Effect of Build Orientation and Annealing on Corrosion Resistance of Additively Manufactured Duplex Stainless Steel in 3.5% NaCl

被引:15
作者
Nigon, Greg N. [1 ,2 ]
Isgor, O. Burkan [2 ,3 ]
Pasebani, Somayeh [1 ,2 ]
机构
[1] Oregon State Univ, Sch Mech Ind & Mfg Engn, Corvallis, OR 97330 USA
[2] Adv Technol & Mfg Inst ATAMI, Corvallis, OR 97330 USA
[3] Oregon State Univ, Sch Civil & Construct Engn, Corvallis, OR 97330 USA
关键词
Selective laser melting; duplex stainless steel; Corrosion; Annealing; Build Orientation; PITTING CORROSION; LOCALIZED CORROSION; LASER; MICROSTRUCTURE; BEHAVIOR; PRECIPITATION; INCLUSIONS; ANISOTROPY; INITIATION; TEXTURE;
D O I
10.1149/1945-7111/abc5dd
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Grade 2205 Duplex stainless steel (DSS) components were built via selective laser melting (SLM) with gas atomized powder (D-90 < 45 mu m) using a 250 W laser in a nitrogen environment. The relative density was 99.1 0.3%, and the ferrite/austenite phase ratio after annealing was 53.0/47.0 4.8%. Two build orientations (parallel and perpendicular to build direction), as well as as-built SLM (no heat treatment) and annealed conditions, were studied. Corrosion properties were characterized in a 3.5% NaCl electrolyte and compared to 2205 wrought. The charge transfer resistance was > 500 kohm.cm(2), and the corrosion rate was < 100 nA cm(-2) for all alloys, which suggest passivity. No stable pit formation occurred during cyclic polarization tests although the as-built perpendicular and annealed SLM conditions showed metastable pitting, likely due to surface porosity and/or chemical inhomogeneity. The as-built parallel condition did not show metastable pitting and had the highest average charge transfer resistance, which is evidence of possible improvements from laser melted material, but not conclusive. Ultimately, all SLM DSS 2205 was similar to 2205 wrought, implying that the build orientation and annealing were not as significant of factors as the chemical composition in predicting the passivity and pitting resistance.
引用
收藏
页数:11
相关论文
共 66 条
  • [1] [Anonymous], 2017, COMMON EQUIVALENT 31
  • [2] [Anonymous], 2018, ASTM STAND NEWS, V86, P1, DOI [10.1520/G0061-86R18.2, DOI 10.1520/G0061-86R18.2]
  • [3] ASTM, 2018, A890A890M18A ASTM
  • [4] ASTM International, 2018, STAND TEST METH COND
  • [5] Charles J, 2009, DUPLEX STAINLESS STEELS, P47
  • [6] Cramer S.D., 2005, ASM HDB CORROSION MA
  • [7] Selective Laser Melting of Duplex Stainless Steel Powders: An Investigation
    Davidson, Karl
    Singamneni, Sarat
    [J]. MATERIALS AND MANUFACTURING PROCESSES, 2016, 31 (12) : 1543 - 1555
  • [8] Metallographic evaluation of duplex stainless steel powders processed by selective laser melting
    Davidson, Karl P.
    Singamneni, Sarat B.
    [J]. RAPID PROTOTYPING JOURNAL, 2017, 23 (06) : 1146 - 1163
  • [9] An overview of the recurrent failures of duplex stainless steels
    de Farias Azevedo, Cesar Roberto
    Pereira, Henrique Boschetti
    Wolynec, Stephan
    Padilha, Angelo Fernando
    [J]. ENGINEERING FAILURE ANALYSIS, 2019, 97 : 161 - 188
  • [10] Optimizing capacity extensions in power systems: a case study of Bavaria and a comparison to Texas
    Deetjen, Thomas A.
    Webber, Michael E.
    Hueber, Matthias
    [J]. 2017 14TH INTERNATIONAL CONFERENCE ON THE EUROPEAN ENERGY MARKET (EEM 17), 2017,