Properties and microstructure of CO2 surface treated cement mortars with subsequent lime-saturated water curing

被引:93
作者
Pan, Xiaoying [1 ]
Shi, Caijun [1 ]
Farzadnia, Nima [1 ]
Hu, Xiang [1 ]
Zheng, Jianlan [2 ]
机构
[1] Hunan Univ, Key Lab Green & Adv Civil Engn Mat & Applicat Tec, Innovat Ctr Green & Adv Civil Engn Mat Hunan Prov, Coll Civil Engn, Changsha 410082, Hunan, Peoples R China
[2] Fujian Jiangxia Univ, Sch Engn, Fuzhou 350116, Fujian, Peoples R China
基金
中国国家自然科学基金;
关键词
Carbonation; Surface treatment; Lime water curing; Permeability; Microstructure; BACTERIAL CARBONATE PRECIPITATION; CONCRETE; PERMEABILITY; DURABILITY; GAS; CORROSION; STRENGTH; PASTES;
D O I
10.1016/j.cemconcomp.2019.03.006
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Previous study has shown that CO2 surface treatment can provide significant protective effects on cement mortar at early ages. This study examines the compressive strength, water permeability, water-vapor transmission and chloride migration of mortars after CO2 surface treatment with subsequent lime water curing. Thermogravimetric analysis (TGA), Fourier Transform Infrared Spectroscopy (FTIR), and Environmental Scanning Electron Microscope (ESEM) combined with Energy Dispersive X-ray Spectroscopy (EDS) analysis were also employed to investigate the underlying microstructure and mechanisms. Results showed that combined effect of CO2 surface treatment and subsequent lime-water curing showed a slight effect on compressive strength, but a significant effect on the impermeability of the mortar. The effect on impermeability increased and calcium carbonate formed during the CO2 surface treatment transformed from amorphous to crystallized form as subsequent the lime water curing period was prolonged. Furthermore, the formation of more C-S-H was observed owing to the hydration of uncarbonated calcium silicates in cement clinker and the reactions of the silica gel from CO2 surface treatment and Ca(OH)(2) from the hydration of uncarbonated calcium silicates.
引用
收藏
页码:89 / 99
页数:11
相关论文
共 54 条
[1]  
Achal V, 2012, ACI MATER J, V109, P157
[2]   Carbonation of surface protected concrete [J].
Aguiar, Jose B. ;
Junior, Cristela .
CONSTRUCTION AND BUILDING MATERIALS, 2013, 49 :478-483
[3]  
American Society for Testing and Materials, 2013, STAND TEST METH WAT
[4]   Surface treatment of concrete bricks using calcium carbonate precipitation [J].
Amidi, Shahrooz ;
Wang, Jialai .
CONSTRUCTION AND BUILDING MATERIALS, 2015, 80 :273-278
[5]   INFRARED-SPECTRA OF AMORPHOUS AND CRYSTALLINE CALCIUM-CARBONATE [J].
ANDERSEN, FA ;
BRECEVIC, L .
ACTA CHEMICA SCANDINAVICA, 1991, 45 (10) :1018-1024
[6]  
[Anonymous], 2008, 8076 GB CHIN NAT STA
[7]  
ASTM International, 2004, STAND TEST METH MEAS, pC1585
[8]   Assessment of the durability of concrete from its permeation properties: a review [J].
Basheer, L ;
Kropp, J ;
Cleland, DJ .
CONSTRUCTION AND BUILDING MATERIALS, 2001, 15 (2-3) :93-103
[9]   Surface treatments for concrete: assessment methods and reported performance [J].
Basheer, PAM ;
Basheer, L ;
Cleland, DJ ;
Long, AE .
CONSTRUCTION AND BUILDING MATERIALS, 1997, 11 (7-8) :413-429
[10]  
Bier T. H. A., 1989, ACI SPEC PUBL, P114