Thermoelectric Properties of Bi Doped Tetrahedrite

被引:37
作者
Kumar, D. S. Prem [1 ]
Chetty, R. [2 ]
Femi, O. E. [3 ]
Chattopadhyay, K. [3 ]
Malar, P. [1 ]
Mallik, R. C. [2 ]
机构
[1] SRM Univ, Res Inst, Dept Phys & Nanotechnol, Kattankulathur 603203, India
[2] Indian Inst Sci, Dept Phys, Thermoelect Mat & Device Lab, Bangalore 560012, Karnataka, India
[3] Indian Inst Sci, Dept Mat Engn, Bangalore 560012, Karnataka, India
关键词
Tetrahedrite; x-ray diffraction (XRD); electron probe micro analysis (EPMA); transport properties; NATURAL MINERAL TETRAHEDRITE; THERMAL-CONDUCTIVITY; SUBSTITUTION; PERFORMANCE; CRYSTAL; SB;
D O I
10.1007/s11664-016-4826-5
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Bi doped tetrahedrites with nominal compositions of Cu12Sb4-x Bi (x) S-13 (x = 0, 0.2, 0.4, 0.6, 0.8) were synthesized by the solid state reaction method. Powder x-ray diffraction patterns confirmed that Cu12Sb4S13 (tetrahedrite structure) was the main phase, along with Cu3SbS4 and Cu3SbS3 as the secondary phases. Electron probe microanalysis provided the elemental composition of all the samples. It was confirmed that the main phase is the tetrahedrite phase with slight deviations in the stoichiometry. All the transport properties were measured between 423 K and 673 K. The electrical resistivity increased with an increase in Bi content for all the samples, possibly induced by the variation in the carrier concentration, which may be due to the influence of impurity phases. The increase in electrical resistivity with an increase in temperature indicates the degenerate semiconducting nature of the samples. The absolute Seebeck coefficient is positive throughout the temperature range indicating the p-type nature of the samples. The Seebeck coefficient for all the samples increased with an increase in Bi content as electrical resistivity. The variation of electrical resistivity and the Seebeck coefficient with doping can be attributed to the changes in the carrier concentration of the samples. The total thermal conductivity increases with an increase in temperature and decreases with an increase in the Bi content that could be due to the reduction in carrier thermal conductivity. The highest thermoelectric figure of merit (zT) similar to 0.84 at 673 K was obtained for the sample with x = 0.2 due to lower thermal conductivity (1.17 W/m K).
引用
收藏
页码:2616 / 2622
页数:7
相关论文
共 24 条
[1]   Thermoelectric Materials: A New Rapid Synthesis Process for Nontoxic and High-Performance Tetrahedrite Compounds [J].
Barbier, Tristan ;
Rollin-Martinet, Sabrina ;
Lemoine, Pierric ;
Gascoin, Franck ;
Kaltzoglou, Andreas ;
Vaqueiro, Paz ;
Powell, Anthony V. ;
Guilmeau, Emmanuel .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2016, 99 (01) :51-56
[2]  
Blatt F.J., 1968, Physics of electronic conduction in solids, P210
[3]   Crystal structure, electronic band structure and high-temperature thermoelectric properties of Te-substituted tetrahedrites Cu12Sb4-xTexS13 (0.5 ≤ x ≤ 2.0) [J].
Bouyrie, Y. ;
Candolfi, C. ;
Ohorodniichuk, V. ;
Malaman, B. ;
Dauscher, A. ;
Tobola, J. ;
Lenoir, B. .
JOURNAL OF MATERIALS CHEMISTRY C, 2015, 3 (40) :10476-10487
[4]   From crystal to glass-like thermal conductivity in crystalline minerals [J].
Bouyrie, Y. ;
Candolfi, C. ;
Pailhes, S. ;
Koza, M. M. ;
Malaman, B. ;
Dauscher, A. ;
Tobola, J. ;
Boisron, O. ;
Saviot, L. ;
Lenoir, B. .
PHYSICAL CHEMISTRY CHEMICAL PHYSICS, 2015, 17 (30) :19751-19758
[5]   Tetrahedrites as thermoelectric materials: an overview [J].
Chetty, R. ;
Bali, A. ;
Mallik, R. C. .
JOURNAL OF MATERIALS CHEMISTRY C, 2015, 3 (48) :12364-12378
[6]   Thermoelectric properties of Co substituted synthetic tetrahedrite [J].
Chetty, R. ;
Bali, A. ;
Naik, M. H. ;
Rogl, G. ;
Rogl, P. ;
Jain, M. ;
Suwas, S. ;
Mallik, R. C. .
ACTA MATERIALIA, 2015, 100 :266-274
[7]   Thermoelectric properties of a Mn substituted synthetic tetrahedrite [J].
Chetty, Raju ;
Kumar, Prem D. S. ;
Rogl, Gerda ;
Rogl, Peter ;
Bauer, Ernst ;
Michor, Herwig ;
Suwas, Satyam ;
Puchegger, Stephan ;
Giester, Gerald ;
Mallik, Ramesh Chandra .
PHYSICAL CHEMISTRY CHEMICAL PHYSICS, 2015, 17 (03) :1716-1727
[8]   SUBSTITUTION OF Bi FOR Sb AND As IN MINERALS OF THE TETRAHEDRITE SERIES FROM REDZINY, LOWER SILESIA, SOUTHWESTERN POLAND [J].
Golebiowska, Bozena ;
Pieczka, Adam ;
Parafiniuk, Jan .
CANADIAN MINERALOGIST, 2012, 50 (02) :267-279
[9]   Fast and scalable preparation of tetrahedrite for thermoelectrics via glass crystallization [J].
Goncalves, A. P. ;
Lopes, E. B. ;
Monnier, J. ;
Bourgon, J. ;
Vaney, J. B. ;
Piarristeguy, A. ;
Pradel, A. ;
Lenoir, B. ;
Delaizir, G. ;
Pereira, M. F. C. ;
Alleno, E. ;
Godart, C. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 664 :209-217
[10]   Design Meets Nature: Tetrahedrite Solar Absorbers [J].
Heo, Jaeseok ;
Ravichandran, Ram ;
Reidy, Christopher F. ;
Tate, Janet ;
Wager, John F. ;
Keszler, Douglas A. .
ADVANCED ENERGY MATERIALS, 2015, 5 (07)