The high-temperature resistant mechanism of α-starch composite binder for foundry

被引:31
|
作者
Zhou, Xia [1 ]
Yang, Jinzong [2 ]
Su, Depeng [1 ]
Qu, Guohui [3 ]
机构
[1] Dalian Univ Technol, Fac Vehicle Engn & Mech, Dept Engn Mech, State Key Lab Struct Anal Ind Equipment, Dalian 116024, Peoples R China
[2] Dalian Univ Technol, State Key Lab Fine Chem, Dalian 116021, Peoples R China
[3] Dalian Heavy Machinery Enterprise Grp Ltd, Dalian Heavy Cast Iron Plant, Dalian 116022, Peoples R China
关键词
alpha-Starch composite binder; Sand casting; High-temperature resistant mechanism; High-temperature mechanical properties; SAND; CORE;
D O I
10.1016/j.jmatprotec.2009.04.010
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A new binder composed of a-starch, kaolin, sodium silicate, dextrin, phosphate and water in proportions 2.5-4.0%, 1.5-3.0%, 0.55%, 0.35%, 0.04% and 2.5-3.5% by weight percent respectively has been developed. The high-temperature resistant mechanism of the mold and core sand bonded with alpha-starch composite binder was studied by way of differential scanning calorimetry (DSC). X-ray diffraction (XRD), infrared (IR) spectra and scanning electron microscopy (SEM) analyses without sand or on a sand base. It is believed that the high-temperature strength of the sand mold or sand core is mainly dependent on the cohesive strength of the adhesive membrane between sand grains. When the binder was heated over 600 degrees C, the kaolin in it reacted with the sodium silicate and phosphate separately, forming Al-O-Si three-dimensional skeleton and heat-resistant AlPO(4), thus, the binder is provided with higher high-temperature resistant strength. This conclusion is also confirmed by the experimental research on the high-temperature mechanical properties of the binder bonded sand and the microstructure observation of the binding film. The research on the high-temperature resistant mechanism of the starch binder bonded sand is helpful to its high-temperature performance optimization and its application in the foundry industry. Crown Copyright (C) 2009 Published by Elsevier B.V. All rights reserved.
引用
收藏
页码:5394 / 5398
页数:5
相关论文
共 50 条
  • [21] Influence of High-temperature Volatilization on Performance of Bituminous Binder
    Cui Peiqiang
    Zhang Honghua
    Wu Shaopeng
    SILICATE BUILDING MATERIALS - SBM 2013, 2014, 599 : 164 - 167
  • [22] ROLE OF BINDER IN HIGH-TEMPERATURE PELLET STRENGTHENING PROCESS
    TIKHOMIROV, VB
    VOITKOVSKII, YB
    BAKUMOVA, NV
    PASHKOV, NF
    STEEL IN THE USSR, 1988, 18 (09): : 390 - 391
  • [23] A MECHANISM FOR HIGH-TEMPERATURE SUPERCONDUCTIVITY
    OVSHINSKY, SR
    APPLIED SUPERCONDUCTIVITY, 1993, 1 (3-6) : 263 - 267
  • [24] MECHANISM FOR HIGH-TEMPERATURE SUPERCONDUCTIVITY
    EMERY, VJ
    REITER, G
    PHYSICAL REVIEW B, 1988, 38 (07): : 4547 - 4556
  • [25] High-temperature creep of alumosilicate concretes on phosphate binder
    U. Sh. Shayakhmetov
    I. M. Valiev
    K. A. Vasin
    R. S. Malikov
    Refractories and Industrial Ceramics, 1999, 40 : 499 - 502
  • [26] New criterion for superpave high-temperature binder specification
    Dongré, R
    D'Angelo, J
    Reinke, G
    BITUMINOUS BINDERS 2004, 2004, (1875): : 22 - 32
  • [27] Unraveling high-temperature mechanism of NO
    Xu, Kangwei
    Zhang, Wei
    Ye, Yue
    Song, Qianshi
    Zhang, Lidong
    Wang, Xiaohan
    JOURNAL OF ENVIRONMENTAL CHEMICAL ENGINEERING, 2024, 12 (05):
  • [28] High-Temperature Interactions of Metal Oxides and a PVDF Binder
    Rehwoldt, Miles C.
    Wang, Yujie
    Xu, Feiyu
    Ghildiyal, Pankaj
    Zachariah, Michael R.
    ACS APPLIED MATERIALS & INTERFACES, 2022, 14 (07) : 8938 - 8946
  • [29] Principles of Alloying of High-Temperature Nickel Alloys Resistant to High-Temperature Corrosion
    A. D. Koval'
    S. B. Belikov
    E. L. Sanchugov
    Metal Science and Heat Treatment, 2001, 43 (9-10) : 373 - 377
  • [30] Principles of alloying of high-temperature nickel alloys resistant to high-temperature corrosion
    Koval, AD
    Belikov, SB
    Sanchugov, EL
    METAL SCIENCE AND HEAT TREATMENT, 2002, 43 (9-10) : 373 - 377