摘要
W fibre-reinforced Cu shows great promise to improve the mechanical performance at high-temperatures compared to conventional Cu-based alloys. Focus was placed on the optimization of the interface to achieve an enhanced adhesion between W fibre and Cu matrix. The interfacial properties were investigated through pull-out measurements of single matrix-coated fibres for different interfacial concepts. The interfacial adhesion of W and Cu is determined solely through mechanical interlocking. Interdiffusion and segregations experiment showed that there are no interface reactions between W and Cu at elevated temperatures. From the investigated interfacial concepts, a stepwise graded transition interface with additional heat treatment was found to achieve the highest interfacial shear strength. The thermal stability of the MMC in thermal cycling tests can be assured by depositing a stepwise graded transition between W fibre and Cu matrix. (C) 2009 Elsevier B.V. All rights reserved.
引用
收藏
页码:453 / 456
页数:4
相关论文
共 10 条
[1]  
[Anonymous], 1996, BIN ALL PHAS DIAGR
[2]   Plasma-material interactions in current tokamaks and their implications for next step fusion reactors [J].
Federici, G ;
Skinner, CH ;
Brooks, JN ;
Coad, JP ;
Grisolia, C ;
Haasz, AA ;
Hassanein, A ;
Philipps, V ;
Pitcher, CS ;
Roth, J ;
Wampler, WR ;
Whyte, DG .
NUCLEAR FUSION, 2001, 41 (12R) :1967-2137
[3]   Divertor issues on ITER and extrapolation to reactors [J].
Kukushkin, AS ;
Pacher, HD ;
Federici, G ;
Janeschitz, G ;
Loarte, A ;
Pacher, GW .
FUSION ENGINEERING AND DESIGN, 2003, 65 (03) :355-366
[4]  
MAISONNIER D, 2004, EFDA FINAL REPORT EU
[5]  
Mayer M., 1997, 9113 IPP M PLANCK I
[6]  
McDanels D.L., 1989, 2924 NASA
[7]   Erosion lifetime of ITER divertor plates [J].
Pacher, HD ;
Smid, I ;
Federici, G ;
Igitkhanov, Y ;
Janeschitz, G ;
Raffray, R ;
Vieider, G .
JOURNAL OF NUCLEAR MATERIALS, 1997, 241 :255-259
[8]  
RAUSCH G, 1992, J EUR CERAM SOC, V10, P229, DOI 10.1016/0955-2219(92)90036-D
[9]  
SHETTY DK, 1988, J AM CERAM SOC, V71, pC107, DOI 10.1111/j.1151-2916.1988.tb05843.x
[10]   Overall mechanical properties of fiber-reinforced metal matrix composites for fusion applications [J].
You, JH ;
Bolt, H .
JOURNAL OF NUCLEAR MATERIALS, 2002, 305 (01) :14-20