Erosion-enhanced corrosion of stainless steel and carbon steel measured electrochemically under liquid and slurry impingement

被引:48
作者
Zheng, Z. B. [1 ]
Zheng, Y. G. [1 ]
机构
[1] Chinese Acad Sci, Inst Met Res, Key Lab Nucl Mat & Safety Assessment, Shenyang 110016, Peoples R China
基金
中国国家自然科学基金;
关键词
Carbon steel; Stainless steel; Erosion; Polarization; Passivity; CAVITATION EROSION; PITTING CORROSION; PARTICLE-VELOCITY; IMPACT ANGLE; BEHAVIOR; FLOW; RESISTANCE; MECHANISM; PASSIVITY; KINETICS;
D O I
10.1016/j.corsci.2015.10.014
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The erosion-enhanced corrosion of 304 stainless steel and carbon steel under impingement by NaCl solution has been investigated. With increasing flow velocity, the open-circuit potential of carbon steel increases in the sand-free solution, while,decreases in the sand-containing solution. The passive current density of stainless steel under impingement is close to that in quiescent condition in most cases, while increases by an order of magnitude at a flow velocity higher than the critical flow velocity. An ideal schematic has been used to explain the electrochemical results. The passivation of stainless steel under impingement is further analyzed by potentiostatic polarization. (C) 2015 Elsevier Ltd. All rights reserved.
引用
收藏
页码:259 / 268
页数:10
相关论文
共 46 条
[11]   The electrochemical response of stainless steels in liquid-solid impingement [J].
Hu, X ;
Neville, A .
WEAR, 2005, 258 (1-4) :641-648
[12]   An examination of the electrochemical characteristics of two stainless steels (UNS S32654 and UNS S31603) under liquid-solid impingement [J].
Hu, XM ;
Neville, A .
WEAR, 2004, 256 (05) :537-544
[13]   Erosion-corrosion behavior of Zr-based bulk metallic glass in saline-sand slurry [J].
Ji, Xiulin ;
Zhao, Jianhua ;
Zhang, Xunwei ;
Zhou, Meiying .
TRIBOLOGY INTERNATIONAL, 2013, 60 :19-24
[14]  
Kabir KB., 2010, J Chem Eng, V25, P13
[15]   Cavitation erosion-corrosion behaviour of laser surface alloyed AISI 1050 mild steel using NiCrSiB [J].
Kwok, CT ;
Man, HC ;
Cheng, FT .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 303 (1-2) :250-261
[16]   Passive behavior of a bulk nanostructured 316L austenitic stainless steel consisting of nanometer-sized grains with embedded nano-twin bundles [J].
Li, Tianshu ;
Liu, Li ;
Zhang, Bin ;
Li, Ying ;
Yan, Fengkai ;
Tao, Nairong ;
Wang, Fuhui .
CORROSION SCIENCE, 2014, 85 :331-342
[17]   Effect of particle velocity and impact angle on the corrosion-erosion of AISI 304 and AISI 420 stainless steels [J].
López, D ;
Congote, JP ;
Cano, JR ;
Toro, A ;
Tschiptschin, AP .
WEAR, 2005, 259 (1-6) :118-124
[18]   Erosion-enhanced corrosion of carbon steel at passive state [J].
Lu, B. T. ;
Luo, J. L. ;
Guo, H. X. ;
Mao, L. C. .
CORROSION SCIENCE, 2011, 53 (01) :432-440
[19]   Synergism of electrochemical and mechanical factors in erosion-corrosion [J].
Lu, BT ;
Luo, JL .
JOURNAL OF PHYSICAL CHEMISTRY B, 2006, 110 (09) :4217-4231
[20]   A systematic erosion-corrosion study of two stainless steels in marine conditions via experimental design [J].
Meng, H. ;
Hu, X. ;
Neville, A. .
WEAR, 2007, 263 :355-362