Printed circuit board recycling: Physical processing and copper extraction by selective leaching

被引:149
作者
Silvas, Flavia P. C. [1 ]
Jimenez Correa, Monica M. [1 ]
Caldas, Marcos P. K. [1 ,2 ]
de Moraes, Viviane T. [1 ]
Espinosa, Denise C. R. [1 ]
Tenorio, Jorge A. S. [1 ]
机构
[1] Univ Sao Paulo, Polytech Sch, Dept Chem Engn, BR-05424970 Sao Paulo, Brazil
[2] Fed Inst Technol Sci & Educ Espirito Santo, BR-29173087 Serra, ES, Brazil
基金
巴西圣保罗研究基金会;
关键词
Copper; Leaching; Recycling; WEEE; ELECTRONIC EQUIPMENT; METAL RECOVERY; MOBILE PHONES; WIRING BOARDS; WASTE; SEPARATION; SCRAP; DISSOLUTION;
D O I
10.1016/j.wasman.2015.08.030
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Global generation of waste electrical and electronic equipment (WEEE) is about 40 million tons per year. Constant increase in WEEE generation added to international legislations has improved the development of processes for materials recovery and sustainability of electrical and electronic industry. This paper describes a new hydrometallurgical route (leaching process) to recycle printed circuit boards (PCBs) from printers to recover copper. Methodology included PCBs characterization and a combined route of physical and hydrometallurgical processing. Magnetic separation, acid digestion and chemical analysis by ICP-OES were performed. On leaching process were used two stages: the first one in a sulfuric media and the second in an oxidant media. The results showed that the PCBs composition was 74.6 wt.% of non-magnetic material and 25.4 wt.% of magnetic one. The metallic fraction corresponded to 44.0 wt.%, the polymeric to 28.5 wt.% and the ceramic to 27.5 wt.%. The main metal was copper and its initial content was 32.5 wt.%. On sulfuric leaching 90 wt.% of Al, 40 wt.% of Zn and 8.6 wt.% of Sn were extracted, whereas on oxidant leaching tests the extraction percentage of Cu was 100 wt.%, of Zn 60 wt.% and of Al 10 wt.%. At the end of the hydrometallurgical processing was obtained 100% of copper extraction and the recovery factor was 98.46%, which corresponds to a 32 kg of Cu in 100 kg of PCB. (C) 2015 Elsevier Ltd. All rights reserved.
引用
收藏
页码:503 / 510
页数:8
相关论文
共 45 条
[1]   Study on the influence of various factors in the hydrometallurgical processing of waste printed circuit boards for copper and gold recovery [J].
Birloaga, Ionela ;
De Michelis, Ida ;
Ferella, Francesco ;
Buzatu, Mihai ;
Veglio, Francesco .
WASTE MANAGEMENT, 2013, 33 (04) :935-941
[2]   KINETICS OF SPONTANEOUS DISSOLUTION OF COPPER-47.3 ATOM-PERCENT ZINC BRASS WITH HYDROGEN DEPOLARIZATION [J].
BURZYNSKA, L ;
ZEMBURA, Z .
REACTIVITY OF SOLIDS, 1988, 4 (04) :373-381
[3]   Comparison of the spontaneous and anodic processes during dissolution of brass [J].
Burzynska, L .
CORROSION SCIENCE, 2001, 43 (06) :1053-1069
[4]   Metallurgical recovery of metals from electronic waste: A review [J].
Cui, Jirang ;
Zhang, Lifeng .
JOURNAL OF HAZARDOUS MATERIALS, 2008, 158 (2-3) :228-256
[5]   Mechanical recycling of waste electric and electronic equipment: a review [J].
Cui, JR ;
Forssberg, E .
JOURNAL OF HAZARDOUS MATERIALS, 2003, 99 (03) :243-263
[6]   Hydrogen peroxide: Importance and determination. [J].
de Mattos, IL ;
Shiraishi, KA ;
Braz, AD ;
Fernandes, JR .
QUIMICA NOVA, 2003, 26 (03) :373-380
[7]  
Devecci H., 2010, GOING GREEN CAR INN, V45
[8]   A study of the separation of cobalt from spent Li-ion battery residues [J].
Dorella, Germano ;
Mansur, Marcelo Borges .
JOURNAL OF POWER SOURCES, 2007, 170 (01) :210-215
[9]  
Doyle F.M., 1987, AICHE J, P1580
[10]   Metals recovering from waste printed circuit boards (WPCBs) using molten salts [J].
Flandinet, L. ;
Tedjar, F. ;
Ghetta, V. ;
Fouletier, J. .
JOURNAL OF HAZARDOUS MATERIALS, 2012, 213 :485-490