Effect of prestrain on fracture toughness of HSLA steels

被引:58
|
作者
Sivaprasad, S
Tarafder, S [1 ]
Ranganath, VR
Ray, KK
机构
[1] Natl Met Lab, Fatigue & Fracture Grp, Jamshedpur 831007, Bihar, India
[2] Indian Inst Technol, Dept Met Engn, Kharagpur 721302, W Bengal, India
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2000年 / 284卷 / 1-2期
关键词
prestrain; fracture toughness; tensile flow;
D O I
10.1016/S0921-5093(00)00739-5
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of tensile prestraining on the ductile fracture behaviour of two varieties of Cu-strengthened HSLA steels has been studied. It was observed that for both the HSLA steels the fracture toughness, J(C), remained invarient up to 2% prestrain, beyond which it decreased deleteriously. The nature of variation of fracture toughness with prestrain has been explained in terms of variation of the tensile flow properties of the steels with prestrain. A model correlating fracture toughness and the tensile flow properties has been proposed and it is demonstrated that the predictions of the model matched closely with the experimental observations. (C) 2000 Elsevier Science S.A. All rights reserved.
引用
收藏
页码:195 / 201
页数:7
相关论文
共 50 条
  • [41] Effects of weld strength undermatch on fracture toughness of HAZ notched weldments in a HSLA steel
    Yaowu Shi
    Zhunxiang Han
    Jianqin Fu
    International Journal of Fracture, 1998, 91 : 349 - 358
  • [42] Study on ductile fracture strain and fracture toughness of irradiated austenitic stainless steels
    Nishimura, S
    Sakamoto, H
    Kato, T
    Effects of Radiation on Materials: 21st International Symposium, 2004, 1447 : 15 - 31
  • [43] The quantitative relationship between fracture toughness and impact toughness in high-strength steels
    Li, H. F.
    Duan, Q. Q.
    Zhang, P.
    Zhou, X. H.
    Wang, B.
    Zhang, Z. F.
    ENGINEERING FRACTURE MECHANICS, 2019, 211 : 362 - 370
  • [44] Effect of microstructure evolution on fracture toughness in isothermally aged austenitic stainless steels for cryogenic applications
    Saucedo-Muñoz, ML
    Watanabe, Y
    Shoji, T
    Takahashi, H
    CRYOGENICS, 2000, 40 (11) : 693 - 700
  • [45] The effect of carbide precipitate morphology on fracture toughness in low-tempered steels containing Ni
    Krawczyk, J.
    Bala, P.
    Pacyna, J.
    JOURNAL OF MICROSCOPY, 2010, 237 (03) : 411 - 415
  • [46] Dynamic Fracture Behavior in HSLA Steel
    Sahu, Parul
    Bar, H. N.
    Kumar, Ashok
    STRUCTURAL INTEGRITY ASSESSMENT, ICONS 2018, 2020, : 523 - 533
  • [47] STUDY OF THE EFFECT OF SULFUR CONTENTS ON FRACTURE TOUGHNESS OF RAILWAY WHEEL STEELS FOR HIGH SPEED TRAIN
    Ma Yue
    Pan Tao
    Jiang Bo
    Cui Yinhui
    Su Hang
    Peng Yun
    ACTA METALLURGICA SINICA, 2011, 47 (08) : 978 - 983
  • [48] Fracture Toughness of Advanced TRIP-Aided Martensitic Steels
    Sugimoto, Koh-ichi
    Kobayashi, Junya
    Ina, Daiki
    ADVANCES IN FRACTURE AND DAMAGE MECHANICS XII, 2014, 577-578 : 97 - +
  • [49] The radiation swelling effect on fracture properties and fracture mechanisms of irradiated austenitic steels. Part I. Ductility and fracture toughness
    Margolin, B.
    Sorokin, A.
    Shvetsova, V.
    Minkin, A.
    Potapova, V.
    Smirnov, V.
    JOURNAL OF NUCLEAR MATERIALS, 2016, 480 : 52 - 68
  • [50] Fracture Toughness of Welded Commercial Lean Duplex Stainless Steels
    Henrik Sieurin
    Elin M. Westin
    Mats Liljas
    Rolf Sandström
    Welding in the World, 2009, 53 : R24 - R33