Performance and wear characteristics of ceramic, cemented carbide, and metal nozzles used in coal-water-slurry boilers

被引:18
作者
Deng Jianxin [1 ]
Ding Zeliang [2 ]
Zhou Houming [1 ]
Tan Yuanqiang [1 ]
机构
[1] Xiangtan Univ, Sch Mech Engn, Xiangtan 411105, Hunan, Peoples R China
[2] Hunan Univ Technol, Hunan Engn Technol Key Lab Inorgan & Nonmet Mat, Zhuzhou 412008, Hunan, Peoples R China
关键词
Nozzles; Erosion wear; Coal-water-slurry; Ceramics; THERMAL-SHOCK; EROSION; MECHANISMS; SAND; RESISTANCE; HARDMETALS;
D O I
10.1016/j.ijrmhm.2009.05.007
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Ceramics, cemented carbides, and metals were prepared to be used as nozzles in CWS boilers. CWS burning tests in a boiler with these nozzles were carried out. The erosion wear resistance of these nozzles was compared by determining their erosion rates and hole diameter variation. Results showed that the life of the ceramic nozzles is about 30 times high than that of the metal nozzles. The wear types at the nozzle wall surface differed in various positions. The nozzle center wall section suffers form abrasive impact under low impact angles, and the damage at the center wall mainly occurs by plowing and plastic deformation for metals, and by polishing action for carbides and ceramics. The primary wear mechanisms at the exit of ceramic nozzle exhibited thermal shock damage with chipping owing to the greater thermal stresses. (C) 2009 Elsevier Ltd. All rights reserved.
引用
收藏
页码:919 / 926
页数:8
相关论文
共 24 条
[1]  
Boylu F., 2000, 5 COAL UT TECHN S AN, P195
[2]  
CEN KF, 1997, THEORY APPL COMBUSTI
[3]   Analysis and prediction of thermal shock in brittle materials [J].
Collin, M ;
Rowcliffe, D .
ACTA MATERIALIA, 2000, 48 (08) :1655-1665
[4]   A MODIFIED INDENTATION TOUGHNESS TECHNIQUE [J].
COOK, RF ;
LAWN, BR .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1983, 66 (11) :C200-C201
[5]   Wear mechanisms of gradient ceramic nozzles in abrasive air-jet machining [J].
Deng, Jianxin ;
Wu, Fengfang ;
Zhao, Jinlong .
INTERNATIONAL JOURNAL OF MACHINE TOOLS & MANUFACTURE, 2007, 47 (12-13) :2031-2039
[6]   Erosion wear mechanisms of coal-water-slurry (CWS) ceramic nozzles in industry boilers [J].
Deng, JX ;
Ding, ZL ;
Yuan, DL .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 417 (1-2) :1-7
[7]   Wear of ceramic nozzles by dry sand blasting [J].
Deng, JX ;
Zhang, XH ;
Niu, PZ ;
Liu, LL ;
Wang, JH .
TRIBOLOGY INTERNATIONAL, 2006, 39 (03) :274-280
[8]  
Deng JX, 2003, J EUR CERAM SOC, V23, P323, DOI 10.1016/S0955-2219(02)00183-8
[9]   Wear behavior of ceramic nozzles in coal water slurry burning [J].
Ding, ZL ;
Deng, JX ;
Li, JF ;
Sun, GZ ;
Ai, X .
CERAMICS INTERNATIONAL, 2004, 30 (04) :591-596
[10]  
DING ZL, 2004, THESIS SHANDONG U JI