摘要
Ti-TiN and TiN-CrN nanomultilayers were thermally stable retaining uniform and sharp layer interfaces up to 24 h at 773 K, without any oxidation or phase transformation accompanying each individual layer. Decreasing the multilayer spacing resulted in an increase in the hardness in both cases. The coating hardness was found to be independent of the substrate type, when applied on HS718, Ti64 and HCHCr substrates. In scratch testing, the multilayers displayed a better resistance to the onset of failure, as compared to the monolayer TiN. The substrate plasticity played an important role in determining the coating failure mode. Self-mated wear tests revealed the CrN-TiN system to exhibit the best wear behaviour, both at room temperature and at 773 K. The Ti-TiN coatings are more accommodative with all three substrates, as compared to TiN-CrN and TiN. (c) 2006 Elsevier Ltd. All rights reserved.
引用
收藏
页码:266 / 277
页数:12
相关论文
共 42 条
  • [31] High-temperature thermal stability and oxidation resistance of Cr and Ta co-alloyed Ti - Al - N coatings deposited by cathodic arc evaporation
    Peng, Bin
    Li, Haiqing
    Zhang, Quan
    Xu, Yu X.
    Wei, Tiefeng
    Wang, Qimin
    Zhang, Fengge
    Kim, Kwang Ho
    CORROSION SCIENCE, 2020, 167
  • [32] STRUCTURE AND PHASE TRANSFORMATIONS IN THE SURFACE LAYERS OF COMPOSITE CERAMIC MATERIALS BASED ON THE SYSTEMS (TiN-AlN)-(TiN-Cr3C2) AND (TiN-AlN)-(Ni-Cr)-(TiN-Cr3C2) WITH HIGH-TEMPERATURE OXIDATION UNDER CONDITIONS OF CONCENTRATED SOLAR RADIATION
    Mosina, T. V.
    REFRACTORIES AND INDUSTRIAL CERAMICS, 2011, 52 (01) : 48 - 51
  • [33] Growth conditions, electrical resistivity, microhardness and thermal properties of Nb5Sn2Ga single crystals synthesized from high-temperature tin solutions
    Okada, S
    Kudou, K
    Shishido, T
    Higashi, I
    Horiuchi, H
    Fukuda, T
    JOURNAL OF ALLOYS AND COMPOUNDS, 1998, 281 (02) : 160 - 162
  • [34] High-temperature fretting wear behavior and microstructure stability of a laser-cladding Ti-Al-C-N composite coating meditated by variable cycle conditions
    Sun, Linghong
    Wang, Xiaoli
    Cao, Yue
    Wang, Yuecun
    Ma, Qiang
    Wu, Hongxing
    Hua, Ke
    Wang, Haifeng
    TRIBOLOGY INTERNATIONAL, 2025, 201
  • [35] Self-Healing and Thermal Stability of LaMgAl11O19-Ti3AlC2 Composites for High-Temperature Abradable Applications
    Huang, Jingqi
    Chen, Wenbo
    Lu, Kaiyue
    Xu, Mingyi
    Deng, Longhui
    Jiang, Jianing
    Dong, Shujuan
    Chen, Meizhu
    Cao, Xueqiang
    COATINGS, 2024, 14 (08)
  • [36] A comparative study of high-temperature erosion wear of plasma-sprayed NiCrBSiFe and WC-NiCrBSiFe coatings under simulated coal-fired boiler conditions
    Hidalgo, VH
    Varela, FJB
    Menéndez, AC
    Martínez, SP
    TRIBOLOGY INTERNATIONAL, 2001, 34 (03) : 161 - 169
  • [37] Laser cladding for high-temperature self-lubricating wear-resistant composite coatings on γ-TiAl intermetallic alloy Ti-48Al-2Cr-2Nb
    Liu, XB
    Wang, CM
    Yu, LG
    Wang, HM
    HIGH-POWER LASERS IN MANUFACTURING, 2000, 3888 : 312 - 317
  • [38] Tribological behavior of plasma-sprayed Yttria-stabilized zirconia thermal barrier coatings on 316L stainless steel under high-temperature conditions
    Yetim, A. F.
    Tekdir, H.
    Turalioglu, K.
    Taftali, M.
    Yetim, T.
    MATERIALS LETTERS, 2023, 336
  • [39] Research on the chemical barrier and failure behavior of WS2 and WS2/Ti coatings under high-temperature conditions and the effects on the lifespan of diamond-coated cutting tools
    Zhang, Zhao
    Tan, Zhuoming
    Lu, Wenzhuang
    Yi, Siguang
    Qin, Xudong
    SURFACE & COATINGS TECHNOLOGY, 2023, 469
  • [40] Solid-State Reactions of SiC/W-25Re Alloy and Thermal Stability of SiC/Ti/W-25Re Alloy under High-Temperature Annealing
    Han, Jun Sae
    Jang, Seung Sik
    Park, Dong Yong
    Oh, Yong Jun
    Park, Seong Jin
    ADVANCED ENGINEERING MATERIALS, 2016, 18 (09) : 1574 - 1580