Effects of elevated water temperatures on interfacial delaminations, failure modes and shear strength in externally-bonded CFRP-concrete beams using infrared thermography, gray-scale images and direct shear test

被引:35
作者
Lai, W. L. [1 ]
Kou, S. C. [1 ]
Poon, C. S. [1 ]
Tsang, W. F. [2 ]
Lai, C. C. [2 ]
机构
[1] Hong Kong Polytech Univ, Dept Civil & Struct Engn, Hong Kong, Hong Kong, Peoples R China
[2] Hong Kong Polytech Univ, Dept Bldg & Real Estate, Hong Kong, Hong Kong, Peoples R China
关键词
Accelerated exposure conditions; Delamination; Externally-bonded CFRP and concrete composites; Quantitative infrared thermography (IRT); DURABILITY;
D O I
10.1016/j.conbuildmat.2009.06.012
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
This paper reports the results of a durability study of the effects of exposing externally-bonded CFRP-concrete beams to three elevated water temperatures (25 degrees C, 40 degrees C and 60 degrees C). The effects of the heated water environments on the adhesive bonding layer between the CFRP and concrete beams were evaluated by quantifying: (1) the changes of delaminations within the adhesive bonding layer, (2) the changes in resistance to direct shear force and (3) the changes of failure mode distribution. Before the exposure, the condition of the adhesive bonding layer was inspected by infrared thermography (IRT). After exposure, the deterioration of the same bonding layer and failure mode distributions were measured by analyzing the visual photos on the failed CFRP strips. The failure modes were found to be affected largely by the combined effect of elevated temperature and moisture ingress, in which three types were identified: failure at concrete beams, at adhesive bonding layer and interface between CFRP strip and concrete. With these methods, results of 54 specimens show that the adhesive bonding layers of all the specimens had gradually deteriorated in the 40 degrees C and 60 degrees C water baths. This deterioration was due to the weakening of the adhesive bonding layers when the glass transition temperature (T-g) or the heat distortion temperature (HDT) was approached or even exceeded, and gradual development of delaminations at adhesive bonding layer. (C) 2009 Elsevier Ltd. All rights reserved.
引用
收藏
页码:3152 / 3160
页数:9
相关论文
共 37 条
[1]  
*ACI COMM, 2004, GUID TEST METH FIB R
[2]  
ASTM (American Society for Testing and Materials), 1995, D3039D3039M ASTM
[3]   ACCELERATED TEST METHODS TO DETERMINE THE LONG-TERM BEHAVIOR OF FRP COMPOSITE STRUCTURES - ENVIRONMENTAL-EFFECTS [J].
BANK, LC ;
GENTRY, TR ;
BARKATT, A .
JOURNAL OF REINFORCED PLASTICS AND COMPOSITES, 1995, 14 (06) :559-587
[4]   Definition of a new thermal contrast and pulse correction for defect quantification in pulsed thermography [J].
Benitez, Hernan D. ;
Ibarra-Castanedo, Clemente ;
Bendada, AbdelHakim ;
Maldague, Xavier ;
Loaiza, Humberto ;
Caicedo, Eduardo .
INFRARED PHYSICS & TECHNOLOGY, 2008, 51 (03) :160-167
[5]  
BYARS EA, 2000, VEN CAMBR M FIB TASK
[6]  
*CEB FIP TASK GROU, 2001, COM EUR BET B, V14
[7]   Shear capacity of FRP-strengthened RC beams: FRP debonding [J].
Chen, JF ;
Teng, JG .
CONSTRUCTION AND BUILDING MATERIALS, 2003, 17 (01) :27-41
[8]  
EWAN AB, 2003, INT J MATER PROD TEC, V19, P28
[9]   Water effects on the bond strength of concrete/concrete adhesive joints [J].
Frigione, M. ;
Aiello, M. A. ;
Naddeo, C. .
CONSTRUCTION AND BUILDING MATERIALS, 2006, 20 (10) :957-970
[10]   Non-destructive defect characterization of concrete structures reinforced by means of FRP [J].
Galletti, U. ;
Luprano, V. ;
Nenna, S. ;
Spagnolo, L. ;
Tundo, A. .
INFRARED PHYSICS & TECHNOLOGY, 2007, 49 (03) :218-223