll Environm & Energy, Guangzhou 510006, Guangdong, Peoples R China
[2] Sun Yat Sen Univ, Dept Water Resources & Environm, Guangzhou 510275, Guangdong, Peoples R China
[3] Minist Educ, Key Lab Pollut Control & Ecosyst Restorat Ind Clu, Guangzhou 510006, Guangdong, Peoples R China
[4] S China Univ Technol, State Key Lab Pulp & Paper Engn, Guangzhou 510640, Guangdong, Peoples R China
[5] S China Univ Technol, Sch Chem & Chem Engn, Guangzhou 510640, Guangdong, Peoples R China
基金:
中国国家自然科学基金;
关键词:
Zero-valent iron (ZVI);
Persulfate;
Dibutyl phthalate (DBP);
Iron oxides;
Corrosion products;
ACTIVATED PERSULFATE;
GRANULAR IRON;
IN-SITU;
DEGRADATION;
PEROXYDISULFATE;
DECOMPOSITION;
REMEDIATION;
REMOVAL;
ACID;
D O I:
10.1016/j.cej.2014.03.092
中图分类号:
X [环境科学、安全科学];
学科分类号:
08 ;
0830 ;
摘要:
Batch tests were conducted to investigate the effect of initial pH on the degradation of dibutyl phthalate (DBP), the formation and evolution of iron corrosion products, and the role of iron oxides on the further degradation of DBP in zero-valent iron (ZVI)-persulfate system. The study indicated that the half-lives for the oxidation of DBP by persulfate activated with ZVI were 30-176 min at pH 3.0-11.0. The constituents and the morphology of the iron corrosion coating along different initial pH and over reaction time were investigated with Raman spectroscopy, X-ray photoelectron spectroscopy and Scanning electron microscopy. The results illustrated that magnetite (Fe3O4), wustite (FeO), hematite (alpha-Fe2O3) and goethite (alpha-FeOOH) were identified as the corrosion products. In alkaline and neutral solutions, the inner layer of iron oxides was mainly composed of alpha-Fe2O3 with some alpha-FeOOH while the outer layer mostly consisted of Fe3O4 and alpha-FeOOH. Oppositely, the iron oxides formation in acidic solution mainly consisted of Fe3O4, alpha-FeOOH and a small amount of alpha-Fe2O3 and FeO in the inner layer, the outer layer was mostly composed of alpha-Fe2O3 and some alpha-FeOOH. These iron corrosion coatings exhibited an inhibitory effect on the degradation of DBP, which may be due to that the iron oxides hindered the electron transfer from ZVI core to the solid-liquid interface. (C) 2014 Elsevier B.V. All rights reserved.