Effect of heat treatment of polymethyl methacrylate powder on mechanical properties of denture base resin

被引:22
作者
Kawaguchi, Tomohiro [1 ,2 ]
Lassila, Lippo V. J. [1 ]
Sasaki, Hirono [2 ]
Takahashi, Yutaka [2 ]
Vallittu, Pekka K. [1 ]
机构
[1] Univ Turku, Inst Dent, Dept Biomat Sci, BioCity Turku Biomat Res Program, Turku, Finland
[2] Fukuoka Dent Coll, Dept Oral Rehabil, Div Removable Prosthodont, Fukuoka 8140193, Japan
基金
日本学术振兴会;
关键词
Heat treatment; PMMA; Denture base polymer; Flexural property; Interpenetrating polymer network; RESIDUAL MONOMER; REINFORCEMENT; WATER;
D O I
10.1016/j.jmbbm.2014.07.012
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Objectives: The aim of this research was to investigate the effects of heat treatment of polymethyl methacrylate powder on mechanical properties of denture base resin. Methods: PMMA powder was applied after heat treatment at 100 degrees C for 2 h (code: HT100) or 130 degrees C for 2 h (code: HT130). The test specimens were fabricated from autopolymerizing resin to investigate the flexural properties of denture base resin cross-linked with methacrylated dendrimer, the surface microhardness of PMMA beads, and the thickness of the swollen layer of PMMA beads. The specimens were autopolymerized, and all specimens were stored in 37 degrees C water for 24 h. Half of the specimens were immersed in 37 degrees C water for an additional 6 months (water storage period: 24 h and 6 months). The flexural strength and flexural modulus (n=10/group) were measured with a three point bending test. Statistical analysis was performed using ANOVA and the Newman-Keuls test at a significance level of 0.05. Results: Heat treatment and the water storage period had a significant effect on flexural strength. The flexural strength of HT130 showed significantly higher values than in other groups. The surface microhardness of PMMA beads of HT130 showed a significantly greater microhardness than other groups. The thickness of a swollen layer of PMMA beads of HT100 and HT130 was significantly decreased. Conclusions: The flexural strength and the surface microhardness were increased after heat treatment at 130 degrees C. The thickness of a swollen layer of PMMA beads was decreased after heat treatment. (C) 2014 Elsevier Ltd. All rights reserved.
引用
收藏
页码:73 / 78
页数:6
相关论文
共 21 条
[1]  
Anusavice KJ, 2013, PHILLIPS SCI DENT MA, P92
[2]   Release of dibenzoyl peroxide from polymethyl methacrylate denture base resins: An in vitro evaluation [J].
Boeckler, Arne F. ;
Morton, Dean ;
Poser, Sven ;
Dette, Karl-Ernst .
DENTAL MATERIALS, 2008, 24 (12) :1602-1607
[3]   Effect of post-polymerization heat-treatments on degree of conversion, leaching residual MMA and in vitro cytotoxicity of autopolymerizing acrylic repair resin [J].
Bural, Canan ;
Aktas, Esin ;
Deniz, Gunnur ;
Unlucerci, Yesim ;
Kizilcan, Nilgun ;
Bayraktar, Gulsen .
DENTAL MATERIALS, 2011, 27 (11) :1135-1143
[4]   DENTURE FRACTURE - A SURVEY [J].
DARBAR, UR ;
HUGGETT, R ;
HARRISON, A .
BRITISH DENTAL JOURNAL, 1994, 176 (09) :342-345
[5]   THE EFFECT OF PREPARATION CONDITIONS OF ACRYLIC DENTURE BASE MATERIALS ON THE LEVEL OF RESIDUAL MONOMER, MECHANICAL-PROPERTIES AND WATER-ABSORPTION [J].
DOGAN, A ;
BEK, B ;
CEVIK, NN ;
USANMAZ, A .
JOURNAL OF DENTISTRY, 1995, 23 (05) :313-318
[6]   Relining of prosthesis with auto-polymerizing hard denture reline resins: effect of post-polymerization treatment on flexural strength [J].
Ferreira Koyama Takahashi, Jessica Mie ;
Machado, Fernanda Miranda ;
Costa Nunez, Juliana Maria ;
Xediek Consani, Rafael Leonardo ;
Mesquita, Marcelo Ferraz .
GERODONTOLOGY, 2009, 26 (03) :232-236
[7]   The reinforcement of dentures [J].
Jagger, DC ;
Harrison, A ;
Jandt, KD .
JOURNAL OF ORAL REHABILITATION, 1999, 26 (03) :185-194
[8]   THERMOFORMING POLYMETHYL METHACRYLATE [J].
JAGGER, RG ;
OKDEH, A .
JOURNAL OF PROSTHETIC DENTISTRY, 1995, 74 (05) :542-545
[9]  
Jerolimov V, 1991, Acta Stomatol Croat, V25, P17
[10]   Mechanical properties of denture base resin cross-linked with methacrylated dendrimer [J].
Kawaguchi, Tomohiro ;
Lassila, Lippo V. J. ;
Vallittu, Pekka K. ;
Takahashi, Yutaka .
DENTAL MATERIALS, 2011, 27 (08) :755-761