Basswood has been converted to a porous biocarbon template by carbonizing under vacuum at 1200degreesC. Subsequent reactive infiltration of gaseous silicon at 1500-1700degreesC for 0.5-8 h in inert atmosphere resulted in the formation of a porous, cellular beta-SiC ceramic. X-ray diffraction (XRD) studies show the resulting SiC, obtained at 1600degreesC for 6 h in static argon atmosphere, is beta-SiC. Scanning electron microscopy (SEM) reveals the resulting SiC ceramic reproduces the biomorphic cellular morphology of basswood tissue with high precision. Gaseous Si diffuses into charcoal through its continuous tracheidal cell channels, and reacts with carbon in the cell wall to form SiC. Growth of SiC layer is dependent of the diffusion of Si vapor through the primary porous SiC layer and further gas-solid reaction of Si(g) and C(s) at C/SiC interface. The densification of SiC strut material may occur at moderate temperatures and holding time. (C) 2003 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:947 / 951
页数:5
相关论文
共 20 条
  • [1] Gibson E., 1992, MET MATER, V8, P333
  • [2] Biomorphic cellular silicon carbide ceramics from wood: I. Processing and microstructure
    Greil, P
    Lifka, T
    Kaindl, A
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1998, 18 (14) : 1961 - 1973
  • [3] Effect of microstructure on the fracture behavior of biomorphous silicon carbide ceramics
    Greil, P
    Vogli, E
    Fey, T
    Bezold, A
    Popovska, N
    Gerhard, H
    Sieber, H
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2002, 22 (14-15) : 2697 - 2707
  • [4] Near net shape manufacturing of ceramics
    Greil, P
    [J]. MATERIALS CHEMISTRY AND PHYSICS, 1999, 61 (01) : 64 - 68
  • [5] Effect of carbonizing speed on the property changes of woodceramics impregnated with liquefacient wood
    Hirose, T
    Fan, TX
    Okabe, T
    Yoshimura, M
    [J]. MATERIALS LETTERS, 2002, 52 (03) : 229 - 233
  • [6] KAINDL A, 2000, THESIS U ERLANGEN NU
  • [7] High temperature compressive mechanical behavior of biomorphic silicon carbide ceramics
    Martínez-Fernández, J
    Valera-Feria, FM
    Singh, M
    [J]. SCRIPTA MATERIALIA, 2000, 43 (09) : 813 - 818
  • [8] High temperature compressive mechanical behavior of joined biomorphic silicon carbide ceramics
    Muñoz, A
    Fernández, JM
    Singh, M
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2002, 22 (14-15) : 2727 - 2733
  • [9] Porous titania ceramic prepared by mimicking silicified wood
    Ota, T
    Imaeda, M
    Takase, H
    Kobayashi, M
    Kinoshita, N
    Hirashita, T
    Miyazaki, H
    Hikichi, Y
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2000, 83 (06) : 1521 - 1523
  • [10] Biomimetic process for producing SiC ''wood''
    Ota, T
    Takahashi, M
    Hibi, T
    Ozawa, M
    Suzuki, S
    Hikichi, Y
    Suzuki, H
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1995, 78 (12) : 3409 - 3411