Micro-shear bond strength and surface micromorphology of a feldspathic ceramic treated with different cleaning methods after hydrofluoric acid etching

被引:14
|
作者
Steinhauser, Henrique Caballero [1 ]
Turssi, Cecilia Pedroso [2 ]
Gomes Franca, Fabiana Mantovani [2 ]
Botelho do Amaral, Flavia Lucisano [2 ]
Basting, Roberta Tarkany [2 ]
机构
[1] Imperatriz Sch Dent, Imperatriz, MA, Brazil
[2] Sao Leopoldo Mand Dent Res Inst, Sch Dent, Campinas, SP, Brazil
关键词
Ceramics; Hydrofluoric acid; Scanning electron microscopy; RESIN CEMENT; COMPOSITE RESIN; MICROTENSILE; PORCELAIN; ROUGHNESS;
D O I
10.1590/1678-775720130339
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objective: The aim of this study was to evaluate the effect of feldspathic ceramic surface cleaning on micro-shear bond strength and ceramic surface morphology. Material and Methods: Forty discs of feldspathic ceramic were prepared and etched with 10% hydrofluoric acid for 2 minutes. The discs were randomly distributed into five groups (n=8): C: no treatment, S: water spray + air drying for 1 minute, US: immersion in ultrasonic bath for 5 minutes, F: etching with 37% phosphoric acid for 1 minute, followed by 1-minuterinse, F+US: etching with 37% phosphoric acid for 1 minute, 1-minute rinse and ultrasonic bath for 5 minutes. Composite cylinders were bonded to the discs following application of silane and hydrophobic adhesive for micro-shear bond strength testing in a universal testing machine at 0.5 mm/min crosshead speed until failure. Stereomicroscopy was used to classify failure type. Surface micromorphology of each treatment type was evaluated by scanning electron microscopy at 500 and 2,500 times magnification. Results: One-way ANOVA test showed no significant difference between treatments (p=0.3197) and the most common failure types were cohesive resin cohesion followed by adhesive failure. Micro-shear bond strength of the feldspathic ceramic substrate to the adhesive system was not influenced by the different surface cleaning techniques. Absence of or less residue was observed after etching with hydrofluoric acid for the groups US and F+US. Conclusions: Combining ceramic cleaning techniques with hydrofluoric acid etching did not affect ceramic bond strength, whereas, when cleaning was associated with ultrasound, less residue was observed.
引用
收藏
页码:85 / 90
页数:6
相关论文
共 50 条
  • [1] Fatigue failure load of feldspathic ceramic crowns after hydrofluoric acid etching at different concentrations
    Venturini, Andressa B.
    Prochnow, Catina
    May, Liliana G.
    Kleverlaan, Cornelis J.
    Valandro, Luiz Felipe
    JOURNAL OF PROSTHETIC DENTISTRY, 2018, 119 (02) : 278 - 285
  • [2] Bond strength of metal brackets to feldspathic ceramic treated with different surface conditioning methods: an in vitro study
    Recen, Duygu
    Yildirim, Bengisu
    Othman, Eman
    Comlekoglu, Erhan
    Aras, Isil
    EUROPEAN ORAL RESEARCH, 2021, 55 (01) : 1 - 7
  • [3] Shear bond strength of ceramic brackets bonded to surface-treated feldspathic porcelain after thermocycling
    Cevik, Pinar
    Eraslan, Oguz
    Eser, Kursat
    Tekeli, Suleyman
    INTERNATIONAL JOURNAL OF ARTIFICIAL ORGANS, 2018, 41 (03) : 160 - 167
  • [4] Effect of Different Etching Times with Hydrofluoric Acid on the Bond Strength of CAD/CAM Ceramic Material
    Avram, Liane Tabitha
    Galatanu, Sergiu-Valentin
    Opris, Carmen
    Pop, Cristian
    Jivanescu, Anca
    MATERIALS, 2022, 15 (20)
  • [5] Effect of Low-Concentration Hydrofluoric Acid Etching on Shear Bond Strength and Biaxial Flexural Strength after Thermocycling
    Kang, You-Jung
    Shin, Yooseok
    Kim, Jee-Hwan
    MATERIALS, 2020, 13 (06)
  • [6] Effect of Different Surface Treatments on the Micro-Shear Bond Strength and Surface Characteristics of Zirconia: An In Vitro Study
    Sales, Ann
    Rodrigues, Shobha J.
    Mahesh, M.
    Ginjupalli, Kishore
    Shetty, Thilak
    Pai, Umesh Y.
    Saldanha, Sharon
    Hegde, Puneeth
    Mukherjee, Sandipan
    Kamath, Vignesh
    Bajantri, Prashant
    Srikant, N.
    Kotian, Ravindra
    INTERNATIONAL JOURNAL OF DENTISTRY, 2022, 2022
  • [7] Effect of the Etching Duration and Ultrasonic Cleaning on Microtensile Bond Strength Between Feldspathic Ceramic and Resin Cement
    Leite, Fabiola Pessoa
    Oezcan, Mutlu
    Valandro, Luiz Felipe
    Cunha Moreira, Carlos Heitor
    Amaral, Regina
    Bottino, Marco Antonio
    Kimpara, Estevao Tomomitsu
    JOURNAL OF ADHESION, 2013, 89 (03) : 159 - 173
  • [8] Shear Bond Strength of Lithium Disilicate to Resin Cement After Treatment with Hydrofluoric Acid and a Self-etching Ceramic Primer
    Pinto Klippel, Gesinete Goncalves
    de Melo-Silva, Claudio Luis
    Favieri de Melo-Silva, Tereza Cristina
    Elias, Carlos Nelson
    de Biasi, Ronaldo Sergio
    dos Santos, Claudinei
    MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2021, 24 (04):
  • [9] The Effect of Surface Treatments on the Micro-shear Bond Strength of a Resin Luting Agent and Four All-ceramic Systems
    Torres, S. M. P.
    Borges, G. A.
    Spohr, A. M.
    Cury, A. A. D. B.
    Yadav, S.
    Platt, J. A.
    OPERATIVE DENTISTRY, 2009, 34 (04) : 399 - 407
  • [10] Shear Bond Strength of Ceramic Brackets with Different Base Designs to Feldspathic Porcelains
    Samruajbenjakul, Buncha
    Kukiattrakoon, Boonlert
    ANGLE ORTHODONTIST, 2009, 79 (03) : 571 - 576