Fracture and toughening mechanisms in SiC nanofiber reinforced SiC matrix nanocomposites with amorphous carbon coatings

被引:9
作者
Li, Lili [1 ]
Niu, Jianbing [2 ]
Yang, Yanqing [4 ]
Xia, Zhenhai [2 ,3 ]
机构
[1] Fujian Univ Technol, Sch Mat Sci & Engn, Fuzhou 350108, Peoples R China
[2] Univ N Texas, Dept Mat Sci & Engn, Denton, TX 76203 USA
[3] Univ N Texas, Dept Chem, Denton, TX 76203 USA
[4] Northwestern Polytech Univ, Sch Mat Sci & Engn, Xian 710072, Peoples R China
基金
美国国家科学基金会;
关键词
Molecular dynamic simulation; Mechanical properties; Coatings; Interface/interphase; Nanocomposites; HIGH-STRENGTH; COMPOSITES; DESIGN; POTENTIALS; SIMULATION; TOUGHNESS;
D O I
10.1016/j.commatsci.2013.11.005
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Fracture behavior of SiC matrix nanocomposites reinforced by SiC nanofiber coated with amorphous carbon (a-C) coatings is studied via molecular dynamics simulations. The a-C coating plays a significant role in the tensile strength, and fracture energy of the nanocomposites. With increasing thickness of the a-C coating, the failure behavior of nanocomposites transitions from brittle fracture to a non-catastrophic mode of ductile performance while the tensile strength increases. An introduction of appropriate functionally-graded a-C coating can significantly enhance nanofiber pullout and thus pullout energy by an order of magnitude. Our results suggest that material design directions - coating thickness and the functionally-graded coating - are all efficient approaches for engineering nanoscale SiC/SiC composites for high strength and toughness. (C) 2013 Elsevier B. V. All rights reserved.
引用
收藏
页码:255 / 260
页数:6
相关论文
共 50 条
  • [31] Fabrication and characterization of in-situ grown carbon nanotubes reinforced SiC/SiC composite
    Zhao, Shuang
    Yang, Zichun
    Zhou, Xingui
    Sun, Ke
    [J]. CERAMICS INTERNATIONAL, 2016, 42 (07) : 9264 - 9269
  • [32] Microstructure and Properties of Carbon Fiber Reinforced SiC Matrix Composites Containing Ti3SiC2
    Fan, Xiaomeng
    Yin, Xiaowei
    [J]. ADVANCED ENGINEERING MATERIALS, 2014, 16 (06) : 670 - 683
  • [33] Fracture behaviour of SiC/SiC ceramic matrix composite at room temperature
    Delage, Justine
    Saiz, Eduardo
    Al Nasiri, Nasrin
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2022, 42 (07) : 3156 - 3167
  • [34] Toughening of SiC matrix with in-situ created TiB2 particles
    Bucevac, Dusan
    Boskovic, Snezana
    Matovic, Branko
    Krstic, Vladimir
    [J]. CERAMICS INTERNATIONAL, 2010, 36 (07) : 2181 - 2188
  • [35] Study of toughening behavior of SiC whiskers on 8YSZ thermal barrier coatings
    Liu, Dianchao
    Jing, Yongzhi
    Cui, Xiufang
    Jin, Guo
    Chen, Zhuo
    Wang, Xinhe
    Liu, Anying
    Li, Qicheng
    Tian, Haoliang
    Fang, Yongchao
    [J]. SURFACE & COATINGS TECHNOLOGY, 2023, 455
  • [36] Thermophysical properties of carbon fiber reinforced multilayered (PyC-SiC)n matrix composites
    Jia, Yan
    Li, Kezhi
    Xue, Lizhen
    Huang, Liye
    Ren, Junjie
    Zhang, Shouyang
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2017, 37 (10) : 3255 - 3261
  • [37] Structural and Mechanical Characterization of Aluminum Matrix Nanocomposites Reinforced with SiC and Al2O3 Nanoparticles
    Gharaibeh, Nabeel
    Alajlouni, Musa
    Rayes, Alaa
    [J]. REVUE DES COMPOSITES ET DES MATERIAUX AVANCES-JOURNAL OF COMPOSITE AND ADVANCED MATERIALS, 2024, 34 (06): : 749 - 754
  • [38] The fatigue and final fracture behavior of SiC particle reinforced 7034 aluminum matrix composites
    Srivatsan, TS
    Al-Hajri, M
    [J]. COMPOSITES PART B-ENGINEERING, 2002, 33 (05) : 391 - 404
  • [39] Fatigue properties and fracture analysis of a SiC fiber-reinforced titanium matrix composite
    Feng, G. H.
    Yang, Y. Q.
    Luo, X.
    Li, J.
    Huang, B.
    Chen, Y.
    [J]. COMPOSITES PART B-ENGINEERING, 2015, 68 : 336 - 342
  • [40] Effect of Isothermal Forging on Fracture Toughness of SiC Particle Reinforced Aluminum Matrix Composite
    Wei Shaohua
    Nie Junhui
    Liu Yanqiang
    Zuo Tao
    Hao Xinxiang
    Ma Zili
    Fan Jianzhong
    [J]. RARE METAL MATERIALS AND ENGINEERING, 2017, 46 (11) : 3464 - 3468