The Effect of Nitric Acid Oxidation Parameters to The Structural and Electrochemical Behavior of Multi-Walled Carbon Nanotubes

被引:0
作者
Shamsuddin, Shahidah Anna [1 ]
Derman, Mohd Nazree [1 ,2 ]
Ismail, Jasni Mohamed [1 ]
Halim, Nur Hamidah Abdul [1 ]
Hashim, Uda [1 ]
Rusop, Mohamad [3 ]
机构
[1] Univ Malaysia Perlis, Inst Nano Elect Engn, Blok A,Jln Kangar AStar, Kangar 01000, Perlis, Malaysia
[2] Univ Malaysia Perlis, Sch Mat Engn, Kompleks Pusat Pengajian Jejawi 2, Arau 02600, Perlis, Malaysia
[3] Univ Teknol MARA UiTM, Fac Elect Engn, Nano Elect Ctr, Shah Alam 40450, Selangor, Malaysia
来源
4TH ELECTRONIC AND GREEN MATERIALS INTERNATIONAL CONFERENCE 2018 (EGM 2018) | 2018年 / 2045卷
关键词
Multi-walled carbon nanotubes; Fourier Transform Infra-Red Spectroscopy; Raman Spectroscopy;
D O I
10.1063/1.5080831
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
In this paper, the effects of acid oxidation parameters to the structural and electrochemical behavior of multi walled carbon nanotubes (MWCNTs) were investigated. The parameters studied were acid concentration, oxidation temperature and oxidation time. The measurement of effects was calculated by how much amount of carboxylic groups (-COOH) introduced and how much structural defects occurred, measured by Fourier Transform Infra-Red Spectroscopy (FTIR) and Raman spectroscopy, respectively. Morphological study was carried out by using SEM. Meanwhile, cyclic voltammetry test (CV) was used in purpose to study the effect of COOH amounts and structural defect to the electrochemical behavior of the COOH-MWCNTs by measuring the oxidation current peaks of DNA immobilization (immobilization current, I-immo). At the end of this study, we had found that the structural defect of COOH-MWCNTs was directly proportional to the amount of COOH produced. By increasing the acid concentration, oxidation temperature and oxidation time, the amounts of COOH will continuously increase, and so on with the structural defect. Meanwhile, from the cyclic voltammetry test, the results had shown that the immobilization current(I-immo) was directly proportional to the increasing number of COOH. However, the current will started to reduce once the structural defect had occurred too much.
引用
收藏
页数:8
相关论文
共 13 条
[1]  
Abuilaiwi FA, 2010, ARAB J SCI ENG, V35, P37
[2]  
Cheraghali R., 2011, INT J ACAD RES, V3, P820
[3]   Demonstration of the importance of oxygenated species at the ends of carbon nanotubes for their favourable electrochemical properties [J].
Chou, A ;
Böcking, T ;
Singh, NK ;
Gooding, JJ .
CHEMICAL COMMUNICATIONS, 2005, (07) :842-844
[4]  
Djordjevic V, 2006, J OPTOELECTRON ADV M, V8, P1631
[5]   Purification of carbon nanotubes [J].
Hou, Peng-Xiang ;
Liu, Chang ;
Cheng, Hui-Ming .
CARBON, 2008, 46 (15) :2003-2025
[6]   Nitric acid purification of single-walled carbon nanotubes [J].
Hu, H ;
Zhao, B ;
Itkis, ME ;
Haddon, RC .
JOURNAL OF PHYSICAL CHEMISTRY B, 2003, 107 (50) :13838-13842
[7]   Determination of the acidic sites of purified single-walled carbon nanotubes by acid-base titration [J].
Hu, H ;
Bhowmik, P ;
Zhao, B ;
Hamon, MA ;
Itkis, ME ;
Haddon, RC .
CHEMICAL PHYSICS LETTERS, 2001, 345 (1-2) :25-28
[8]  
Lidong S., 2007, CHEM COMMUN, P5090
[9]  
Shamsuddin S. A., 2011, Proceedings of the 2011 IEEE Regional Symposium on Micro and Nanoelectronics (RSM 2011), P263, DOI 10.1109/RSM.2011.6088339
[10]  
Shamsuddin S. A., 2012, IMIEJS2012 P 2012 KU, P983