Study on dimensional stabilization of 12,500-year-old waterlogged subfossil Scots pine wood from the Kozmin Las site, Poland

被引:8
作者
Babinski, Leszek [1 ]
Fabisiak, Ewa [2 ]
Dabrowski, Henryk P. [3 ]
Kittel, Piotr [4 ]
机构
[1] Archaeol Museum Biskupin, Dept Conservat, Biskupin 17, PL-88410 Gasawa, Poland
[2] Poznan Univ Life Sci, Fac Wood Technol, Dept Wood Sci, Ul Wojska Polskiego 38-42, PL-60627 Poznan, Poland
[3] Archaeol Museum Biskupin, Dendroarchaeol Lab, Biskupin 17, PL-88410 Gasawa, Poland
[4] Univ Lodz, Fac Geog Sci, Dept Geomorphol & Palaeogeog, Ul Narutowicza 88, PL-90139 Lodz, Poland
关键词
Waterlogged subfossil wood; Scots pine; Dimensional stabilization; Polyethylene glycol; Sugar alcohol; Freeze-drying; ARCHAEOLOGICAL WOOD; CHEMICAL-COMPOSITION; PRESERVATION; PARAMETERS; BACTERIA; VALLEY; STATE;
D O I
10.1016/j.culher.2016.08.002
中图分类号
K85 [文物考古];
学科分类号
0601 ;
摘要
The study examines the efficiency of selected conservation treatments proposed for dimensional stabilization of 12,500-year-old waterlogged subfossil Scots pine (Pines sylvestris L.) tree trunks found at the KoZmin Las site, Poland. The research was done on 198 samples drawn from various parts of the same trunk. Experimental material was characterized on the basis of annual ring width, percentage of latewood, maximum moisture content, density at maximum moisture content, basic density, and wood porosity. Waterlogged wood samples were pre-treated with aqueous solutions of polyethylene glycol (PEG) 300, mixtures of PEG 300 and PEG 4000, a mixture of lactitol and trehalose or a mixture of mannitol and trehalose (nine variants of impregnation) and then freeze-dried or air-dried. Dimensional changes in the wood samples were measured after seasoning to reach equilibrium moisture content at 50% relative humidity and 20 degrees C. In the majority of the tested conservation treatments, tangential and radial shrinkages or tangential and radial swelling of wood did not exceed 1%. However, differences in dimensional changes depended on the conservation method used and sampling location. Regardless of the state of wood preservation and macroscopic structure features, the best dimensional stability, evaluated on the basis of average anti-shrink efficiency indices, was observed in wood pre-treated with aqueous solutions of 10% PEG 300 + 5% PEG 4000, 10% PEG 300 + 10% PEG 4000 or 10% lactitol/trehalose mixture, and then freeze-dried. (C) 2016 Elsevier Masson SAS. All rights reserved.