TiC-High Mn Steel-Bonded Cermets with Improved Strength and Impact Toughness

被引:4
|
作者
Li, Guoping [1 ]
Zhou, Haojun [1 ]
Lu, Jing [1 ]
Wu, Ning [1 ]
Lyu, Yinghai [2 ]
Luo, Fenghua [1 ]
机构
[1] Cent South Univ, State Key Lab Powder Met, Changsha 410083, Peoples R China
[2] Shandong Univ Sci & Technol, Coll Chem & Environm Engn, Dept Bioengn, Qingdao 266590, Peoples R China
关键词
ceramic materials; core– rim structure; impact toughness; titanium carbide; toughening mechanism; HIGH MANGANESE STEEL; MECHANICAL-PROPERTIES; MICROSTRUCTURE; BEHAVIOR; WC; DISSOLUTION; WEAR; MO2C; ADDITIONS; CARBIDES;
D O I
10.1002/srin.202000400
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
TiC-high Mn steel-bonded cermets are prepared by powder metallurgy techniques. The effects of (Ti0.5W0.5)C or WC on the microstructure, hardness, transverse rupture strength (TRS), and impact toughness (IM) are investigated. The results show that regardless of the additives used, the hardness and TRS of cermets increase with the increase in W content. However, IM is not directly proportional to the W content. Peak IM value is obtained at 5% WC addition. The highest IM of 15.12 J cm(-2) is measured from the cermet with (Ti0.5W0.5)C additive with a hardness and TRS of 64.8 HRC and 2510 MPa, respectively. Liquid phase sintering occurs at vacuum sintering. Black core-gray outer rim structure is formed in cermets with WC additives and white inner rims appear in cermets with higher W content. White core-gray rim structure is formed in cermets with (Ti0.5W0.5)C additives. The impact fracture mode of the cermets is the intergranular fracture accompanied by the tearing edges of the binder. The tearing of the high Mn steel binder is the main source of IM. IM peaks are attributed to the contradictory effects of decreased fraction and refined binder microstructure.
引用
收藏
页数:10
相关论文
共 50 条
  • [31] High-strength and high-toughness steel
    Sumitomo Metals, 1996, 48 (04): : 198 - 200
  • [32] Toughness of Ultra High Strength Steel Sheets
    Hlebova, Stanislava
    Pesek, Ladislav
    METALLOGRAPHY XV, 2014, 782 : 57 - +
  • [33] Microstructure and toughness of high strength steel welds
    Gianetto, JA
    Bowker, JT
    Braid, JEM
    Tyson, WR
    METAL WELDING AND APPLICATIONS: THERMOMECHANICAL PROCESSING OF ALLOYS, 1999, : 73 - 87
  • [35] High-strength steels with improved toughness
    Hochfeste Stähle mit verbesserter Zähigkeit
    Fecht, Nikolaus, 1600, Verlag Stahleisen GmbH (134): : 59 - 61
  • [36] THE EFFECT OF STRAIN RATE ON THE IMPACT STRENGTH OF THE HIGH-Mn STEEL
    Smiglewicz, A.
    Jablonska, M. B.
    METALURGIJA, 2015, 54 (04): : 631 - 634
  • [37] Effect of toughness and inclusion on fatigue strength of high strength steel
    Iwakura, Seigo
    Shimizu, Masao
    Kawasaki, Kazuhiro
    Nippon Kikai Gakkai Ronbunshu, A Hen/Transactions of the Japan Society of Mechanical Engineers, Part A, 1988, 54 (506): : 1826 - 1830
  • [38] The combination of strength and cryogenic impact toughness in low carbon 5Mn-5Ni steel
    Chen, Jun
    Liu, Zhen-yu
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 837
  • [39] Superior fracture toughness with high yield strength in a high-Mn steel induced by heterogeneous grain structure
    Zhang, Shengde
    Yang, Muxin
    Wu, Xiaolei
    Yuan, Fuping
    MATERIALS & DESIGN, 2023, 225
  • [40] Microstructure characterization and its relationship with impact toughness of C-Mn and high strength low alloy steel weld metals - a review
    Jorge, J. C. F.
    de Souza, L. F. G.
    Mendes, M. C.
    Bott, I. S.
    Araujo, L. S.
    dos Santos, V. R.
    Rebello, J. M. A.
    Evans, G. M.
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 10 : 471 - 501