Development of nanostructured icephobic aluminium oxide surfaces for aeronautic applications

被引:20
作者
Belaud, Clementine [1 ,2 ,3 ]
Vercillo, Vittorio [1 ,4 ]
Kolb, Maximilian [1 ]
Bonaccurso, Elmar [1 ]
机构
[1] Airbus Cent Res & Technol, Mat X, Willy Messerschmitt Str 1, D-82024 Taufkirchen, Germany
[2] CPE Lyon, 43 Blvd 11 Novembre 1918, F-69616 Villeurbanne, France
[3] Univ Claude Bernard Lyon 1, 43 Blvd 11 Novembre 1918, F-69616 Villeurbanne, France
[4] Tech Univ Dresden, Inst Fertigungstech, George Bahr Str 3c, D-01069 Dresden, Germany
关键词
Anodization; Superhydrophobicity; Icephobicity; Wind tunnel; aluminium oxide; SUPERHYDROPHOBIC SURFACES; WETTABILITY; IMPACT;
D O I
10.1016/j.surfcoat.2020.126652
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In-flight icing due to the impingement of supercooled water droplets modifies the shape of the aerodynamic surfaces of aircraft, resulting in lower stall speeds and higher fuel consumption. Icephobic coatings help reducing the adhesion strength of ice to a surface and represent a promising technology to support mechanical/thermal ice protection systems. Superhydrophobic surfaces are water-repellent and embody a straightforward solution to tackle icing: nanostructured porous aluminium oxide layers are generated with anodization and superhydrophobicity can be reached by tuning the pores size. However, not much research has been done to verify if such surfaces are generally icephobic in representative icing conditions, or if they need to have additional properties to effectively reduce ice adhesion. In this work, we investigate the ice adhesion strength on cladded Aluminium Alloy 2024 (AA2024), an alloy commonly used for aerospace components, anodized with different process parameters in sulphuric and oxalic acid and hydrophobized by a commercial fluorinated product. Upon the optimization of the two anodization processes, the micro-/nanostructures generated on the surface were effective in reducing the ice adhesion strength. From icing wind tunnel tests, the surfaces anodized in oxalic acid showed superior icephobic (i.e., lower ice adhesion) properties compared to the ones anodized in sulphuric acid because of their larger air-to-solid surface ratio. The proposed anodization process is fast, easy to perform and to implement in existing production lines, low-cost, and operator- and environmentally-friendly.
引用
收藏
页数:11
相关论文
共 37 条
[1]   Interface strength and degradation of adhesively bonded porous aluminum oxides [J].
Abrahami, Shoshan T. ;
de Kok, John M. M. ;
Gudla, Visweswara C. ;
Ambat, Rajan ;
Terryn, Herman ;
Mol, Johannes M. C. .
NPJ MATERIALS DEGRADATION, 2017, 1 (01)
[2]   Fabrication of One-Dimensional Organic Nanostructures Using Anodic Aluminum Oxide Templates [J].
Al-Kaysi, Rabih O. ;
Ghaddar, Tarek H. ;
Guirado, Gonzalo .
JOURNAL OF NANOMATERIALS, 2009, 2009
[3]  
[Anonymous], 1987, NORMENSTELLE LUFTFAH
[4]  
B. of M Australian Government, 2010, AIRCR IC
[5]   Purity of the sacred lotus, or escape from contamination in biological surfaces [J].
Barthlott, W ;
Neinhuis, C .
PLANTA, 1997, 202 (01) :1-8
[6]   Modus Operandi of Protective and Anti-icing Mechanisms Underlying the Design of Longstanding Outdoor Icephobic Coatings [J].
Boinovich, Ludmila B. ;
Emelyanenko, Alexandre M. ;
Emelyanenko, Kirill A. ;
Modin, Evgeny B. .
ACS NANO, 2019, 13 (04) :4335-4346
[7]   Surface Wettability of Macroporous Anodized Aluminum Oxide [J].
Buijnsters, Josephus G. ;
Zhong, Rui ;
Tsyntsaru, Natalia ;
Celis, Jean-Pierre .
ACS APPLIED MATERIALS & INTERFACES, 2013, 5 (08) :3224-3233
[8]   Wettability of porous surfaces. [J].
Cassie, ABD ;
Baxter, S .
TRANSACTIONS OF THE FARADAY SOCIETY, 1944, 40 :0546-0550
[9]   Fabrication of ideally ordered nanoporous alumina films and integrated alumina nanotubule arrays by high-field anodization [J].
Chu, SZ ;
Wada, K ;
Inoue, S ;
Isogai, M ;
Yasumori, A .
ADVANCED MATERIALS, 2005, 17 (17) :2115-+
[10]   Improvement of lubricant-infused surfaces for anti-icing applications [J].
Erbil, Husnu Yildirim .
SURFACE INNOVATIONS, 2016, 4 (04) :214-217