Tin whisker growth under cycling current pulse

被引:0
|
作者
Jiang, Bo [1 ]
Xian, Ai-Ping [1 ]
机构
[1] Chinese Acad Sci, Shenyang Natl Lab Mat Sci, Met Res Inst, 72 Wenhua Rd, Shenyang 110016, Peoples R China
关键词
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A new test method, called as cycling current pulse method, was developed to evaluate the trend of whisker growth, which the cycling current pulse was first applied for cyclical heating and cooling on the tin coating sample in order to accelerate the whisker growth. The loading current in samples was controlled by the device composed of cc-simple Applied Controller and a constant current source, and the working current density varied from 5 X 10(4)A/dm(2) to 10 X 104A/dm(2). It resulted in temperature of the samples varied from 40 degrees C to 75 degrees C, and both heating and cooling dwell time per cycle were 5 min, 0-2200 cycles (about 15 days) were carried out in present work. Tin whisker growth on surface finish is observed by SEM after different cycles; the results showed that the longest fluted whisker about 120 microns in length was observed after 2200 cycles current pulse test. As a comparison with the isothermal condition, there was a relative short incubation period in cycling current pulse test at current density 5 X 104A/dm2. However, at current density of 10 X 104A/dm2, whisker growth was slowdown, the reason is not clear now. Present work shows that the cycling current pulse method is effective to evaluate the trend of whisker growth.
引用
收藏
页码:27 / +
页数:2
相关论文
共 50 条
  • [31] Elimination of whisker growth on tin plated electrodes
    Endo, M
    Higuchi, S
    Tokuda, Y
    Sakabe, Y
    ISTFA '97 - PROCEEDINGS OF THE 23RD INTERNATIONAL SYMPOSIUM FOR TESTING AND FAILURE ANALYSIS, 1997, : 305 - 311
  • [32] Mechanism and prevention of spontaneous tin whisker growth
    Tu, KN
    Suh, JO
    Wu, ATC
    Tamura, N
    Tung, CH
    MATERIALS TRANSACTIONS, 2005, 46 (11) : 2300 - 2308
  • [33] A Model for Nucleation and Growth Processes of Tin Whisker
    Nakai, Kiyomichi
    Sakamoto, Tatsuaki
    Kobayashi, Sengo
    Arakawa, Kazuto
    Mori, Hirotaro
    Takamizawa, Masao
    Murakami, Koji
    Hino, Makoto
    THERMEC 2009, PTS 1-4, 2010, 638-642 : 2688 - +
  • [34] Tin whisker growth on electroplated Sn multilayers
    Liu, Ting
    Ding, Dongyan
    Hu, Yu
    Gong, Yihua
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2015, 26 (09) : 6411 - 6418
  • [35] Tin whisker growth driven by electrical currents
    Liu, S.H., 1600, American Institute of Physics Inc. (95):
  • [36] Whisker growth on annealed and recrystallized tin platings
    Horvath, Barbara
    Illes, Balazs
    Shinohara, Tadashi
    Harsanyi, Gabor
    THIN SOLID FILMS, 2012, 520 (17) : 5733 - 5740
  • [37] μ-CT investigation of tin whisker growth mechanisms
    Hasn, S.
    Vavrik, D.
    Dusek, K.
    Pichotka, M.
    JOURNAL OF INSTRUMENTATION, 2020, 15 (02):
  • [38] Interface flow mechanism for tin whisker growth
    Howard, H. P.
    Cheng, J.
    Vianco, P. T.
    Li, J. C. M.
    ACTA MATERIALIA, 2011, 59 (05) : 1957 - 1963
  • [39] Whisker growth on tin finishes of different electrolytes
    Jiang, Bo
    Man, Ai-Ping
    MICROELECTRONICS RELIABILITY, 2008, 48 (01) : 105 - 110
  • [40] Tin whisker growth on electroplated Sn multilayers
    Ting Liu
    Dongyan Ding
    Yu Hu
    Yihua Gong
    Journal of Materials Science: Materials in Electronics, 2015, 26 : 6411 - 6418