Solid-Solution Effects on the High-Temperature Oxidation Behavior of Polymer-Derived (Hf,Ta)C/SiC and (Hf,Ti)C/SiC Ceramic Nanocomposites

被引:34
作者
Wen, Qingbo [1 ]
Riedel, Ralf [1 ]
Ionescu, Emanuel [1 ]
机构
[1] Tech Univ Darmstadt, Inst Mat Sci, Otto Berndt Str 3, D-64287 Darmstadt, Germany
关键词
hafnium carbide; high-temperature oxidation; passivation; solid solution; ultrahigh-temperature ceramic nanocomposites; SOURCE-PRECURSOR SYNTHESIS; DIBORIDE-SILICON-CARBIDE; ABLATION BEHAVIOR; HAFNIUM CARBIDE; THERMAL-EXPANSION; KINETICS; COMPOSITES; STABILITY; MICROSTRUCTURE; INFILTRATION;
D O I
10.1002/adem.201800879
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In the present study, two concepts to improve the oxidation resistance at high-temperatures of ceramic nanocomposites consisting of 85-90 vol% SiC, 5-8 vol% group IV metal carbides (i.e., HfC, TaC), and 5-7 vol% carbon are introduced and discussed. First improvement concept relates to the passivation of the samples upon short-term oxidation at 1400 degrees C (30 min). This is a critical step, especially with respect to silica formation, which is relatively sluggish at temperatures lower than 1000-1200 degrees C. Moreover, solid-solution metal carbides (Hf,Ta)C and (Hf,Ti)C are shown to be clearly more oxidation resistant than the binary HfC and TaC phases. Whereas, the solid-solution effect contributes to a significant improvement of the short-term oxidation resistance of the studied nanocomposites, the passivation of the materials prior exposure of high-temperature oxidation conditions provides a remarkably improved long-term behavior thereof. Possible mechanisms involved in the oxidation processes of (Hf,Ta)C/SiC and (Hf,Ti)/SiC ceramic nanocomposites are highlighted and critically assessed.
引用
收藏
页数:11
相关论文
共 50 条
[21]   Microstructure, mechanical properties and ablation behavior of ultra-high-temperature Ta-Hf-C solid solution coating prepared by a step-by-step plasma solid solution method [J].
Tan, Z. Y. ;
Zhu, W. ;
Yang, L. ;
Zhou, Y. C. ;
Wu, Q. ;
Gong, L. J. .
SURFACE & COATINGS TECHNOLOGY, 2020, 403
[22]   Oxidation Behavior and Meso-macro Model of Tubular C/SiC Composites in High-temperature Environment [J].
Quan, Wenxin ;
Yu, Yiping ;
Fang, Bing ;
Li, Wei ;
Wang, Song .
JOURNAL OF INORGANIC MATERIALS, 2024, 39 (08) :921-928
[23]   High-temperature phase and microstructure evolution of polymer-derived SiZrCN and SiZrBCN ceramic nanocomposites [J].
Feng, Bo ;
Peter, Johannes ;
Fasel, Claudia ;
Wen, Qingbo ;
Zhang, Yue ;
Kleebe, Hans-Joachim ;
Ionescu, Emanuel .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2020, 103 (12) :7001-7013
[24]   Ablation behavior of graphite-film-modified C/C and C/C-(Hf, Ta) C-SiC composites [J].
Chen, Lei ;
Yang, Xin ;
Fang, Cunqian ;
Shi, Anhong ;
Zhang, Ze ;
Huang, Qizhong .
DIAMOND AND RELATED MATERIALS, 2025, 154
[25]   Fabrication, Microstructural Evolution, and Mechanical Properties of SiC/(Hf0.25Ta0.25Zr0.25Nb0.25)C/C Nanocomposites [J].
Wang, Zhenyue ;
Zhou, Tianci ;
Yang, Xiantao ;
Liu, Yuenong ;
Wen, Qingbo ;
Yu, Zhaoju .
MATERIALS, 2024, 17 (21)
[26]   The effect of SiC whiskers addition on the microstructure and mechanical properties of a (Hf-Ta-Zr-Nb-Ti)C-SiC composite [J].
Hrubovcakova, Monika ;
Csanadi, Tamas ;
Sedlak, Richard ;
Kovalcikova, Alexandra ;
Shepa, Ivan ;
Mudra, Erika ;
Sopcak, Tibor ;
Unsal, Hakan ;
Tatarko, Peter ;
Sajgalik, Pavol ;
Dusza, Jan .
CERAMICS INTERNATIONAL, 2023, 49 (14) :24179-24186
[27]   Ablation behavior of C/C composites matrix-modified by solid solution ceramic (Ta,Zr)C-SiC with different Zr/Ta ratios [J].
Zhou, Yuanming ;
Li, Shuxin ;
Zhu, Shuangxing ;
Liu, Ruizhi ;
Tang, Zhenxiao ;
Yi, Maozhong ;
Peng, Ke .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2025, 45 (13)
[28]   Enhanced Toughness of High-Entropy (Ti0.2Zr0.2Hf0.2Nb0.2Ta0.2)C Ceramics with SiC Whiskers by High-Pressure and High-Temperature Sintering [J].
Li, Hao ;
Yang, Zhenxing ;
Lian, Min ;
Ma, Shuailing ;
Li, Wei ;
Wei, Xinmiao ;
Zhao, Xingbin ;
Pan, Yilong ;
She, Yunfeng ;
Dang, Lingyan ;
Yuan, Bao ;
Cui, Tian .
MATERIALS, 2025, 18 (07)
[29]   Low-temperature reactive hot-pressing of Ta0.2Hf0.8C-SiC ceramics at 1700°C [J].
Qin, Yanyan ;
Ni, Dewei ;
Chen, Bowen ;
Lu, Jun ;
Cai, Feiyan ;
Zou, Xuegang ;
Gao, Le ;
Zhang, Xiangyu ;
Ding, Yusheng ;
Dong, Shaoming .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2023, 106 (07) :4390-4398
[30]   Preparation and ablation behavior of solid solution ceramic Ta0.2Zr0.8C-SiC matrix-modified C/C composites under high heat flux [J].
Zhou, Yuanming ;
Tang, Zhenxiao ;
Liu, Ruizhi ;
Zhou, Zhe ;
Yi, Maozhong ;
Peng, Ke .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2025, 35 :1875-1888