The effects of steel composition on the oxidation kinetics, scale structure, and scale-steel interface adherence of low and ultra-low carbon steels

被引:8
作者
Chen, Rex Y.
Yuen, W. Y. D.
机构
[1] BlueScope Steel Western Port Works, Hastings, Vic 3915, Australia
[2] BlueScope Steel Res, Port Kembla, NSW 2505, Australia
来源
HIGH-TEMPERATURE OXIDATION AND CORROSION 2005 | 2006年 / 522-523卷
关键词
oxidation; low carbon steel; IF Steel; oxide scale;
D O I
10.4028/www.scientific.net/MSF.522-523.451
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The oxidation behaviors of several commercial low and ultra low carbon steels in air at 700-950 degrees C were studied. Under isothermal oxidation conditions, the oxidation kinetics, scale structure and scale-steel interface adherence were significantly affected by the steel composition.
引用
收藏
页码:451 / 459
页数:9
相关论文
共 50 条
  • [21] Effects of Manganese on Deformation of Oxide Scale on Low-carbon Steel Sheet during Hot Rolling
    Nishio, Koharu
    Matsumoto, Ryo
    Utsunomiya, Hiroshi
    Hayashi, Kosuke
    Hidaka, Yasuyoshi
    Sugiyama, Masaaki
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2023, 109 (09): : 27 - 32
  • [22] Characteristics of scale/substrate interface area of Si-containing low-carbon steels at high temperatures
    Taniguchi, S
    Yamamoto, K
    Megumi, D
    Shibata, T
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 308 (1-2): : 250 - 257
  • [23] Characteristic Fatigue Crack Growth Behavior of Low Carbon Steel under Low-pressure Hydrogen Gas Atmosphere in an Ultra-low Frequency
    Onishi, Yosuke
    Koyama, Motomichi
    Sasaki, Daisuke
    Noguchi, Hiroshi
    ISIJ INTERNATIONAL, 2016, 56 (05) : 855 - 860
  • [24] Grain Subdivision Mechanism For Constructing Lamellar Microstructure In Cold-Rolled Ultra-Low Carbon Steel
    Morikawa, Tatsuya
    Kurosaka, Ryuta
    Tanaka, Masaki
    Ichie, Takeru
    Murakami, Ken-ichi
    ISIJ INTERNATIONAL, 2022, 62 (02) : 335 - 342
  • [25] Strain Distribution Analysis Using Precise Markers in Cold-Rolled Ultra-Low Carbon Steel
    Morikawa, Tatsuya
    Kurosaka, Ryuta
    Tanaka, Masaki
    Ichie, Takeru
    Murakami, Ken-ichi
    ISIJ INTERNATIONAL, 2022, 62 (10) : 2069 - 2073
  • [26] A study on oxide scale formation of low carbon steel using thermo gravimetric technique
    Wikstrom, P.
    Blasiak, W.
    Du, S. C.
    IRONMAKING & STEELMAKING, 2008, 35 (08) : 621 - 632
  • [27] Precipitation behavior of magnetite in oxide scale during cooling of microalloyed low carbon steel
    Yu, Xianglong
    Jiang, Zhengyi
    Yang, Daijun
    Wei, Dongbin
    Yang, Quan
    ADVANCES IN ROLLING EQUIPMENT AND TECHNOLOGIES II, 2012, 572 : 249 - +
  • [28] ON THE EFFECTS OF PREDEFORMATION ON WORK-HARDENING OF ULTRA-LOW-CARBON SHEET STEEL
    MIRSHAMS, RA
    MOHAMADIAN, HP
    CROSBY, KE
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 1994, 3 (01) : 65 - 71
  • [29] Thermodynamic and experimental study on CO2 injection in RH decarburization process of ultra-low carbon steel
    Chen, Gujun
    Yang, Jiang
    Li, Long
    Zhang, Min
    He, Shengping
    JOURNAL OF CO2 UTILIZATION, 2021, 50
  • [30] The influence of cooling conditions on the secondary scale in hot rolled low carbon steel wire rod
    Baarman, MH
    Fredriksson, JT
    SCANDINAVIAN JOURNAL OF METALLURGY, 1999, 28 (01) : 25 - 32