The Effects of Rare Earth Pr and Heat Treatment on the Wear Properties of AZ91 Alloy

被引:12
|
作者
Li, Ning [1 ,2 ]
Yan, Hong [1 ]
机构
[1] Nanchang Univ, Sch Mech Elect Engn, Nanchang 330031, Jiangxi, Peoples R China
[2] Nanchang Hangkong Univ, Sch Aviat Mfg Engn, Nanchang 330069, Jiangxi, Peoples R China
来源
CRYSTALS | 2018年 / 8卷 / 06期
基金
中国国家自然科学基金;
关键词
AZ91; alloy; Pr; heat treatment; wear resistance; MAGNESIUM ALLOY; TRIBOLOGICAL BEHAVIOR; ELEVATED-TEMPERATURES;
D O I
10.3390/cryst8060256
中图分类号
O7 [晶体学];
学科分类号
0702 ; 070205 ; 0703 ; 080501 ;
摘要
This paper investigated the influences of Pr addition and heat treatment (T6) on the dry sliding wear behavior of AZ91 alloy. The wear rates and friction coefficients were measured by using a pin-on-disc tribometer under loads of 30, 60 and 90 N at dry sliding speeds of 100 rpm, over a sliding time of 15 min. The worn surfaces were examined using a scanning electron microscope and was analyzed with an energy dispersive spectrometer. The experimental results revealed that AZ91-1.0%Pr magnesium alloy exhibited lower wear rate and friction coefficient than the other investigated alloys. As the applied load increased, the wear rate and friction coefficient increased. Compared with the as-cast AZ91-1.0%Pr magnesium alloy, the hardness and wear resistance of the alloy after solution treatment were reduced, and through the subsequent aging, the hardness and wear resistance of the alloy were improved and the hardness was 101.1 HB (compared to as-cast AZ91 magnesium alloy, it increased by 45%). The AZ91-1.0%Pr with T6 magnesium alloy exhibited best wear resistance. Abrasion was dominant at load of 30 N, delamination was dominant at load of 60 N and plastic deformation was dominant at load of 90 N. Oxidation was observed at all loads.
引用
收藏
页数:13
相关论文
共 50 条
  • [41] The effect of the β phase and heat treatment on the corrosion behavior of magnesium AZ91 alloy
    Uzan, P
    Eliezer, D
    Aghion, E
    SYNTHESIS OF LIGHTWEIGHT METALS III, 1999, : 171 - 176
  • [42] Microstructural Evolution of AZ91 Magnesium Alloy during Deformation and Heat Treatment
    Li, Jing-Yuan
    Xie, Jian-Xin
    ADVANCES IN MATERIALS AND PROCESSING TECHNOLOGIES II, PTS 1 AND 2, 2011, 264-265 : 66 - 71
  • [43] Microstructural evolution of AZ91 magnesium alloy during extrusion and heat treatment
    Li Jing-yuan
    Xie Jian-xin
    Jin Jun-bing
    Wang Zhi-xiang
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2012, 22 (05) : 1028 - 1034
  • [44] Influence of heat treatment on the machinability and corrosion behavior of AZ91 Mg alloy
    Chowdary, Swetha, V
    Dumpala, Ravikumar
    Kumar, Anand S.
    Kondaiah, V. V.
    Sunil, Ratna B.
    JOURNAL OF MAGNESIUM AND ALLOYS, 2018, 6 (01) : 52 - 58
  • [45] Effect of Intermetallic Phases on Corrosion Initiation of AZ91 Alloy With Rare Earth Y Addition
    Zhang, Li-na
    Jia, Ruiling
    Li, Dan
    Zhang, Wei
    Guo, Feng
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2015, 31 (05) : 504 - 511
  • [46] Effect of rare earth elements addition on thermal fatigue behaviors of AZ91 magnesium alloy
    Hossein Bayani
    Ehsan Saebnoori
    Journal of Rare Earths, 2009, 27 (02) : 255 - 258
  • [47] Effect of rare earth elements addition on thermal fatigue behaviors of AZ91 magnesium alloy
    Bayani, Hossein
    Saebnoori, Ehsan
    JOURNAL OF RARE EARTHS, 2009, 27 (02) : 255 - 258
  • [48] Effect of rare earth additions on microstructure and mechanical properties of AZ91 magnesium alloys
    佟国栋
    刘海峰
    刘耀辉
    TransactionsofNonferrousMetalsSocietyofChina, 2010, 20(S2) (S2) : 336 - 340
  • [49] Effect of rare earth additions on microstructure and mechanical properties of AZ91 magnesium alloys
    Tong Guo-dong
    Liu Hai-feng
    Liu Yao-hui
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2010, 20 : S336 - S340
  • [50] Effect of rare earth additions on microstructure and mechanical properties of AZ91 magnesium alloys
    Tong G.-D.
    Liu H.-F.
    Liu Y.-H.
    Transactions of Nonferrous Metals Society of China (English Edition), 2010, 20 (SUPPL. 2): : s336 - s340