A preliminary analysis of failures in grey cast iron water pipes

被引:54
作者
Makar, JM [1 ]
机构
[1] Natl Res Council Canada, Inst Res Construct, Ottawa, ON K2P 0W4, Canada
关键词
brittle fracture; corrosion; grey iron; fitting corrosion; water pipes;
D O I
10.1016/S1350-6307(99)00005-9
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Most water utility engineers are familiar with the typical failure modes of grey cast iron pipes such as circumferential breaks and split bells. However, while researchers have examined the forces that are likely responsible for these failures, the failure mechanisms that link those forces with the observed failures have not been thoroughly investigated. Understanding these mechanisms is important for finding ways of detecting damaged pipes and preventing their ultimate failure. This paper presents a failure analysis of five different pipes that show four different failure modes. The analysis suggests that some of these failures occurred in at least two stages, raising the possibility that non-destructive testing could be used to detect pipes that are part way possibility through the failure process. Crown Copyright (C) 1999 Published by Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:43 / 53
页数:11
相关论文
共 20 条
[1]  
[Anonymous], J AM WATER WORKS ASS
[2]  
Arnold G.E, 1960, J AM WATER WORKS ASS, V52, P1041, DOI [10.1002/j.1551-8833.1960.tb00569.x, DOI 10.1002/J.1551-8833.1960.TB00569.X]
[3]  
*CAST IR PIP RES A, 1952, HDB CAST IR PIP WAT
[4]  
De Rose PJ, 1985, TR241 WRC ENG WAT RE
[5]  
HABIBIAN A, 1994, J TRANSP ENG-ASCE, V120, P312, DOI 10.1061/(ASCE)0733-947X(1994)120:2(312)
[6]  
JAKOBS JA, 1985, UNDERGROUND CORROSIO
[7]  
Kirmeyer G.J., 1994, ASSESSMENT WATER DIS
[8]  
KITAURA M, 1996, DAMAGE WATER SUPPLY, P325
[9]  
KOTTMANN A, 1994, P 2 INT C WAT PIP SY, P11
[10]   Damage to water distribution system caused by the 1995 Hyogo-ken Nanbu earthquake [J].
Kuraoka, S ;
Rainer, JH .
CANADIAN JOURNAL OF CIVIL ENGINEERING, 1996, 23 (03) :665-677