Influence of heat treatment conditions on the mechanical properties of Ti-6Al-4V alloy

被引:27
作者
El-Hadad, S. [1 ]
Nady, M. [2 ]
Khalifa, W. [2 ]
Shash, A. [3 ]
机构
[1] Cent Met Res & Dev Inst, Dept Mfg Technol, Helwan, Egypt
[2] Cairo Univ, Fac Engn, Dept Min Petr & Met Engn, Giza, Egypt
[3] Cairo Univ, Fac Engn, Dept Mech Design & Prod, Giza, Egypt
关键词
Ti-6Al-4V alloy; heat treatment; microstructure; mechanical properties; PHASE-TRANSFORMATION; TITANIUM-ALLOY; MICROSTRUCTURE; DEFORMATION; BEHAVIOR; EVOLUTION;
D O I
10.1080/00084433.2017.1412557
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
In the current work, several heat treatments were carried out below and above the beta-transition temperature of the Ti-6Al-4V alloy followed by aging at 550 degrees C for 6 hours. The resultant microstructures and their effects on the mechanical properties of Ti-6Al-4V alloy were investigated. The results showed that solution treatment of Ti-6Al-4V samples followed by water quenching from and alpha/beta fields raised the alloy hardness from 380 to 575 and 656HV, respectively, while no remarkable changes were observed after aging. The hot tensile strength of the as-forged sample increased from 671 to 756MPa after water quenching from the beta- or alpha/beta- field, while the air cooling from beta-phase field decreased the tensile strength to 644 MPa. The fracture mode of the tensile samples was more ductile in case of the solution-treated samples compared to the as-forged samples. A subsurface layer was formed due to the diffusion of oxygen into the surface at high temperatures. This layer which is known as 'oxygen diffusion layer' masked the differences of wear behaviour of the specimens. .
引用
收藏
页码:186 / 193
页数:8
相关论文
共 18 条
[1]   Effect of hot working and post-deformation heat treatment on microstructure and tensile properties of Ti-6Al-4V alloy [J].
Abbasi, S. M. ;
Momeni, A. .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2011, 21 (08) :1728-1734
[2]  
[Anonymous], 2010, ASM HDB ONL, P483
[3]  
Boyer R., 1994, MAT PROPERTIES HDB, P3
[4]   Microstructural effects on corrosion behaviour of investment cast Ti-6.5Al-3.4Mo-1.7Zr alloy [J].
El-Hadad, S. ;
Mhaede, M. ;
Ibrahiem, K. M. .
INTERNATIONAL JOURNAL OF CAST METALS RESEARCH, 2016, 29 (04) :243-250
[5]  
El-Hadad S, 2015, AES ATEMA 22 INT C A
[6]  
Ganesh B.K.C., 2012, Journal of Minerals and Minerals Characterization and Engineering, V11, P735, DOI DOI 10.4236/JMMCE.2012.117061
[7]   The evolution of microstructure of Ti-6Al-4V alloy during concurrent hot deformation and phase transformation [J].
He, Lijia ;
Dehghan-Manshadi, A. ;
Dippenaar, R. J. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 549 :163-167
[8]   The effect of annealing temperatures and cooling rates on microstructure and mechanical properties of investment cast Ti-6Al-4V alloy [J].
Jovanovic, MT ;
Tadic, S ;
Zec, S ;
Miskovic, Z ;
Bobic, I .
MATERIALS & DESIGN, 2006, 27 (03) :192-199
[9]  
Leyens Christoph., 2006, Titanium and Titanium Alloys: Fundamentals and Applications
[10]  
Lutjering G, 2007, ENG MAT PROCESSES SE