Comparative study of wear performance of ceramic/iron composite coatings under two different wear modes

被引:15
作者
Wang, Wenqin [1 ]
Wang, De [2 ]
Yamaguchi, Tomiko [3 ]
Nishio, Kazumasa [4 ]
Yan, Ming [5 ]
Li, Yulong [1 ,6 ]
机构
[1] Nanchang Univ, Sch Mech & Elect Engn, Nanchang 330031, Jiangxi, Peoples R China
[2] Jiangxi Acad Sci, Inst Appl Phys, Nanchang 330029, Jiangxi, Peoples R China
[3] Kyushu Inst Technol, Fac Engn, Fukuoka 8040015, Japan
[4] Nishinippon Inst Technol, Fukuoka 8030812, Japan
[5] South Univ Sci & Technol China, Dept Mat Sci & Engn, Shenzhen 518055, Peoples R China
[6] Nanchang Univ, Key Lab Robot & Welding Automat Jiangxi Prov, Nanchang 330031, Jiangxi, Peoples R China
关键词
Resistance seam welding; A6061; WC-SHA coating; Wear resistance; AL-ALLOY SUBSTRATE; WC-CO COATINGS; ALUMINUM-ALLOY; CORROSION BEHAVIOR; SLIDING WEAR; RESISTANCE; MICROSTRUCTURE; STEEL; RECONSTRUCTION; PARTICLES;
D O I
10.1016/j.surfcoat.2016.11.059
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
WC-SHA coatings (SHA: high carbon iron alloy) with varying WC contents were successfully fabricated on Al-Mg-Si alloy substrates by resistance seam welding. The microstructures and phase compositions were investigated. Wear performance of the coatings was evaluated by both rubber wheel test and ball-on-disc test. The results showed that dense and thick WC-SHA coatings, consisting of WC reinforcement, SHA binder, A6061 and FeAl3, were fabricated on A6061 alloy using different powders. With increasing the contents of WC particles, the surface wear resistance and hardness increases. Moreover, the WC particles behaved significantly different during different wear tests, resulting in different wear mechanisms of the coating. In rubber wheel test, the WC particles relieved the abrasive wear on A6061 and SHA components from abrasive particles. While in ball-on-disc test, the WC particles supported the pressure from counterpart and protected other components until the WC particles were peeled off, leading to three body abrasive wear. (C) 2016 Elsevier B.V. All rights reserved.
引用
收藏
页码:136 / 148
页数:13
相关论文
共 50 条
  • [1] Dry machining of aluminum-silicon alloy using polished CVD diamond-coated cutting tools inserts
    Arumugam, PU
    Malshe, AP
    Batzer, SA
    [J]. SURFACE & COATINGS TECHNOLOGY, 2006, 200 (11) : 3399 - 3403
  • [2] Wear and corrosion behaviour of HVOF WC-CoCr/CVD DLC hybrid coating systems deposited onto aluminium substrate
    Bolelli, G.
    Bonferroni, B.
    Coletta, G.
    Lusvarghi, L.
    Pitacco, F.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2011, 205 (17-18) : 4211 - 4220
  • [3] Micromechanical properties and sliding wear behaviour of HVOF-sprayed Fe-based alloy coatings
    Bolelli, Giovanni
    Bonferroni, Benedetta
    Laurila, Jussi
    Lusvarghi, Luca
    Milanti, Andrea
    Niemi, Kari
    Vuoristo, Petri
    [J]. WEAR, 2012, 276 : 29 - 47
  • [4] Dehghan Hamedan A., 2012, MAT SCI ENG A-STRUCT, V556, P921
  • [5] Cold spray deposition of a WC-25Co cermet onto Al7075-T6 and carbon steel substrates
    Dosta, S.
    Couto, M.
    Guilemany, J. M.
    [J]. ACTA MATERIALIA, 2013, 61 (02) : 643 - 652
  • [6] Wear mechanism maps for thermal-spray steel coatings
    Edrisy, A
    Perry, T
    Alpas, AT
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2005, 36A (10): : 2737 - 2750
  • [7] Improved ball crater micro-abrasion test based on a ball on three disk configuration
    Fildes, J. M.
    Meyers, S. J.
    Kilaparti, R.
    Schlepp, E.
    [J]. WEAR, 2012, 274 : 414 - 422
  • [8] Microstructural aspects determining the adhesive wear of tool steels
    Fontalvo, GA
    Humer, R
    Mitterer, C
    Sammt, K
    Schemmel, I
    [J]. WEAR, 2006, 260 (9-10) : 1028 - 1034
  • [9] Guilemany JM, 2005, J THERM SPRAY TECHN, V14, P405, DOI 10.1361/105996305X59350
  • [10] Effects of WC-Ni content on microstructure and wear resistance of laser cladding Ni-based alloys coating
    Guo, Chun
    Chen, Jianmin
    Zhou, Jiansong
    Zhao, Jierong
    Wang, Lingqian
    Yu, Youjun
    Zhou, Huidi
    [J]. SURFACE & COATINGS TECHNOLOGY, 2012, 206 (8-9) : 2064 - 2071