Microstructure and high-temperature oxidation behavior of wire-arc sprayed Fe-based coatings

被引:23
作者
Li, Ran [1 ]
Zhou, Zheng [1 ]
He, Dingyong [1 ]
Zhao, Lidong [2 ]
Song, Xiaoyan [1 ]
机构
[1] Beijing Univ Technol, Coll Mat Sci & Engn, Beijing, Peoples R China
[2] Rhein Westfal TH Aachen, Inst Oberflachentech, Aachen, Germany
关键词
Fe-based coating; Wire-arc spray; Cored wire; High-temperature oxidation; HOT CORROSION BEHAVIOR; NI-BASED SUPERALLOY; NA2SO4-60-PERCENT-V2O5; ENVIRONMENT; IRON; CR; RESISTANCE; ALLOYS; 900-DEGREES-C; NICRBSI; NICKEL;
D O I
10.1016/j.surfcoat.2014.04.024
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A series of Fe-xCr cored wires (x = 15, 20, 25, 30, 35 and 40% in weight) were used to produce protective coatings for components used in high-temperature environments by wire-arc spraying. The microstructure, morphology and high-temperature oxidation behavior of the Fe-xCr coatings were investigated. The Fe-xCr coatings presented a homogeneous structure with thin oxide inclusions and low porosity. Thermogravimetric analysis was used to evaluate the high-temperature oxidation behavior of the coatings at a temperature of 650 degrees C under cyclic oxidation conditions. The results showed that all the Fe-xCr coatings exhibited significantly lower weight gain than the uncoated substrate. As Cr content of the coatings increased, the thickness of oxide scales decreased and oxidation resistance improved. (C) 2014 Elsevier B.V. All rights reserved.
引用
收藏
页码:186 / 190
页数:5
相关论文
共 27 条
[1]   The Toxic Effects of Nickel Chloride on Liver, Erythropoiesis, and Development in Wistar albino Preimplanted Rats Can Be Reversed with Selenium Pretreatment [J].
Adjroud, Ounassa .
ENVIRONMENTAL TOXICOLOGY, 2013, 28 (05) :290-298
[2]   Erosion resistance of arc-sprayed coatings to iron ore at 25 and 315 °C [J].
Dallaire, S ;
Levert, H ;
Legoux, JG .
JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2001, 10 (02) :337-350
[3]   OXIDATION OF FE-CR SURFACE AND BULK ALLOYS AT 300-DEGREES-C [J].
DRISCOLL, TJ ;
NEEDHAM, PB .
OXIDATION OF METALS, 1979, 13 (03) :283-298
[4]   Deposition and corrosion resistance of HVOF sprayed nanocrystalline iron aluminide coatings [J].
Ji, G ;
Elkedim, O ;
Grosdidier, T .
SURFACE & COATINGS TECHNOLOGY, 2005, 190 (2-3) :406-416
[5]   Hot corrosion behavior of detonation gun sprayed Cr3C2-NiCr coatings on Ni and Fe-based superalloys in Na2SO4-60%V2O5 environment at 900°C [J].
Kamal, Subhash ;
Jayaganthan, R. ;
Prakash, S. ;
Kumar, Sanjay .
JOURNAL OF ALLOYS AND COMPOUNDS, 2008, 463 (1-2) :358-372
[6]   Evaluation of cyclic hot corrosion behaviour of detonation gun sprayed Cr3C2-25%NiCr coatings on nickel- and iron-based superalloys [J].
Kamal, Subhash ;
Jayaganthan, R. ;
Prakash, Satya .
SURFACE & COATINGS TECHNOLOGY, 2009, 203 (08) :1004-1013
[7]   High-Temperature Erosion-Corrosion Performance of High-Velocity Oxy-Fuel Sprayed Ni-20 Cr Coating in Actual Boiler Environment [J].
Kaushal, G. ;
Singh, H. ;
Prakash, S. .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2011, 42A (07) :1836-1846
[8]   Evaluation of new corrosion-resistant superheater tubing in high-efficiency waste-to-energy plants [J].
Kawahara, Y ;
Nakamura, M ;
Tsuboi, H ;
Yukawa, K .
CORROSION, 1998, 54 (07) :576-589
[9]   High temperature corrosion of pure Fe, Cr and Fe-Cr binary alloys in O2 containing trace KCl vapour at 750 °C [J].
Ma, H. T. ;
Zhou, C. H. ;
Wang, L. .
CORROSION SCIENCE, 2009, 51 (08) :1861-1867
[10]   THE OBSERVATION OF STRESS EFFECTS DURING THE HIGH-TEMPERATURE OXIDATION OF IRON [J].
MITCHELL, TE ;
VOSS, DA ;
BUTLER, EP .
JOURNAL OF MATERIALS SCIENCE, 1982, 17 (06) :1825-1833